... Abstract This article describes the methods used for coloring anodized aluminum coatings: integral coloring, electrolytic coloring, chemical coloring, and organic dyeing. It discusses organic dye chemistry in terms of single-component organic dyes and multicomponent dyes. The article reviews...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006511
EISBN: 978-1-62708-207-5
... discussed in the article “Coloring Anodized Aluminum” in this Volume. Applications of the chemical and electrolytic brightening processes are functional and decorative. They include jewelry, razor parts, automotive trim and wheel rims, shower door trim, sink faucets, drapery rods, fountain pens...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003748
EISBN: 978-1-62708-177-1
... Abstract Metallographic preparation of a material involves the elimination of artifacts or scratches from fine polishing and may be achieved by methods such as attack polishing, vibratory polishing, chemical polishing, electrolytic polishing, and electromechanical polishing. This article...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003752
EISBN: 978-1-62708-177-1
... esthetic value only. Color etching methods are widely used, although they are not universal. Color etchants have been developed for a limited number of metals and alloys, and they are not always easy to use, nor are they fully reliable. Color etchants are used by immersion or electrolytically. A complete...
Book Chapter

Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004221
EISBN: 978-1-62708-184-9
... Abstract This article includes a collection of color images that aid in the identification and classification of forms of corrosion in industries and environments. It emphasizes the negative aspects of corrosion and examines the cost and the effort to test, evaluate, simulate, and prevent...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... coating, cladding, porcelain enameling, and thermal spray. Organic coatings have a wide variety of properties, but their primary use is for corrosion resistance combined with a pleasing colored appearance. The article discusses the various types of organic coatings applied to cast irons. Practically any...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006342
EISBN: 978-1-62708-179-5
... °F) for 1–3 min Dip etch for 10 s to 2 min at boiling point Electrolytic etch (a) 2. Klemm’s I 50 mL saturated aqueous sodium thiosulfate (Na 2 S 2 O 3 ⋅5H 2 O) 1 g potassium metabisulfite (K 2 S 2 O 5 ) Immerse sample for 40–100 s. Reveals phosphorus segregation (white); colors...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001250
EISBN: 978-1-62708-170-2
... Abstract A tin deposit provides sacrificial protection to copper, nickel, and many other nonferrous metals and alloys. Tin also provides good protection to steel. Tin can be deposited from either alkaline or acid electrolytes. This article explains the compositions and operating conditions of...
Series: ASM Handbook Archive
Volume: 10
Publisher: ASM International
Published: 01 January 1986
DOI: 10.31399/asm.hb.v10.a0001742
EISBN: 978-1-62708-178-8
... Abstract Electrogravimetry is the oldest electroanalytical technique in which the element of interest is deposited electrolytically onto an electrode and weighed. This article discusses the principles involved in determining the electrolysis rate of the solution, and describes different methods...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002161
EISBN: 978-1-62708-188-7
... Abstract This article describes the various characteristics of electrochemical grinding (ECG). It discusses grinding methods that can be performed with ECG components, namely, the electrolyte delivery and circulating system, the electrolyte, the DC power supply, grinding wheel, and the...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003215
EISBN: 978-1-62708-199-3
... Abstract Copper can be electrodeposited from numerous electrolytes. Cyanide and pyrophosphate alkalines, along with sulfate and fluoborate acid baths, are the primary electrolytes used in copper plating. This article provides information on the chemical composition, plating baths, and operating...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001261
EISBN: 978-1-62708-170-2
... Abstract Selective plating, also known as brush plating, differs from traditional tank or bath plating in that the workpiece is not immersed in a plating solution (electrolyte). Instead, the electrolyte is brought to the part and applied by a handheld anode or stylus, which incorporates an...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003680
EISBN: 978-1-62708-182-5
... high resistance to alkali, and anodizing with alternative current in sulfuric acid solution gives flexible anodic oxide films. Coloring of anodic oxide films is classified into three groups: integral coloring, dyeing and electrolytic coloring. In integral coloring, many kinds of organic acids, oxalic...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001281
EISBN: 978-1-62708-170-2
... finishes. Certain mineral pigments can be precipitated within the pores to yield a limited range of stable colors. Integral color anodizing, depending on the alloy composition, is used to provide a range of stable earth-tone colors suitable for architectural applications. Electrolytic coloring is a two...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003749
EISBN: 978-1-62708-177-1
..., but greater attention must be given to fine scratch removal. Anodizing is an electrolytic process for depositing a thin oxide film on the surface of the specimen in a standard electropolishing unit. The resulting interference colors are a function of the anodic film thickness, which depends...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001314
EISBN: 978-1-62708-170-2
... reduced oxide, sometimes followed by a flash pickle to brighten; and black or dark-colored surface requiring removal of adherent oxide film or scale. The article also reviews specialized pickling operations of nickel alloys and various cleaning and finishing operations, including grinding, polishing...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003774
EISBN: 978-1-62708-177-1
... mL HBF 4 200 mL H 2 O Electrolytic: use stainless steel cathode; specimen is anode. Use minimum etching time and voltage (less than 40 s and 20 V dc respectively). When viewed with polarized light, grains with the same orientation are colored similarly. Shows general structure, intergranular...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001253
EISBN: 978-1-62708-170-2
... Abstract Gold electroplating was invented in 1840. During the first 100 years electrodeposited gold was used primarily for its aesthetic appeal as a decorative finish. This article provides a description of the gold plating process and the electrolytes used. It discusses the decorative and...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
.... For compositions and operating conditions of tin electrolytes, see the article “Tin Plating” in this Volume. The 40 to 50% Sn alloy, speculum metal, has been used as a decorative coating because of its silverlike color. The bronze alloy coatings containing 10 to 20% Sn are producible to match the...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004103
EISBN: 978-1-62708-184-9
... hot electrolytic solutions. It is a precursor to either class 3A or 3B rouge. The color is iridescent gold, red, or blue. The color is related to the oxide thickness ( Ref 12 ). Figure 21 illustrates the depth of oxygen as a function of color. The control is the standard silver electropolished film...