Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006727
EISBN: 978-1-62708-210-5
... as valid for the whole profile cross section. Source: Ref 1 Abstract Abstract This datasheet provides information on composition limits, product specifications, fabrication characteristics, processing effects on physical and mechanical properties, and applications of extrusion alloy 7003...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004015
EISBN: 978-1-62708-185-6
...Aluminum extrusion alloys by series Table 1 Aluminum extrusion alloys by series Series Alloys 1 xxx 1060, 1100, 1350 2 xxx 2011, 2014, 2024, 2219 3 xxx 3003, 3004 5 xxx 5066, 5083, 5086, 5154, 5454, 5456 6 xxx (a) 6005 (1962), 6005A, 6020, 6021, 6040, 6060...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006534
EISBN: 978-1-62708-207-5
...Abstract Abstract This article describes the direct hot extrusion process and the typical sequence of operations for producing extruded aluminum shapes from soft and medium-grade aluminum alloys, hard alloys, and aluminum-matrix composites. It discusses key process variables, including...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006516
EISBN: 978-1-62708-210-5
... conserved for the war effort. Another important application for 1 xxx alloys is for containers used to hold aerosols and other personal-care products. The alloys used for this type of can production include 1100, 1050, and simple 99.7% Al. The cans are produced by impact extrusion from sheet...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
...Abstract Abstract A four-digit numerical designation system is used to identify wrought aluminum and aluminum alloys. In addition to providing a detailed account of the temper designation system for aluminum and aluminum alloys, this article describes wrought and cast aluminum and aluminum...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006268
EISBN: 978-1-62708-169-6
...Copper-magnesium ratio and corresponding location in the phase diagram of Al-Cu-Mg Table 4 Copper-magnesium ratio and corresponding location in the phase diagram of Al-Cu-Mg Copper:magnesium, wt%/wt% Phase field Dominating equilibrium precipitates Commercial alloy >20 α + θ θ...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3