Book Chapter

By S.D. Brandi, S. Liu, R.D. Thomas, Jr.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005591
EISBN: 978-1-62708-174-0
... Abstract Electroslag welding (ESW) involves high energy input relative to other welding processes, resulting generally in inferior mechanical properties and specifically in lower toughness of the heat-affected zone. Electrogas welding (EGW) is a method of gas metal or flux cored arc welding...
Book Chapter

By S. Liu, S.D. Brandi, R.D. Thomas, Jr.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001371
EISBN: 978-1-62708-173-3
... Abstract Electroslag welding (ESW) and electrogas welding (EGW) are two related procedures that are used to weld thick-section materials in the vertical or near-vertical position between retaining shoes. This article discusses the fundamentals of the electroslag process in terms of heat flow...
Image
Published: 31 October 2011
Fig. 11 Schematic illustration of the electrogas welding process used for heavy deposition welding in position or in a vertical plane using special tooling (as shown). Source: Ref 2 More
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
... welding processes. The article also describes failure origins in other welding processes, such as electroslag welds, electrogas welds, flash welds, upset butt welds, flash welds, electron and laser beam weld, and high-frequency induction welds. arc welding brittle fracture electrogas welds...
Book Chapter

By Ronald B. Smith
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001432
EISBN: 978-1-62708-173-3
..., electrogas welding, electroslag welding, and stud arc welding. arc welding carbon steel electrogas welding electroslag welding flux-cored arc welding gas-metal arc welding gas-tungsten arc welding heat-affected zone hydrogen-induced cracking lamellar tearing mechanical properties plasma arc...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003206
EISBN: 978-1-62708-199-3
... Abstract Arc welding methods can be classified into shielded metal arc welding, flux-cored arc welding, submerged arc welding, gas metal arc welding, gas tungsten arc welding, plasma arc welding, plasma-metal inert gas (MIG) welding, and electroslag and electrogas welding. This article provides...
Image
Published: 01 December 1998
Fig. 21 Comparison of primary components of two vertical welding processes in which molten weld pools are confined by cooling shoes. (a) Electroslag welding. (b) Electrogas welding More
Image
Published: 01 January 1993
Fig. 15 Schematics comparing primary components of two vertical welding processes in which molten weld pools are confined by cooling shoes. (a) Electroslag welding. (b) Electrogas welding More
Image
Published: 31 October 2011
Fig. 21 Schematics comparing primary components of two vertical welding processes in which molten weld pools are confined by cooling shoes. (a) Electroslag welding. (b) Electrogas welding (EGW) More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003205
EISBN: 978-1-62708-199-3
... welding) Gas tungsten arc welding (GTAW), which is also commonly referred to as TIG welding (or tungsten inert gas welding) Plasma arc welding (PAW) Plasma-MIG welding Electrogas welding (EGW) Stud arc welding (SW) Of these, the shielded metal arc welding process is the most widely...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005647
EISBN: 978-1-62708-174-0
... electrogas welding ELI extra-low interstitial emf electromotive force EPA Environmental Protection Agency EPFM elastic-plastic fracture mechanics EPRI Electric Power Research Institute Eq equation ESW electroslag welding et al. and others ETP. electrolytic tough pitch...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0005663
EISBN: 978-1-62708-173-3
... candela Center form during heating CE carbon equivalent EGW electrogas welding cgs centimeter-gram-second (system of units) ELI extra-low interstitial AC3 temperature at which transformation of cm centimeter emf electromotive force ferrite to austenite is completed during CMC ceramic-matrix composite EPA...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005643
EISBN: 978-1-62708-174-0
... can be a problem. Electrogas welding (EGW)/electroslag welding (ESW): Limited to vertical or near-vertical. O.K. outside. Fair portability. Used on plate 9.5 to 102 mm ( 3 8 to 4 in. thick). High joint-completion rate. High deposition efficiency (solid wires 99%, cored wires lower...
Book Chapter

By Robert W. Messler, Jr.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005552
EISBN: 978-1-62708-174-0
... (GMAW) Shielded metal arc welding (SMAW) Flux-cored arc welding (FCAW) Submerged arc welding (SAW) Electrogas welding (EGW) Electroslag welding (ESW) Only GTAW, PAW, GMAW, SMAW, FCAW, and SAW are described here. The reader interested in other processes or desiring more details...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005631
EISBN: 978-1-62708-174-0
... arc tungsten welding (GTAW) X … X X X … X Electrogas welding (EGW) X … X X X X X Gas metal arc welding (GMAW) X … X X X X X Flux cored arc welding (FCAW) X X X X X X X Shielded metal arc welding (SMAW) X X X X X X X Carbon arc welding (CAW) X X X X...
Book Chapter

By F.J. Winsor
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001433
EISBN: 978-1-62708-173-3
... processes can be used with low-alloy steels. Shielded metal arc, gas-tungsten arc, gas-metal arc, flux-cored arc, and submerged arc welding processes are used for most applications. Electroslag and electrogas processes can be used to weld some of the low-alloy structural and pressure vessel steels...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005646
EISBN: 978-1-62708-174-0
... wetting by the welding circuit through which current is con- backing shoe A nonconsumable backing device solder. ducted and which terminates at the arc. used in electroslag and electrogas welding. actual throat The shortest distance between the arc welding gun A device used in semiauto- weld root...
Book

Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.9781627081733
EISBN: 978-1-62708-173-3
Book

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001337
EISBN: 978-1-62708-173-3
... arc welding (GMAW-P) • … Flux-cored arc welding (FCAW) … • Submerged arc welding (SAW) … • Electrogas welding (EGW) • • Electroslag welding (ESW) … • Plasma arc welding (PAW) • … Carbon arc cutting (CAC) • • Plasma arc cutting (PAC) • … Alternating Current...