Skip Nav Destination
Close Modal
Search Results for
ethylene propylene
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 41 Search Results for
ethylene propylene
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003011
EISBN: 978-1-62708-200-6
... rubber, styrene-butadiene rubber, aerylonitrile-butadiene (nitrile) rubber, isobutylene-isoprene (butyl) rubber, ethylene-propylene (-diene) rubber, and silicone rubber. The article also provides an outline of the concerns related to the processing stages of rubbers or elastomers, including mixing or...
Abstract
This article discusses the properties, chemical structures, and applications of different types of elastomers grouped based on their resistance to aging (oxidative degradation), solvents, and temperature. These include butadiene rubber, natural rubber, isoprene rubber, chloroprene rubber, styrene-butadiene rubber, aerylonitrile-butadiene (nitrile) rubber, isobutylene-isoprene (butyl) rubber, ethylene-propylene (-diene) rubber, and silicone rubber. The article also provides an outline of the concerns related to the processing stages of rubbers or elastomers, including mixing or compounding, shaping, and vulcanizing or crosslinking.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003847
EISBN: 978-1-62708-183-2
... natural rubber, semihard natural rubber, hard natural rubber, neoprene or polychloroprene, chlorobutyl, three-ply linings, nitrile, and ethylene propylene with a diene monomer. Emphasis is placed on advantages, disadvantages, and common uses of each material discussed. abrasion resistance corrosion...
Abstract
Natural and synthetic rubber linings are used extensively in many industries for their corrosion and/or abrasion resistance. These industries include transportation, chemical processing, water treatment, power, mineral processing, and mining. This article provides information on soft natural rubber, semihard natural rubber, hard natural rubber, neoprene or polychloroprene, chlorobutyl, three-ply linings, nitrile, and ethylene propylene with a diene monomer. Emphasis is placed on advantages, disadvantages, and common uses of each material discussed.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0006515
EISBN: 978-1-62708-200-6
... ethylene glycol EGA evolved gas analysis EL electroluminescent emf electromotive force EMI electromagnetic interference EP epoxy EP-BL ethylene-propylene block copolymers EPDM ethylene-propylene-diene monomer EPM ethylene-propylene rubber...
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003001
EISBN: 978-1-62708-200-6
... 478 Epoxy amine coating 400 478 Fluorocarbon, fluorinated ethylene propylene 400 478 Fluorocarbon, polychlorotrifluoroethylene 390 472 Polyacrylate elastomer 375 464 Felt, nylon 350 450 Felt, polyester 350 450 Phenolic coating 350 450 Polyester, thermoplastic...
Book Chapter
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006540
EISBN: 978-1-62708-183-2
... EIS electrochemical impedance spectroscopy emf electromotive force EN electrochemical noise ENA electrochemical noise analysis EPA Environmental Protection Agency (U.S.) EPDM ethylene-propylene-diene monomer (rubber) Eq equation (also used to label...
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003848
EISBN: 978-1-62708-183-2
... … … √ … … Hexafluropropylene … … √ … … Propylene … … … √ √ Ethylene … √ … … √ Special cure monomers Yes No Yes/No No Yes/No Sequence (b) R R R A R See text for description of elastomers. (a) Per ASTM D 1418. (b) R, random; A, alternating...
Abstract
Elastomers belong to a group of materials known as polymers that acquire their properties and strength from their molecular weight, chain entanglements, and crystalline regions. This article focuses on the use of elastomers as seals and describes its performance capabilities from the point of a sealant. The important technical concepts that define the performance capabilities of the elastomeric part include polymer architecture (molecular building blocks), compounding (the ingredients within the polymer), and vulcanization of the elastomer shape. The article discusses the aggressiveness of the chemical environment, temperature, and minor constituents in the environment and in the material itself that affect the chemical resistance of the elastomer. It provides a discussion on performance evaluation methods, namely, immersion testing and application specific testing that are determined using ISO and ASTM standards. The article concludes with information on elastomer failure modes and failure analysis.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003002
EISBN: 978-1-62708-200-6
... 40–95 Chlorosulfonated polyethylene 50–95 Silicone 25–90 Polyacrylate 40–90 Nitrile 20–90 Fluorocarbon 65–90 Ethylene propylene, ethylene propylene diene 30–90 Epichlorohydrin 40–80 Isobutylene-isoprene 40–80 Polybutadiene 45–80 Polysulfide 20–80 Propylene...
Abstract
This article is a comprehensive collection of engineering tables providing information on the mechanical properties of and the techniques for processing and characterizing polymeric materials, such as thermosets, thermoset-matrix unidirectional advanced composites, and unreinforced and carbon-and glass-reinforced engineering thermoplastics. Values are also provided for chemical resistance ratings for selected plastics and metals, and hardness of selected elastomers.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003006
EISBN: 978-1-62708-200-6
.... Note that the PE structure is shown as a combination of two identical —CH 2 —units. Why is the mer unit not shown as a single —CH 2 — unit? Strictly speaking, this would be the correct mer unit for PE. However, because PE is actually polymerized from the compound ethylene and almost all other polymers...
