1-20 of 350 Search Results for

electroplated coatings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003687
EISBN: 978-1-62708-182-5
... by uneven buffing. Sharply angled edges Undesirable. Reduced coating thickness at center areas requires increased plating time to obtain a minimum thickness of durable electroplate. All edges should be rounded. Edges that will contact painted surfaces should have a minimum radius of 0.8 mm (0.03...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006395
EISBN: 978-1-62708-192-4
... 0.0170 349.8 Electroplated hard chrome 0.0469 966.6 Cemented tungsten carbide 0.0274 43.7 Tool steel, R c 63 0.1281 3478.6 Adapted from Ref 25 Friction coefficients for electroless nickel (EN) composites and other common coatings Table 6 Friction coefficients...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001255
EISBN: 978-1-62708-170-2
...) Copper (as metal), g/L (oz/gal) 20 (2.7) Tin (as metal), g/L (oz/gal) 14 (1.9) Hydroxide, g/L (oz/gal) 10 (1.3) Operating conditions Temperature, °C (°F) 65 (149) Abstract Abstract Copper alloys are widely used as electroplated coatings. They can also be used with practically...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004126
EISBN: 978-1-62708-184-9
... electroplated coatings; conversion coatings; supplemental oils, waxes, and lubricants; organic paint coatings; and other finishes such as vacuum deposits, mechanical plating, thermal spray coatings, and hot-dip coatings. The article also lists the test requirements and time to failure of the coatings...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003022
EISBN: 978-1-62708-200-6
... Adhesion of Metallic Coatings to Plastics Metallizing Processes Environmental Considerations Performance of Metallized Plastics References References 1. Lowenheim F.A. , Electroplating , McGraw-Hill , 1978 2. Saubestre E.B. , Plating on Nonconductors , Modern...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006491
EISBN: 978-1-62708-207-5
... Aluminum Alloys for Electroplating , J. Electrochem. Soc. , Vol 96 , 1950 , p 143 – 151 10.1149/1.2777981 14. Zelley W.G. , Formation of Immersion Zinc Coatings on Aluminum , J. Electrochem. Soc. , Vol 100 , 1953 , p 328 – 333 10.1149/1.2781127 15. Dreissig R...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001271
EISBN: 978-1-62708-170-2
.... , Guzzetta F.H. , and Lin R.Y. , The Effect of Processing Temperature on the Microroughness of Electroplated Zinc Coatings on Steel , Proceedings of the Fifth Continuous Steel Strip Plating Symposium , American Electroplaters and Surface Finishers Society , 1987 13. Watson S.A...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004107
EISBN: 978-1-62708-184-9
... resistance. This article discusses thermal spray, hotdipping, and electroplating processes used to apply coatings in steel structures. It describes the corrosion attributes of the resulting coatings and discusses the methods of protecting steel from corrosion using aluminum and zinc coatings. References...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
... irons are not usually heat treated, except for stress relief and to continue austenite transformation. Properties and characteristics of conventional electroplated metal coatings Table 6 Properties and characteristics of conventional electroplated metal coatings Metal Coating hardness...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005707
EISBN: 978-1-62708-171-9
... but requires an absorptive coating that may need cleaning Investment Lowest on high-power applications Lowest on low-power applications (a) Pattern size is controlled by the available power of the equipment. Nominally, 15–30 W/mm 2 (10–20 kW/in. 2 ) is used. Source: Ref 3 Electroplated...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001308
EISBN: 978-1-62708-170-2
..., and coating of aluminum. These include abrasive blast cleaning, barrel finishing, polishing, buffing, satin finishing, chemical cleaning, chemical brightening, electrolytic brightening, chemical etching, alkaline etching, acid etching, chemical conversion coating, electroplating, immersion plating...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
... coatings, hot-dip coating processes, electrogalvanizing, electroplating, metal cladding, organic coatings, zinc-rich coatings, porcelain enameling, thermal spraying, hardfacing, vapor-deposited coatings, surface modification, and surface hardening via heat treatment. alloy steel cadmium plating...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003105
EISBN: 978-1-62708-199-3
...Guide to corrosion prevention for carbon steels in various environments Table 7 Guide to corrosion prevention for carbon steels in various environments Preventive method Atmosphere Soil Fresh water Seawater Steam systems Acids and pickling baths Metal coatings: electroplating...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001323
EISBN: 978-1-62708-170-2
... electroplating, spray coating applications, and cobalt/molybdenum-base conversion coating. The article discusses the material and process substitutions that can be used to eliminate the use or emissions of chromium in industrial processes. It describes the physical characteristics of each coating, economics...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005164
EISBN: 978-1-62708-186-3
... steels are produced by batch annealing the cold rolled steel in coil form, temper rolling, then electroplating a layer of essentially pure zinc crystals on the surface of the sheet. As with hot dip galvanized products, the zinc coating is much softer than the base steel and can help provide some...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001307
EISBN: 978-1-62708-170-2
... hot-working or heat-treating operations on nickel-, cobalt-, and iron-base heat-resistant alloys. It provides a brief description of applicable finishing and coating processes, including polishing, electroplating, ceramic coatings, diffusion coatings, and shot-peening. The article presents numerous...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001313
EISBN: 978-1-62708-170-2
... on common plating and coating methods, including electroplating, anodizing, and oxidation-resistant coatings. References References 1. Timmons G.A. , Machining Molybdenum , Climax Specialty Metals , Cleveland, OH , 1993 2. Beat T.G. , Kelly W.K. , and Dini J.W...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003145
EISBN: 978-1-62708-199-3
... the primary and secondary production of tin and explains the uses of tin in coating, namely tinplating, electroplating, and hot dip coatings. It presents a short note on pure (unalloyed) tin and uses of tin in chemicals. The article also covers the compositions and uses of tin alloys which include solders...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
..., electroplating, passivation, coloring, and organic coatings. Selected References Selected References • Durney Lawrence J. , Ed., Electroplating Engineering Handbook , 4th ed. , Van Nostrand Reinhold , 1984 • Fishlock David , Metal Coloring , Robert Draper Ltd., 1970...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
... linings; glass and porcelain enamels; electroplating; thermal spray coatings; and rubber linings. Reference Reference 1. GalvInfo Center , GalvInfo Note #2.3 rev 1.0, January 2011 . Available from https://www.galvinfo.com/project/galv-info-notes/ Selected References Selected...