Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005611
EISBN: 978-1-62708-174-0
... processes start with a 3-D model designed in a computer-aided design (CAD) environment, where the deposition path and process parameters are generated. The article provides a description of the electron beam direct manufacturing (EBDM) system used for manufacturing of target parts with the aid of a case...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0009211
EISBN: 978-1-62708-194-8
... of Direct Laser Sintered Ti-6Al-V4,” Materials Science & Technology ( Columbus, OH ), 2011 17. Rengers S. , “Electron Beam Melting (EBM) vs. Direct Metal Laser Sintering (DMLS),” presented at Direct Part Manufacturing Workshop, SAMPE Midwest Chapter, Wright State University, Nov 2012...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006581
EISBN: 978-1-62708-290-7
.... , “Electron Beam Melting (EBM) vs. Direct Metal Laser Sintering (DMLS),” presented at Direct Part Manufacturing Workshop, SAMPE Midwest Chapter , Wright State University , Nov 2012 39. Svensson M. , “ Ti6Al4V Manufactured with Electron Beam Melting (EBM): Mechanical and Chemical Properties...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006549
EISBN: 978-1-62708-290-7
...-energy deposition system applied to produce a complex IN-718 alloy casing, which is also shown in the completed near-net form. Courtesy of RPM Innovations Fig. 28 Images of electron-beam-based directed-energy deposition of Ti-6Al-4V alloy during deposition, the completed near-net shape...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006545
EISBN: 978-1-62708-290-7
... P. , Residual Stress and Distortion Modeling of Electron Beam Direct Manufacturing Ti-6Al-4V , Proc. Inst. Mech. Eng. B, J. Eng. Manuf. , Vol 229 , 2015 , p 1803 – 1813 , 10.1177/0954405414539494 62. Shimizu S. , Fujii H.T. , Sato Y.S. , Kokawa H. , Sriraman M.R...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006838
EISBN: 978-1-62708-329-4
... for melting and depositing Direct manufacturing Uses electron beam and metal wire for melting and depositing Shaped metal deposition or wire and arc AM Uses electric arc and metal wire for melting and depositing Powder-bed fusion methods Selective laser sintering Uses laser and metal powder...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006564
EISBN: 978-1-62708-290-7
... Abstract This article covers in-line process monitor