Abstract
This article outlines the fundamentals of polymer science and emphasizes the aspects that are necessary and useful to applications of engineering plastics. The basic structure of polymers influences the properties of both polymers and the plastics made from them. An understanding of this basic structure permits the engineers to understand which polymers may be acceptable for a certain application, and which may not. There are various possible classification schemes for polymers. Typical classification categories include polymerization process, chemical elements that make up the monomer, or crystalline versus noncrystalline structure. The article describes the various aspects of chemical structure that are important to an understanding of polymer properties and, thus, affect eventual end uses. It discusses different types of names assigned to polymers. The article details the aspects of polymer structure and examines the properties of polymers and the way they are altered by structure.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003133
EISBN: 978-1-62708-199-3
... tension on the stranded wire. The most common polymers are polyvinyl chloride (PVC), polyethylene, ethylene propylene rubber (EPR), silicon rubber, polytetrafluoroethylene (PTFE), and fluorinated ethylene propylene (FEP). Polyimide coatings are used where fire resistance is of prime importance, such...
Abstract
This article provides an overview of the classification system of coppers for conductors and for wires and cables, as well as wire rod fabrication techniques such as rolling and continuous casting. Wiredrawing and wire stranding operations, including the preparation of rod surface, drawing, production of flat rectangular wire, annealing, and coating, are discussed. The article also provides information on electrical insulation and jacketing techniques, including polymeric insulation, enamel insulation, and paper-and-oil insulation.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
...) Butyl rubber (IIR, a blend of isoprene and isobutylene copolymers) Chlorobutyl rubber (CUR, manufactured by the chlorination of IIR) Ethylene-propylene rubber (EPDM, a copolymer of ethylene and propylene with the addition of a diene monomer) Nitrile rubber (NBR, a copolymerization of...
Abstract
This article provides a brief discussion on the common types of overlayers that can be used on a metal surface to protect it from corrosion. These overlayers include phosphate, chromate, and chromate-free conversion coatings; hot dip galvanizing; cementitious linings; glass and porcelain enamels; electroplating; thermal spray coatings; and rubber linings.
Book Chapter
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005687
EISBN: 978-1-62708-198-6
... PEEK Fixation devices Poly(etheretherketone), composite Polyetheretherketone composite, polyketone composite PEEK Fixation devices Polyolefins Poly(ethylene), low density ASTM F639 Low-density polyethylene LDPE Knees Poly(propylene) ASTM D4101, ASTM D5857 Polypropylene PP...
Abstract
This article tabulates materials that are known to have been used in orthopaedic and/or cardiovascular medical devices. The materials are grouped as metals, ceramics and glasses, and synthetic polymers in order. These tables were compiled from the Medical Materials Database which is a product of ASM International and Granta Design available by license online and as an in-house version. The material usage was gleaned from over 24,000 U.S. Food and Drug Administration (USFDA), Center for Devices and Radiological Health, Premarket notifications (510k), and USFDA Premarket Approvals, and other device records that are a part of this database. The database includes other material categories as well. The usage of materials in predicate devices is an efficient tool in the material selection process aiming for regulatory approval.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003026
EISBN: 978-1-62708-200-6
...) … Polysulfide Widely used for potting of electrical connectors EPR R Ethylene-propylene Good general-purpose electrical properties EPT R Ethyl-propylene terpolymer Good general-purpose electrical properties Hypalon (HYP) CSM Chlorosulfonated polyethylene Not outstanding electrically...
Abstract
In terms of their electrical properties, plastics can be divided into thermosetting and thermoplastic materials, some of which are conductive or semiconductive. This article provides detailed information on factors that affect the property of plastics. It discusses the major test methods used to determine the following dielectric properties of plastics: dielectric breakdown voltage, dielectric strength, dielectric constant, dissipation factor, arc tracking resistance, insulation resistance, volume, and surface resistivity or conductivity. The test specifications and conditions, recommended by several U.S. and foreign testing organizations for characterizing the electrical properties of plastic materials are listed. The article describes the influence of these properties on selection of plastics for insulation application. An outline of the electromagnetic shielding and testing methods of electromagnetic interference are also provided. Designations, electrical properties, and applications of elastomers are tabulated.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001319
EISBN: 978-1-62708-170-2
... that have been created on the surface of these materials. Contact angle measurements and electron spectroscopy of plasma-treated surfaces have confirmed the permanent nature of plasma surface modification of polymers. For example, plasma-modified fluorinated ethylene propylene (FEP) was shown to retain...
Abstract
This article provides an overview of plasma surface treatments for plastics. It covers the equipment and methods used in plasma processing, providing detailed explanations of the plasma discharge reactions and how they affect surface state and topography. It also provides information on contamination removal, plasma surface modification, plasma-induced grafting, and plasma film deposition.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001278
EISBN: 978-1-62708-170-2
.... These substrates are still widely used, including EPDM (ethylene-propylene-diene monomers), reaction injected molded polyurethane, glass-filled reaction injection molded polyurethane, and thermoplastic polyurethane. More recently, rubber-modified poly-propylene thermoplastic olefin has been used for...
