1-20 of 279

Search Results for electromagnetic inspection

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006467
EISBN: 978-1-62708-190-0
... of flaws encountered in the inspection of steel bars, including porosity, inclusions, scabs, cracks, seams, and laps. Inspection methods, such as magnetic-particle inspection. liquid penetrant inspection, ultrasonic inspection, and electromagnetic inspection, of steel bars are also described. The article...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006475
EISBN: 978-1-62708-190-0
... Abstract Electromagnetic signals at microwave and millimeter-wave frequencies are well suited for inspecting dielectric materials and composite structures in many critical applications. This article presents a partial list of reported nondestructive testing (NDT) application areas...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006450
EISBN: 978-1-62708-190-0
... Abstract Eddy-current inspection is based on the principles of electromagnetic induction and is used to identify or differentiate among a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic and nonferromagnetic metals and metal parts...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003234
EISBN: 978-1-62708-199-3
... Abstract Eddy-current inspection is a nondestructive evaluation method based on the principles of electromagnetic induction. Eddy-current methods are used to identify or differentiate a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003235
EISBN: 978-1-62708-199-3
... metallic coatings microwave inspection nondestructive evaluation plastic materials thickness measurements MICROWAVES (or radar waves) are a form of electromagnetic radiation with wavelengths between 1000 cm and 1 mm in free space. Because microwaves have wavelengths that are 10 4 to 10 5 times...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006465
EISBN: 978-1-62708-190-0
... for additively manufactured metallic parts. It also examines nondestructive testing (NDT) inspection and characterization methods for each of the manufacturing stages in their natural order. The article provides information on various inspection techniques for completed AM manufactured parts. The various...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006461
EISBN: 978-1-62708-190-0
... structures. air-coupled ultrasonics electromagnetic acoustic transducers lasers nondestructive evaluation nonlinear ultrasonic inspection piezoelectric transducers Rayleigh wave defect detection surface acoustic wave microscopy THIS ARTICLE OFFERS a brief overview of the characteristics...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006336
EISBN: 978-1-62708-179-5
... conditions such as hardness, thickness, or the presence of corrosion, porosity, or cracks. Eddy-current inspection has been used to detect objectionable casting microstructure near the surface, such as chill or near-surface voids or inclusions. Eddy-current inspection uses the electromagnetic principles...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005857
EISBN: 978-1-62708-167-2
... and process variations cause continual adjustment of process parameters. At first-article inspection, all heat treating requirements must be inspected. This is done by destructive metallurgical testing. Nondestructive electromagnetic testing can help to reduce downtime due to setup and changeovers...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006471
EISBN: 978-1-62708-190-0
... of noncontact inspection uses electromagnet acoustic transducers (EMATs), which use an electromagnetic field and magnet, to achieve wave generation ( Ref 7 ). Electromagnet acoustic transducers are considered in detail in the article “ Electromagnetic Acoustic Transducers for Nondestructive Evaluation...
Image
Published: 30 June 2023
Fig. 25 Illustration of the x - z image acquired via in-process eddy current inspection of the fabrication of four Ti-6Al-4V parts. The colors indicate the electromagnetic response of the sensor. More
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006479
EISBN: 978-1-62708-190-0
... Practice for Digital Imaging and Communication Nondestructive Evaluation (DICONDE) for Computed Radiography (CR) Test Methods” ASTM E268 “Electromagnetic Testing” ASTM E426 “Practice for Electromagnetic (Eddy-Current) Examination of Seamless and Welded Tubular Products, Austenitic Stainless Steel...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006438
EISBN: 978-1-62708-190-0
... with their applications, limitations, and advantages. It includes details on NDE codes, calibration standards, inspection frequency, guidance on how to perform inspections, applicability, and mandatory and nonmandatory practice. The article also provides tips on where to focus inspections in order to align...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003237
EISBN: 978-1-62708-199-3
... Abstract Acoustic-emission inspection detects and analyzes minute acoustic-emission signals generated by discontinuities in materials under applied stress. This article discusses the types of acoustic emissions (continuous-type emissions and burst-type emissions) and applications, including...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003228
EISBN: 978-1-62708-199-3
... Abstract This article reviews nondestructive testing (NDT) and inspection techniques, namely liquid penetrant, magnetic particle, ultrasonics, X-ray, eddy current, visual and radiography that are commonly used to detect and evaluate flaws or leaks in an engineering system. This article compares...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003232
EISBN: 978-1-62708-199-3
... Abstract Magnetic-particle inspection is a nondestructive testing technique used to locate surface and subsurface discontinuities in ferromagnetic materials. Beginning with an overview of the applications, advantages, and limitations of magnetic-particle inspection, this article provides...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003233
EISBN: 978-1-62708-199-3
... . In this application, the part is magnetized by an electromagnet, as indicated in Fig. 5 (a). The race is rotated by a spindle, and the surface is scanned using an induction coil sensor. The active portion of the raceway is inspected by incrementally indexing the sensor across the raceway. Magnetizing fields...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003658
EISBN: 978-1-62708-182-5
...) tools: microwave NDE and guided wave (GW) ultrasonic NDE methods. The in-service inspection scenario is complicated by the fact that corrosion is often hidden, and expensive disassembly can be required to complete an inspection. Microwave and GW NDE techniques have promise as methods that minimize...
Book Chapter

By J.F. Libsch
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001387
EISBN: 978-1-62708-173-3
... of induced current ( I 2 R losses) in the assembly components. It occurs when the electrically conductive components are placed in the electromagnetic field created by rapidly alternating current flow in the inductor ( Fig. 1 ). With proper coil design, heating occurs rapidly at the joint area, providing...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003238
EISBN: 978-1-62708-199-3
... is a nondestructive-inspection method that is based on differential absorption of penetrating radiation—either electromagnetic radiation of very short wavelength or particulate radiation—by the part or test piece (object) being inspected. Because of differences in density and variations in thickness of the part...