Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003116
EISBN: 978-1-62708-199-3
... Abstract Fabrication of wrought stainless steels requires use of greater power, more frequent repair or replacement of processing equipment, and application of procedures to minimize or correct surface contamination because of its greater strength, hardness, ductility, work hardenability and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003166
EISBN: 978-1-62708-199-3
... Abstract Very high density materials are used for such applications as counterweights and radiation shields. This article focuses on the metallurgy, processing, properties, fabrication, design considerations, health and safety considerations, and applications of the most commonly used very high...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003199
EISBN: 978-1-62708-199-3
...): 20 CO, 40 H 2 , 40 N 2 , 0.1 to 0.5 CO 2 , 0.2 to 1.2 H 2 O, 0.2 to 0.8 CH 4 . In gas carburizing, a common commercial practice is to use an endothermic gas as a carrier and to enrich it with natural or propane gas additions. WHEN FABRICATED STEEL PARTS are heated in a carbonaceous...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003033
EISBN: 978-1-62708-200-6
... composite structure. Cost is always a key consideration in material selection. Some guidelines to keep in mind are: Fiber: the fewer filaments per tow, the higher the cost Resin: the lower the temperature performance, the lower the cost Prepreg: the wider the product (tape or fabric), the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003089
EISBN: 978-1-62708-199-3
... covered. This is followed by manufacturing process considerations such as material factors, shape factors, process factors, and the characteristics of fabricability, namely formability, workability, castability, machinability, and weldability. engineered materials fabricability manufacturing...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005345
EISBN: 978-1-62708-187-0
... repair welding surface preparation weld repair process selection joint selection weld repair considerations deposition techniques weld repair quality verification REPAIR WELDING, in general, is a necessary operation for most fabricators and can cost more than the price of the original component...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009020
EISBN: 978-1-62708-187-0
... of strength and rigidity that are not obtainable by other methods of fabrication. The shape and size of the part are also primary considerations in the design and application of cast parts. In this category, the possibilities of metal castings are unsurpassed. The key to consistent and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... commercial applications, epoxy resins, bismaleimide resins, polyimide resins, and thermoplastic resins are used for aerospace applications. The article addresses design considerations as well as product forms and fabrication processes. aerospace applications composite materials continuous-fiber...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003020
EISBN: 978-1-62708-200-6
... unique design considerations with respect to the physical properties, geometry, surface quality, process economics, equipment, and tooling of a component that should be considered in choosing RTM or SRIM over other competing processes for fabricating reinforced components. physical properties...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003113
EISBN: 978-1-62708-199-3
... parts by powder forging, focusing on the material considerations, such as hardenability and inclusion assessment; and process considerations, including sintering and reheating, metal flow, and secondary operations. It presents the mechanical property data for copper and graphite powders mixed with an...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
... conceptual design for acceptable reliability. This article discusses the design considerations for the use of structural ceramics for engineering applications. It describes the conceptual design and deals with fast fracture reliability, lifetime reliability, joints, attachments, interfaces, and thermal shock...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003087
EISBN: 978-1-62708-199-3
... Abstract Engineering design should result in a product that performs its function efficiently and economically within the prevailing legal, social, safety, and reliability requirements. This introductory article discusses some key considerations in design, material selection, and manufacturing...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003050
EISBN: 978-1-62708-200-6
... Abstract Ceramic and glass manufacturers take environmental regulations into consideration during all stages of the product cycle, from research and development to purchasing, processing, end use, and disposal. Ceramic and glass products are finding application in the construction industry and...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006761
EISBN: 978-1-62708-295-2
... not be representative of the failed hardware. Another consideration for the failure analyst is that the mechanical testing performed for certain fabricated shapes may not be an exact representation of the actual hardware. Fabrication products such as castings, forgings, and additive manufacturing...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003205
EISBN: 978-1-62708-199-3
... Abstract This article discusses different types of joining processes, including welding, brazing, soldering, mechanical fastening, and adhesive bonding. It examines two broad classes of welding: fusion welding and solid-state welding. The article discusses the process selection considerations...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006797
EISBN: 978-1-62708-295-2
... Abstract Distortion often is observed in the analysis of other types of failures, and consideration of the distortion can be an important part of the analysis. This article first considers that true distortion occurs when it was unexpected and in which the distortion is associated with a...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005308
EISBN: 978-1-62708-187-0
... processes such as die casting and permanent mold casting. The article reviews the pattern features and mold production considerations used in pattern design, namely, parting line considerations, addition of gates and risers, core prints, and locating points. It discusses the pattern allowances for ensuring...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003988
EISBN: 978-1-62708-185-6
... Abstract Powder forging is an extension of the conventional press and sinter powder metallurgy process, which is recognized as an effective technology for producing a variety of parts to net or near-net shape. This article focuses on the material considerations, such as powder characteristics...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001245
EISBN: 978-1-62708-170-2
... Abstract This article discusses the process considerations and deposit properties of nickel plating. It describes the Watts solution and the anode materials used. The article focuses on the nickel plating processes used for decorative, engineering, and electroforming purposes. It provides...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001285
EISBN: 978-1-62708-170-2
... Abstract This article discusses the application of amorphous and crystalline films through plasma-enhanced chemical vapor deposition (PECVD) from the view point of microelectronic device fabrication. It describes the various types of PECVD reactors and deposition techniques. Plasma enhancement...