Skip Nav Destination
Close Modal
By
Mohammed Maniruzzaman, Xiaolan Wang, Richard D. Sisson, Jr.
By
Anne E. Miller, Paul B. Fischer, Allen D. Feller, Tatyana N. Andryushchenko, Kenneth C. Cadien
By
R. Terrence Webster
By
Jude Mary Runge, John Weritz
By
Bernard S. Covino, Jr., Sophie J. Bullard
By
S.R. Freeman
By
R.G. Buchheit, A.E. Hughes
Search Results for
electrochemical cleaning
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 454
Search Results for electrochemical cleaning
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Cleaning of Steel for Heat Treatment
Available to PurchaseSeries: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005777
EISBN: 978-1-62708-165-8
..., mechanical, chemical, and electrochemical and their effectiveness and applicability. The mechanical cleaning methods include grinding, brushing, steam or flame jet cleaning, abrasive blasting, and tumbling. Solvent cleaning, emulsion cleaning, alkaline cleaning, acid cleaning, pickling, and descaling...
Abstract
This article provides an overview of surface contaminants that may affect the heat treatment processes and end-product quality. It presents information on the chemicals used to clean different surface contaminants of steels. The article discusses three types of cleaning methods, namely, mechanical, chemical, and electrochemical and their effectiveness and applicability. The mechanical cleaning methods include grinding, brushing, steam or flame jet cleaning, abrasive blasting, and tumbling. Solvent cleaning, emulsion cleaning, alkaline cleaning, acid cleaning, pickling, and descaling are chemical cleaning methods. The electrochemical cleaning methods include electropolishing, electrolytic alkaline cleaning, and electrolytic pickling. The article provides information on cleanliness measurement methods such as qualitative tests and quantitative tests to ensure product quality. Health hazards that may be associated with each cleaning method and the general control measures to be used for each hazard are tabulated.
Book Chapter
Surface Engineering of Nonferrous Metals
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003221
EISBN: 978-1-62708-199-3
..., electrochemical cleaning, mechanical cleaning, and mass finishing. It also examines coating processes such as plating, anodizing, chemical conversion coating, and thermal spray, and concludes with a discussion on oxidation-resistant coatings for refractory metals. anodizing barrel burnishing buffing...
Abstract
This article discusses surface engineering of nonferrous metals including aluminum and aluminum alloys, copper and copper alloys, magnesium alloys, nickel and nickel alloys, titanium and titanium alloys, zirconium and hafnium, zinc alloys, and refractory metals and alloys. It describes various techniques to improve functional surface properties and enhance the appearance of product forms. The article discusses various cleaning and finishing techniques such as abrasive blast cleaning, polishing and buffing, barrel burnishing, chemical cleaning, pickling, etching and bright dipping, electrochemical cleaning, mechanical cleaning, and mass finishing. It also examines coating processes such as plating, anodizing, chemical conversion coating, and thermal spray, and concludes with a discussion on oxidation-resistant coatings for refractory metals.
Book Chapter
Surface Engineering of Copper and Copper Alloys
Available to PurchaseBook: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
... and bright dipping, abrasive blast cleaning, chemical and electrochemical cleaning, mass finishing, polishing and buffing, electroless plating, immersion plating, electroplating, passivation, coloring, and organic coatings. abrasive blast cleaning bright dipping buffing chemical cleaning cleaning...
Abstract
The selection of surface treatments for copper and copper alloys is generally based on application requirements for appearance and corrosion resistance. This article describes cleaning, finishing, and coating processes for copper and copper alloys. These processes include pickling and bright dipping, abrasive blast cleaning, chemical and electrochemical cleaning, mass finishing, polishing and buffing, electroless plating, immersion plating, electroplating, passivation, coloring, and organic coatings.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003596
EISBN: 978-1-62708-182-5
... Abstract This article discusses four subsystems of the electrochemical machining (ECM) system: power source, electrolyte cleaning and supply system, tool and tool-feed system, and workpiece and workpiece-holding system. It describes the theory of ECM and provides information on the electrolytes...
