1-20 of 604 Search Results for

engineering structural applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
... Abstract The design process for ceramic materials is more complex than that of metals because of low-strain tolerance, low fracture toughness and brittleness. The application of structural ceramics to engineering systems hinges on the functional benefits to be derived and is manifested in the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003061
EISBN: 978-1-62708-200-6
... valve components, rolling elements and bearings, paper and wire manufacturing, biomedical implants, heat exchangers, adiabatic diesel engines, advanced gas turbines, and aerospace applications. advanced ceramics aerospace applications mineral processing equipment structural applications...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001317
EISBN: 978-1-62708-170-2
..., offretite, mordenite, and the pentasil zeolites ZSM-5 and ZSM-11. Titanium oxide (TiO 2 ), or titania, is currently used as a catalyst carrier for the selective catalytic reduction of nitrogen oxide (NO x , or NO + NO 2 ) using ammonia in stationary source applications. It has two crystal structures...