EISBN: 978-1-62708-182-5
... Abstract This article reviews the fundamentals of electrochemical corrosion test methods. The features and requirements of the instrumentation needed for an electrochemical test are briefly discussed. The article provides a discussion on the various electrochemical techniques and tests...
Image
Published: 01 January 1990
Fig. 22 Schematics showing how electrochemical tests can indicate the susceptibility to pitting of a material in a given environment. (a) Specimen has good resistance to pitting. (b) Specimen has poor resistance to pitting. In both cases, attack occurs at the highest potentials. Source: Ref More
Image
Published: 01 January 2005
Fig. 20 Schematics showing how electrochemical tests can indicate the susceptibility to pitting of a material in a given environment. (a) Specimen has good resistance to pitting. (b) Specimen has poor resistance to pitting. In both cases, attack occurs at the highest potentials. Source: Ref More
Image
Published: 01 January 2000
Fig. 13 Environmental fatigue test chamber for electrochemical 20 kHz testing More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003586
EISBN: 978-1-62708-182-5
...) techniques. Gravimetric determination of mass loss, electrical-resistance methods, magnetic methods, quartz crystal microbalance method, solution analysis methods, and metrological methods are nonelectrochemical methods. The article presents an electrochemical test that examines the susceptibility...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003663
EISBN: 978-1-62708-182-5
..., and laboratory testing methods of evaluating galvanic corrosion. The laboratory tests fall into two categories, namely, electrochemical tests and specimen exposures. component testing computer scale modeling electrochemical testing galvanic corrosion laboratory testing method physical scale modeling...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005730
EISBN: 978-1-62708-171-9
... Abstract This article describes the two commonly used standardized tests for determining the mechanical properties of thermal spray coatings: hardness testing and tensile adhesion testing. It discusses the destructive and non-destructive methods of residual-stress measurement. Electrochemical...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003662
EISBN: 978-1-62708-182-5
...-crevice assembly tests, cylindrical materials and products evaluation, component testing, electrochemical tests, and mathematical modeling. crevice corrosion localized corrosion multiple-crevice assembly testing cylindrical material component testing electrochemical testing mathematical...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006113
EISBN: 978-1-62708-175-7
... Abstract This article reviews various test methods used for evaluating the corrosion resistance of powder metallurgy stainless steels. These include immersion testing, salt spray testing, and electrochemical testing. The article discusses the factors that affect corrosion resistance of sintered...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003593
EISBN: 978-1-62708-182-5
... by the combustion of fossil fuels. It explains how salt chemistry, including acid/base and oxidizing properties, affects corrosion rates and mechanisms. The article also provides information on electrochemical testing and explains how Pourbaix methods, normally associated with aqueous corrosion, can be used...
Image
Published: 30 September 2015
Fig. 12 Electrochemical impedance spectroscopy test data. Interpretation of data is based on this scale for coating impedance. Courtesy of Corrosion Probe, Inc. More
Image
Published: 30 September 2015
Fig. 38 Electrochemical impedance spectroscopy (a) test equipment and (b) design illustration. Courtesy of KTA-Tator, Inc. More
Image
Published: 01 January 2003
Fig. 3 Electrochemical polarization tests of titanium and titanium-base alloys, including Ti-6%Al-4%V (Ti-6-4), Ti-15%Mo-3%Nb-3%Al (Ti-15-3-3), Ti-13%Nb-13%Zr (Ti-13-13), Ti-55%Ni, and commercially pure (CP) titanium (grade 2), revealed that titanium and titanium-base alloys are spontaneously More
Image
Published: 01 January 2003
Fig. 4 Electrochemical polarization tests of titanium and titanium-base alloys, including Ti-6%Al-4%V (Ti-6-4), Ti-15%Mo-3%Nb-3%Al (Ti-15-3-3), Ti-13%Nb-13%Zr (Ti-13-13), Ti-55%Ni, and commercially pure (CP) titanium (grade 2), in a deaerated 5 M HCl solution. The potentiodynamic scans were More
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005683
EISBN: 978-1-62708-198-6
... body fluids, very complex solutions containing electrolytes and nonelectrolytes, inorganic and organic constituents, and gases. The article describes the fundamentals of electrochemical corrosion testing and provides a brief discussion on various types of corrosion tests. It illustrates corrosion...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001296
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the testing and typical corrosion behavior of coating-substrate systems in aqueous solutions and humid aggressive atmospheres. It includes a short review of the fundamentals of corrosion, followed by a discussion of specific system behavior, electrochemical...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003661
EISBN: 978-1-62708-182-5
... from which surgical implants will be produced ( Ref 2 ). This is an electrochemical potentiostatic screening test that is used to rank surgical implant alloys in order of their resistance to localized corrosion in a 0.9% NaCl solution at 37 ± 1 °C (98.6 ± 1.8 °F) (average human body temperature). Using...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004206
EISBN: 978-1-62708-184-9
.... The article discusses the surface characteristics and electrochemical behavior of metallic biomaterials. It summaries the clinical context for mechanically assisted corrosion and describes mechanically assisted crevice corrosion. There have been several tests developed to investigate aspects of mechanically...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003656
EISBN: 978-1-62708-182-5
... in the system. This method is in its infancy; its acceptance as an on-line sensor in the field remains to be tested in the future. Electrochemical Biofilm Activity Sensor Microbially induced localized penetration of materials can occur due to a combination of microbially mediated electrochemical...
Book Chapter

By R.G. Kelly
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003613
EISBN: 978-1-62708-182-5
... for crevice corrosion on each side of the coupon. By applying a consistent torque, several replicate samples can be used to develop a statistical basis for comparison of alloy resistance. Fig. 8 Various views of the multiple-crevice assembly. Source: Ref 11 Electrochemical Testing...