Abstract
This article discusses four subsystems of the electrochemical machining (ECM) system: power source, electrolyte cleaning and supply system, tool and tool-feed system, and workpiece and workpiece-holding system. It describes the theory of ECM and provides information on the electrolytes used in ECM. The article reviews the methods associated with workpiece shape prediction. The procedures and integrated approach for the tool design in ECM are discussed. The article also explains the process control, capabilities, and the limitations of ECM. It concludes with information on the applications of ECM.
Book Chapter
Corrosion Characteristics of Carbon and Alloy Steels
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003105
EISBN: 978-1-62708-199-3
... Abstract Corrosion of metals is defined as deterioration caused by chemical or electrochemical reaction of the metal with its environment. This article provides information on corrosion of iron and steel by aqueous and nonaqueous media. It discusses the corrosive environments of carbon...
Abstract
Corrosion of metals is defined as deterioration caused by chemical or electrochemical reaction of the metal with its environment. This article provides information on corrosion of iron and steel by aqueous and nonaqueous media. It discusses the corrosive environments of carbon and alloy steels, namely atmospheric corrosion, soil corrosion, corrosion in fresh water and seawater. The article describes the corrosion process in concrete, which tends to create conditions that increase the rate of attack. The focus is on the stress-corrosion cracking of steels; an environmentally induced crack propagation that results from the combined interaction of mechanical stress and corrosion reactions. The article tabulates a guide on corrosion prevention for carbon steels in various environments. It also discusses protection methods of steel from corrosion, including coatings, such as temporary protection, cleaning, hot dip coating, electroplating, thermal spray coatings, conversion coatings, thin organic coatings, and inhibitors.
Book Chapter
Chemical-Mechanical Planarization for Semiconductors
Available to PurchaseSeries: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003600
EISBN: 978-1-62708-182-5
..., and integrated cleaning units. Discussion of these variations is beyond the scope of this article. Fig. 4 Schematic of chemical-mechanical planarization setup By definition, CMP consists of both mechanical and chemical components. The mechanical wafer environment during CMP consists of the pad...
Abstract
Chemical-mechanical planarization (CMP) of metals is described as mechanically accelerated corrosion, erosion corrosion, or metallic corrosion enhanced by wear. This article reviews the history, process, chemistry, electrochemistry, and defect issues for CMP. It provides an overview of CMP through a schematic illustration of CMP process equipment. The applications of CMP to tungsten and copper alloys are of prime interest in the semiconductor industry. The article discusses copper CMP and tungsten CMP in detail and analyzes polishing mechanism during CMP by application of direct current potentiodynamic polarization and alternating current impedance measurements. It concludes with information on chemically induced defects such as pitting corrosion, galvanic corrosion, and chemical etching.
Image
Schematic cross section of the surface of a cast iron component as it is mo...
Available to PurchasePublished: 01 January 1994
Fig. 1 Schematic cross section of the surface of a cast iron component as it is modified by cleaning in a molten salt bath. (a) As-cast. Note surface scale, burned-in core/mold sand particles, and flake graphite extending to surface. (b) After first reduction cycle. Exposed sand particles have
More
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002160
EISBN: 978-1-62708-188-7
... the effects of valence, work metal density, and other factors. Cleaning Cleaning of the workpiece is nearly always necessary after electrochemical machining. Cleaning should be done before any residue has hardened on the work. A rinse in water may be all that is needed for metals that resist corrosion...
Abstract
Electrochemical machining (ECM) is the controlled removal of metal by anodic dissolution in an electrolytic cell in which the workpiece is the anode and the tool is the cathode. This article begins with a description of the ECM system and then discusses the primary variables that affect current density and the material removal rate in the ECM process. It reviews the various characteristics of electrolytes and considers tool material and design. It also provides an overview of the properties of the workpiece and defines the surface finish and accuracy of an electrochemically machined sample. The variety of work done by electrochemical machining is also exemplified in the article.
Book Chapter
Surface Engineering of Zirconium and Hafnium
Available to PurchaseBook: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001312
EISBN: 978-1-62708-170-2
... Abstract Zirconium and hafnium surfaces require cleaning and finishing for reasons such as preparation for joining, heat treatment, plating, forming, and producing final surface finishes. This article provides information on various surface treatment processes, surface soil removal, blast...
