DOI: 10.31399/asm.hb.v11.a0003517
EISBN: 978-1-62708-180-1
... Abstract This article focuses on the life assessment methods for elevated-temperature failure mechanisms and metallurgical instabilities that reduce life or cause loss of function or operating time of high-temperature components, namely, gas turbine blade, and power plant piping and tubing...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006807
EISBN: 978-1-62708-329-4
... Abstract This article provides some new developments in elevated-temperature and life assessments. It is aimed at providing an overview of the damage mechanisms of concern, with a focus on creep, and the methodologies for design and in-service assessment of components operating at elevated...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006802
EISBN: 978-1-62708-329-4
... on failure and life assessment of components, structural design philosophies, the role of the failure analyst in life assessment, and the role of nondestructive inspection. They also cover fatigue life assessment, elevated-temperature life assessment, fitness-for-service life assessment, brittle fracture...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003512
EISBN: 978-1-62708-180-1
... information on fatigue life assessment, elevated-temperature life assessment, and fitness-for-service life assessment. elevated-temperature life assessment fabrication failure analysis fatigue life assessment fitness-for-service life assessment material defects nondestructive inspection stress...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003545
EISBN: 978-1-62708-180-1
... covered in the article “Elevated-Temperature Life Assessment for Turbine Components, Piping, and Tubing” in this Volume. Bulk Creep Behavior Some of the key material properties at high temperature are thermal expansion coefficient, stress rupture, elastic modulus, fatigue life, and oxidation...
Book Chapter

By Richard P. Baron
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006780
EISBN: 978-1-62708-295-2
... in high-temperature applications. The complex effects of creep-fatigue interaction are also discussed, although more detail on this is described in the article “Thermomechanical Fatigue: Mechanisms and Practical Life Analysis” in this Volume. Life assessment is also covered in the article “Elevated...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006909
EISBN: 978-1-62708-395-9
... of accelerated life testing and aging of unreinforced and fiber-reinforced plastic materials for assessing long-term material properties and life expectancy in hostile service environments. It considers various environmental factors, such as temperature, humidity, pressure, weathering, liquid chemicals (i.e...
Book Chapter

By A.F. Liu
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002390
EISBN: 978-1-62708-193-1
... rate behavior and those essential elements in making spectrum crack growth life prediction. It provides information on life assessment for bulk creep damage. crack growth rate creep damage high temperature life assessment spectrum life prediction CURRENT FRACTURE MECHANICS theory treats...
Book Chapter

By David A. Woodford
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002472
EISBN: 978-1-62708-194-8
... to quantify the accumulation of damage as a function of operating conditions. There are two basic approaches to using the concept of damage accumulation for life assessment: Based on a detailed knowledge of the operating conditions, including temperature and stress changes, the remaining life...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006921
EISBN: 978-1-62708-395-9
... pipe (PEX). The minimum prediction desired for this piping is a 50-year life at 60 °C (140 °F) based on testing at elevated temperatures in chlorinated water. This testing is performed according to ASTM F2023 at three temperatures: 95 °C (203 °F), 105 °C (221 °F), and 115 °C (239 °F), with chlorine...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002413
EISBN: 978-1-62708-193-1
... Abstract This article focuses on the isothermal fatigue of solder materials. It discusses the effect of strain range, frequency, hold time, temperature, and environment on isothermal fatigue life. The article provides information on various isothermal fatigue testing methods used to assess...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003289
EISBN: 978-1-62708-176-4
... Method Many designs for elevated-temperature service require that deformation not exceed some maximum value; in these cases, creep strain rather than rupture life becomes the focus. Although published compilations and computer banks of data include rupture properties for most materials...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001477
EISBN: 978-1-62708-173-3
... of crack growth is a final option. This approach can be used to both monitor crack growth and assess remaining life or to decide whether or not to repair, replace, or retire the component under consideration. High-Temperature Creep Components that operate at elevated temperatures can fail because...
Book Chapter

Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001035
EISBN: 978-1-62708-161-0
...-rupture properties or the degree of deformation from creep. In recent years, the worldwide interest in life extension of high-temperature components has also promoted considerably more interest in elevated-temperature fatigue. This effort has led to tests and methods for evaluating the effects of creep...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006804
EISBN: 978-1-62708-329-4
... vessel shell wall failed due to elevated-temperature stress rupture (creep failure), which was indicated by the extensive bulging, microcracking, and void formation on its outside surface. Figure 23 shows the stress-rupture voids near the outside surface. Microstructural assessment of the shell wall...
Book Chapter

By B.E. Gore, W. Ren, P.K. Liaw
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003307
EISBN: 978-1-62708-176-4
... testing cyclic loading ductile materials life-prediction models material characterization service life static loading structural components time-dependent fracture mechanics HIGH-TEMPERATURE APPLICATIONS in the chemical processing, aerospace, nuclear and fossil power-generation industries...
Book Chapter

By P.F. Timmins
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002387
EISBN: 978-1-62708-193-1
... Abstract This article focuses on the subject of proactive or predictive maintenance with particular emphasis on the control and prediction of corrosion damage for life extension and failure prevention. It discusses creep life assessment from the perspective of creep-rupture properties...
Book Chapter

Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... seriously reduce fatigue life and that fatigue strains can seriously reduce creep life. This effect occurs in both stainless steels and low-alloy or carbon steels when temperatures are in the creep range (see the article “Elevated-Temperature Properties of Ferritic Steels” in this Volume). Creep...
Book Chapter

By Tarsem Jutla
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002384
EISBN: 978-1-62708-193-1
...-relieved nodes in offshore structures. Due consideration has to be given to the complexity of the overall structure when stress relieving and to the time and temperature of the process. Effect of Material Properties Because crack propagation dominates the fatigue life of welded joints, material...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006026
EISBN: 978-1-62708-172-6
... (or coatings on existing walking/working surfaces) are typically tested in both the dry and wet conditions, and a slip index is reported. Fig. 25 Variable-incidence tribometer. Courtesy of Nuent Consulting (formerly Dynamic Safety). Source: Ref 10 Elevated-Temperature Resistance Some...