Abstract
This article describes elastomeric coatings that are suitable for painting flexible plastic substrates. It focuses on coatings systems that find utility in automotive exterior applications, where the requirements of appearance and durability are most severe. The article discusses acrylic polyols, condensation polymers, vapor curing systems, water-based coatings, and coatings for thermoplastic olefins.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005672
EISBN: 978-1-62708-198-6
... Silicones, such as polydimethylsiloxane Styrenic block polymers, such as styrene-butadiene-styrene, styrene-ethylene/butylene-styrene, styrene-ethylene/propylene, and styrene-isoprene-styrene Others, such as polyesters and polyurethanes A PSA formulation usually contains one or more of the...
Abstract
This article provides an overview of curing techniques, adhesive chemistries, surface preparation, adhesive selection, and medical applications for adhesives. The curing techniques are classified into moisture, irradiation, heat, and anaerobic. The article highlights the common types of curable adhesives used for medical device assembly, including acrylics, cyanoacrylates, epoxies, urethanes, and silicones. Other forms of adhesives, such as hot melts, bioadhesives, and pressure-sensitive adhesives, are also discussed. Adhesives are used for medical device assembly, hard-tissue attachment in the fields of orthopedics and dentistry, and soft-tissue attachment such as wound closure. The typical characteristics and applications of biocompatible medical device adhesives are listed in a table. The article concludes with a section on selection of materials for medical adhesives.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006011
EISBN: 978-1-62708-172-6
... steel and aluminum but also may include concrete. It also covers protective coatings used in the built environment on concrete flooring, walls, doors, trim, roofing, and waterproofing. These common substrates include concrete, steel, and wallboard but may include sheet goods such as ethylene propylene...
Abstract
Polyurethane is any polymer consisting of a chain of repeating organic units joined by urethane linkages. Polyurethane polymers are formed through step-growth polymerization by making a monomer containing at least two isocyanate functional groups to react with another monomer containing at least two hydroxyl (alcohol) groups. This article provides a detailed account of the protective coatings used in the building, infrastructure, and architectural markets. It focuses on the various types of polyurethane coatings used in these applications: moisture-cure and two-pack aromatic coatings as primers and topcoats, moisture-cure aromatic elastomeric high-build coatings, moisture-cure aliphatic topcoats, two-pack aliphatic polyurethane coatings as topcoats, and one- and two-pack polyurethane dispersion coatings as sealers and topcoats. It also includes a section on the health effects of isocyanates.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006009
EISBN: 978-1-62708-172-6
... 1 . Table 1 Monomers for unsaturated polyesters Saturated alcohols Remarks 1,2-propylene glycol Most common glycol Ethylene glycol Less compatible with styrene than propylene glycol Diethylene glycol Good drying properties Neopentyl gylcol Good hydrolysis resistance...
Abstract
This article provides a discussion on polyester coating applications such as powder coatings, can coatings, and automotive paints. It includes an overview, structure, properties, and benefits of vinyl ester resins. The article discusses the additives for both unsaturated polyester and vinyl ester coatings, namely, curing systems, thixotropic agents and fillers. It exemplifies polyester and vinyl ester coating, lining and flooring systems that are used for top-to-bottom protection of industrial plants and equipment. The article also highlights the concerns to be addressed when using polyesters and vinyl esters.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001321
EISBN: 978-1-62708-170-2
... Epichlorohydrin (1-Chloro-2,3-epoxypropane) 106887 1,2-Epoxybutane 140885 Ethyl acrylate 100414 Ethyl benzene 51796 Ethyl carbamate (Urethane) 75003 Ethyl chloride (Chloroethane) 106934 Ethylene dibromide (Dibromoethane) 107062 Ethylene dichloride (1,2-Dichloroethane) 107211...
Abstract
This article describes selected U.S. environmental statutes and regulations that are pertinent to material surface finishers. It provides information on the applicability, requirements, and permitting conditions of the Clean Air Act, the Resources Conservation and Recovery Act, the Superfund Amendments and Reauthorization Act, and the Clean Water Act.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003023
EISBN: 978-1-62708-200-6
Abstract
Thermal analysis provides a powerful tool for researchers and engineers in determining both unknown and reproducible behavioral properties of polymer molecules. This article covers the thermal analysis and thermal properties of engineering plastics with respect to chemical composition, chain configuration, conformation of the base polymers, processing of the base polymers with or without additives; and the response to chemical, physical, and mechanical stresses of base polymers as unfilled, shaped articles or as components of composite structures. It also describes thermal analysis techniques, including differential scanning calorimetry, thermogravimetric analysis, thermomechanical analysis, and rheological analysis. This article also summarizes the basic thermal properties used in the application of engineering plastics, such as thermal conductivity, temperature resistance, thermal expansion, specific heat, and the determination of glass transition temperatures. It concludes with a discussion of the thermal and related properties of nine thermostat resin systems divided into three groups by low, medium, and high service temperature capabilities.