Abstract
Zirconium and hafnium surfaces require cleaning and finishing for reasons such as preparation for joining, heat treatment, plating, forming, and producing final surface finishes. This article provides information on various surface treatment processes, surface soil removal, blast cleaning, chemical descaling, pickling or etching, anodizing, autoclaving, polishing, buffing, vapor phase nitriding, and electroplating. Applications of these surface treatment processes are also reviewed.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003660
EISBN: 978-1-62708-182-5
... of suitable test specimens, planning of the experimental technique, posttest sample cleaning, data acquisition, and reporting. It further discusses the test variables addressed during the experimental planning and provides an overview of the other test and evaluation methods of evaluating uniform corrosion...
Abstract
Uniform corrosion refers to the attack on an exposed metal surface that results in homogeneous thickness loss that is evaluated by mass loss or measurement of thickness change. This article focuses on the various processes involved in mass loss tests, namely, selection and preparation of suitable test specimens, planning of the experimental technique, posttest sample cleaning, data acquisition, and reporting. It further discusses the test variables addressed during the experimental planning and provides an overview of the other test and evaluation methods of evaluating uniform corrosion.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003597
EISBN: 978-1-62708-182-5
.... The hydroxides removed during ECD can be safely used as a raw material for the lapping paste. The components should be thoroughly washed before deburring, and properly cleaned after deburring ( Ref 2 ). Electrochemical Deep-Hole Drilling Deep small holes are required in many applications, such as turbine...
Abstract
Specific machining processes that employ electrochemical machining technology include deburring and deep-hole drilling. This article describes the principle and applications of electrochemical deburring as well as the machine tools used in the process. The system, process capabilities, and applications of electrochemical deep-hole drilling are also discussed. The article also reviews the pulse electrochemical machining.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004173
EISBN: 978-1-62708-184-9
... Abstract This article focuses on the various types of corrosion-related failure mechanisms and their effects on passive electrical components. The types include halide-induced corrosion, organic-acid-induced corrosion, electrochemical metal migration, silver tarnish, fretting, and metal...
Abstract
This article focuses on the various types of corrosion-related failure mechanisms and their effects on passive electrical components. The types include halide-induced corrosion, organic-acid-induced corrosion, electrochemical metal migration, silver tarnish, fretting, and metal whiskers. The passive electrical components include resistors, capacitors, wound components, sensors, transducers, relays, switches, connectors, printed circuit boards, and hardware.
Book Chapter
Metallurgy Basics for Aluminum Surface Treatment
Available to PurchaseSeries: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006522
EISBN: 978-1-62708-207-5
..., which are manifested in processes such as cleaning, brightening, etching, conversion coatings, electroplating, and anodizing. Point defects such as vacancies and dislocations agglomerate and accumulate at grain boundaries, which change the interfacial energy and confound the electrochemical reaction...
Abstract
This article discusses the properties of aluminum surface and the applications of aluminum alloys. It explains the effects of trace elements on aluminum alloys. The article considers microstructural development of aluminum in terms of the surface and explains how it will impact corrosion resistance and surface treatment. It describes the thermodynamics of equilibrium oxidation processes and non-equilibrium corrosion processes. The article provides a discussion on aluminum oxidation under atmospheric and dynamic conditions. It presents the potential/pH (Pourbaix) diagram for aluminum under atmospheric and dynamic conditions. The article also explains the polarization effects during the formation of stable aluminum oxide under dynamic conditions. It concludes with information on the designation system for aluminum finishes.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003598
EISBN: 978-1-62708-182-5
... Abstract This article provides a discussion on a working principle, the operations, characteristics, capabilities, and applications of electrochemical grinding (ECG). The basic elements of the ECG machine tool are also presented. electrochemical grinding machine tools HYBRID...
Abstract
This article provides a discussion on a working principle, the operations, characteristics, capabilities, and applications of electrochemical grinding (ECG). The basic elements of the ECG machine tool are also presented.
Book Chapter
Corrosion Rate Probes for Soil Environments
Available to PurchaseSeries: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004117
EISBN: 978-1-62708-184-9
... Abstract This article explores the use of the electrochemical and nonelectrochemical techniques for measuring the corrosion behavior of buried metals and the types of probes used. The electrical resistance technique is the main nonelectrochemical technique used for measuring corrosion rate...
