1-20 of 552 Search Results for

extrusion tooling

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004005
EISBN: 978-1-62708-185-6
...Problems in cold extrusion and some potential causes Table 1 Problems in cold extrusion and some potential causes Problem Potential cause Tool breakage Slug not properly located in die Slug material not completely annealed Slug not symmetrical or not properly shaped...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006385
EISBN: 978-1-62708-192-4
...Functions of the individuals tools Table 1 Functions of the individuals tools Tool Function Die Makes the shape of extrusion Die holder/ring Holds the die with feeder plate and backer Die backer Supports the die to prevent collapse or fracture Bolster Transmits...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006526
EISBN: 978-1-62708-207-5
... for tooling, dies, punches, and other equipment. It covers typical tool materials and their working properties, and provides best practices for sizing aluminum slugs and preparing them for use. The article also discusses the wide range of achievable shapes from shallow cup-like extrusions to deep cups...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006534
EISBN: 978-1-62708-207-5
... extrusion speed and exit temperature, and their effect on product quality. The article also provides information on extrusion presses, press dies, and tooling, and addresses quality issues such as surface defects, blistering, and internal cracking. It concludes with a discussion on the drawing of solid...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001105
EISBN: 978-1-62708-162-7
... applications such as cold upsetting or extrusion, heavy punching, cold forging, and ball heading. For example, on ball-heading tools, the performance of the WC steel-bonded cermet was 10 to 100 times superior to that of a previously used heading die. Procedures for machining in the annealed condition...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006417
EISBN: 978-1-62708-192-4
... (Inserts) H11, H12/47–55 (Inserts) Heat-resistant alloys, nickel-base alloys H11, H12, H13/47–50 (Die blocks, inserts) H11, H13, H26/50–56 Inconel 713C, René 41 (Die blocks, inserts) Source: Ref 31 Steels and hardnesses recommended for hot extrusion tools Table 4 Steels and hardnesses...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004016
EISBN: 978-1-62708-185-6
... This article describes the mechanics and processing characteristics of equal-channel angular extrusion (ECAE). Tool design considerations for the ECAE are discussed. During ECAE, severe plastic strains and simple shear deformation mode contribute to strong, sometimes unusual effects of processing on structure...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009004
EISBN: 978-1-62708-185-6
... Fig. 1 Similarity of deformation under (a) horizontal tension and (b) vertical compression Fig. 5 An element of material at the die contact surfaces during (a) forging, (b) drawing or extrusion, and (c) rolling Fig. 6 An element of material at the center of a forging...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003021
EISBN: 978-1-62708-200-6
.... The article briefly describes the welding processes of thermoplastics, including fusion welding (hot-tool, hot gas, extrusion, and focused infrared), friction welding (vibration, spin, and ultrasonic), and electromagnetic welding (resistance, induction, dielectric, and microwave). It concludes...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003053
EISBN: 978-1-62708-200-6
..., dry pressing, cold isostatic pressing, slip casting, tape casting, roll compaction, extrusion, and injection molding. It describes the advantages, equipment and tooling, and material requirements of green machining, the machining of ceramics in an unfired state with the intent of producing parts...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005147
EISBN: 978-1-62708-186-3
... of superplastic behavior are summarized. The article discusses the superplastic forming methods, namely, blow forming, vacuum forming, thermoforming, deep drawing, superplastic forming/diffusion bonding, forging, extrusion, and dieless drawing. It provides information on superelastic forming equipment and tooling...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001469
EISBN: 978-1-62708-173-3
... joining method. The techniques are hot-tool, hot-gas, extrusion, focused infrared, laser, friction, vibration, spin, ultrasonic, and electromagnetic welding techniques (resistance, induction, dielectric, and microwave welding). The article concludes with a discussion on welding evaluation methods...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004006
EISBN: 978-1-62708-185-6
... Typical alloys and hardness values for tools used in hot extrusion Table 2 Typical alloys and hardness values for tools used in hot extrusion Steel alloys are AISI designations Tooling application For tools used in extruding: Aluminum and magnesium Copper and brass Steel Tool material...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003976
EISBN: 978-1-62708-185-6
... extrusion tools Table 4 Steels and hardnesses recommended for hot extrusion tools Tool Alloys to be extruded Steel, titanium alloys, nickel alloys Copper and copper alloys Aluminum and magnesium alloys Perishable tools Die H11, H13, H21 at 43–47 HRC (a) H21, H23, H26 at 36–45...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006085
EISBN: 978-1-62708-175-7
... Extrusion Continuous Extrusion Process Conclusions References References 1. Pearson C.E. and Parkins R.N. , The Extrusion of Metals , 2nd ed. , London , Chapman and Hall , 1960 2. Lange K. and Stenger H. , Extrusion: Process, Machinery, Tooling , American...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003183
EISBN: 978-1-62708-199-3