1-20 of 434 Search Results for

electrochemical precipitation

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006483
EISBN: 978-1-62708-207-5
... Abstract This article describes the Bayer process for the purification of alumina. The process includes four major stages: digestion, clarification, precipitation, and calcination. The article discusses the aluminum electrolytic process in terms of aluminum electrolysis cell design...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002164
EISBN: 978-1-62708-188-7
... Abstract Shaped tube electrolytic machining (STEM) is a modified electrochemical machining (ECM) process that uses an acid electrolyte so that the removed metal goes into the solution instead of forming a precipitate. This article lists some specific machining applications of the STEM process...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
..., austenitic, duplex, and precipitation-hardenable alloys. The article examines the role of additives, such as sulfur, selenium, tellurium, lead, bismuth, and certain oxides, in improving machining performance. It provides ways to minimize difficulties involved in the traditional machining of stainless steels...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002471
EISBN: 978-1-62708-194-8
... Abstract This article discusses the principles of corrosion and the basis of the various prevention measures that can be taken for different corrosion modes. It describes aqueous corrosion phenomena in terms of the electrochemical reactions that occur at the metal-environment interface...
Image
Published: 01 January 1993
Fig. 4 Depleted regions adjacent to precipitates. These regions cause an electrochemical potential (E) difference that can promote localized corrosion at the microstructural level. More
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002160
EISBN: 978-1-62708-188-7
... Abstract Electrochemical machining (ECM) is the controlled removal of metal by anodic dissolution in an electrolytic cell in which the workpiece is the anode and the tool is the cathode. This article begins with a description of the ECM system and then discusses the primary variables...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006087
EISBN: 978-1-62708-175-7
... Abstract This article provides a discussion on the process descriptions, processing conditions, and processing variables of the most common chemical methods for metal powder production. These methods include oxide reduction, precipitation from solution, and thermal decomposition. Methods...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006545
EISBN: 978-1-62708-210-5
..., microstructural features (dislocation networks, inhibition of recrystallization, precipitation patterns) also are important factors that influence SCC resistance. Nonetheless, there is general agreement that for aluminum the electrochemical factor predominates, and the electrochemical theory continues...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003599
EISBN: 978-1-62708-182-5
... Abstract Electrochemical refining is the purification process for producing commercially pure metals from crude metals. This article describes the principles of electrochemical reactions. It discusses the physical properties of the basic components of electrochemical refining cell. The article...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003606
EISBN: 978-1-62708-182-5
... of atmospheric factors, climatic conditions, and air-chemical pollutants that determine the corrosiveness of the atmosphere and contribute to the metal corrosion process are discussed. The article reviews the phenomenon of precipitation runoff on the corroded metal surface and the corrosive microbial effect...
Book Chapter

By Jerome Kruger
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003585
EISBN: 978-1-62708-182-5
..., structure, electronic properties, and mechanical properties. The article outlines three possible processes that can form passive films: direct film formation, dissolution precipitation, and anodic oxidation of metal ions in solution. It describes the breakdown of the passive film using various models...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003124
EISBN: 978-1-62708-199-3
... and submicroscopic scales, the electrochemical properties develop point-to-point nonuniformities that account for changes in corrosion resistance. Measurements of changes in physical and electrochemical properties have played an important role in completely describing precipitation reactions and are very useful...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003618
EISBN: 978-1-62708-182-5
... particles generally formed from trace impurity elements that play a predominant role in pitting corrosion. The second category comprises the effects from precipitation of secondary phases and effects from solute remaining in solid solution on corrosion of aluminum. metallurgical effects corrosion...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003617
EISBN: 978-1-62708-182-5
... are precipitated at the grain boundaries. These carbides contain more chromium than the matrix does. The precipitation of the carbides depletes the matrix of chromium adjacent to the grain boundary. The diffusion rate of chromium in austenite is slow at the precipitation temperatures; therefore, the depleted...
Book Chapter

By Jude Mary Runge
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006523
EISBN: 978-1-62708-207-5
... Abstract Anodizing produces a uniform, continuous, highly ordered network of individual cells comprising a layer whose thickness and cell dimensions, and ultimately engineering properties, depend on the electrochemical parameters of the anodizing process. This article discusses the nucleation...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003615
EISBN: 978-1-62708-182-5
... Abstract This article provides an introduction on the metal side of the corrosion reaction and describes a wide range of metallurgical factors that influence corrosion. corrosion metallurgical factors THE FUNDAMENTAL UNDERSTANDING of electrochemical corrosion kinetics is based...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.9781627081825
EISBN: 978-1-62708-182-5
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003718
EISBN: 978-1-62708-182-5
... of microvoids amount of segregation. Grain-boundary seg- electrochemical noise. Fluctuations in potential along the fracture path. The fracture surface regation of the chromium-rich precipitates in- or current, or both, originating from the un- of such a ductile fracture appears dimpled creases strength...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003597
EISBN: 978-1-62708-182-5
... Abstract Specific machining processes that employ electrochemical machining technology include deburring and deep-hole drilling. This article describes the principle and applications of electrochemical deburring as well as the machine tools used in the process. The system, process capabilities...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003616
EISBN: 978-1-62708-182-5
... crystallographic types. Often, there is one predominant phase, known as the matrix, and other secondary phases, called precipitates. The presence of these kinds of inhomogeneities often results in the alloy having radically different mechanical properties and chemical reactivities than the pure constituent...