Abstract
This article explores the use of the electrochemical and nonelectrochemical techniques for measuring the corrosion behavior of buried metals and the types of probes used. The electrical resistance technique is the main nonelectrochemical technique used for measuring corrosion rate. Electrochemical techniques discussed include linear polarization resistance, electrochemical noise, harmonic distortion analysis, electrochemical impedance spectroscopy, and hydrogen permeation. The principles of operation for the corrosion measuring techniques are described along with examples of their use in soils.
Book Chapter
Analysis and Prevention of Corrosion-Related Failures
Available to PurchaseSeries: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... Abstract This article provides an overview of the electrochemical nature of corrosion and analyzes corrosion-related failures. It describes corrosion failure analysis and discusses corrective and preventive approaches to mitigate corrosion-related failures of metals. These include: change...
Abstract
This article provides an overview of the electrochemical nature of corrosion and analyzes corrosion-related failures. It describes corrosion failure analysis and discusses corrective and preventive approaches to mitigate corrosion-related failures of metals. These include: change in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive maintenance.
Book Chapter
Chromate and Chromate-Free Conversion Coatings
Available to PurchaseSeries: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003679
EISBN: 978-1-62708-182-5
... on the processing sequence, morphology, composition, and properties of CCCs. The article discusses the electrochemical impedance spectroscopy approach used for evaluating conversion coatings. The test methods for various CCCs properties are also reviewed. The article examines the various coatings associated...
Abstract
Chromate conversion coatings (CCCs) are primarily used to improve adhesion of subsequently applied organic coatings or to impart corrosion resistance during atmospheric exposure. This article describes the factors that affect the formation of CCCs. It provides information on the processing sequence, morphology, composition, and properties of CCCs. The article discusses the electrochemical impedance spectroscopy approach used for evaluating conversion coatings. The test methods for various CCCs properties are also reviewed. The article examines the various coatings associated with chromate-free conversion. These include: titanium and zirconium fluorocomplexes; cerium-base, manganese-base, cobalt-base, and molybdate-base conversion coatings; hydrotalcite coatings; and organic coatings.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003659
EISBN: 978-1-62708-182-5
... the coupons are also discussed. The analysis of electrical-resistance probes, sentry holes, side-stream loop, electrochemical noise, hydrogen-probe, and process streams are used to monitor and estimate corrosion rates. The corrosion rates can also be estimated by ultrasonic thickness measurements...
Abstract
This article describes the criteria for selecting a corrosion-monitoring method used in industrial plants. It provides a detailed discussion on the design, advantages, and disadvantages of plant corrosion-testing program. The basic types of racks used to support and insulate the coupons are also discussed. The analysis of electrical-resistance probes, sentry holes, side-stream loop, electrochemical noise, hydrogen-probe, and process streams are used to monitor and estimate corrosion rates. The corrosion rates can also be estimated by ultrasonic thickness measurements, polarization-resistance measurements, corrosion potential measurements, and alternating current impedance measurements. Corrosion monitoring strategies, such as locations, data analysis, redundancy, and other issues, are discussed. The article concludes with information on the interpretation and reporting of corrosion testing.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001225
EISBN: 978-1-62708-170-2
... Abstract Molten salt baths are anhydrous, fused chemical baths used at elevated temperatures for a variety of industrial cleaning applications. This article discusses their applications in paint stripping, polymer removal, casting cleaning, glass removal, and plasma/flame spray removal...
Abstract
Molten salt baths are anhydrous, fused chemical baths used at elevated temperatures for a variety of industrial cleaning applications. This article discusses their applications in paint stripping, polymer removal, casting cleaning, glass removal, and plasma/flame spray removal. It provides an overview of the basic design and safety considerations of the salt bath equipment and describes the environmental impact of molten salt bath cleaning.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003599
EISBN: 978-1-62708-182-5
... Abstract Electrochemical refining is the purification process for producing commercially pure metals from crude metals. This article describes the principles of electrochemical reactions. It discusses the physical properties of the basic components of electrochemical refining cell. The article...
Abstract
Electrochemical refining is the purification process for producing commercially pure metals from crude metals. This article describes the principles of electrochemical reactions. It discusses the physical properties of the basic components of electrochemical refining cell. The article also explains the engineering considerations required in the refining process. Theoretical and technological principles of electrochemical refining are illustrated, with examples.