EISBN: 978-1-62708-171-9
... 2540 4600 0.31 1.00 4.63 15.20 5.3 14.0 Propane C 3 H 8 1.550 1.858 0.116 101,943 2736 2817 5102 0.46 1.52 3.72 12.20 3.4 13.8 Propylene C 3 H 6 1.476 1.778 0.111 93,895 2520 2924 5295 … … … … 2.0 11.1 Electric arc spray rates for various materials...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001282
EISBN: 978-1-62708-170-2
... 65–130 200–400 Wire flame spray Metallic coatings Wire Grit blasting or rough threading 95–135 200–275 230–295 700–900 Ceramic rod spray Ceramic and cermet coatings Rod Grit blasting 95–135 200–275 260–360 800–1100 Two-wire electric-arc Metallic coatings Wire Grit blasting...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005706
EISBN: 978-1-62708-171-9
...-fed flame spray, wire- or rod-fed flame spray, electric arc spray, plasma arc spray, vacuum plasma spray, high-velocity oxyfuel spray, detonation gun deposition, and cold spray, and their advantages. It provides details on the microstructural characteristics of thermal spray coatings. The article also...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006301
EISBN: 978-1-62708-179-5
... such as electrical resistance welding and thermite welding. It reviews thermal spraying processes, such as flame spraying, arc spraying, and plasma spraying, of a cast iron. arc spraying braze welding cast iron ductile iron electrical resistance welding flame spraying flux cored arc welding fusion...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005717
EISBN: 978-1-62708-171-9
... amount of fumes. Electric arc spray produces more fumes per unit mass and time than most other thermal spray processes, because of the high spray rates and the nature of the arc/wire relationship. To accommodate the increased demands of electric arc spray, dust collectors are designed with a 0.5-to-1...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005740
EISBN: 978-1-62708-171-9
... manufacturers. Thermal spray coating by wire electric arc spraying was adopted in 2006, and by wire plasma spraying ( Ref 9 , 10 ) in 2009. Of note is that thermal spray equipment specialized for thermal spraying of the controlled functional coating onto cylinder bores has been developed to the point...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002494
EISBN: 978-1-62708-194-8
..., passivation, thermal spraying, electric arc spraying Allow for electrical contact to be made on nonsignificant surfaces or use a conductive screen Elecroplating, electropolishing, anodizing, electrocleaning, electrocoating, electropolymerization, electrophoretic plating, ion implantation, ion plating...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005719
EISBN: 978-1-62708-171-9
... spray systems where gas and air pressures, gas flows, and wire speed are all set and maintained by the operator. An example of this type of control for plasma spray would include voltage, current, gas pressure, and gas flow. With electric arc spray the controls are simply voltage, current, and atomizing...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005755
EISBN: 978-1-62708-171-9
.... Courtesy of Thermal Spray Technologies Fig. 4 Plasma-sprayed yttria-stabilized zirconia on vacuum-plasma sprayed NiCrAlY. Courtesy of Drexel University Fig. 5 Electric-arc-sprayed low-carbon steel. Courtesy of Thermal Spray Technologies Figures 4 and 5 show micrographs...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005713
EISBN: 978-1-62708-171-9
... to impact, spread (if molten), and solidify. The results were coatings that were incrementally formed from impacting droplets. Electric arc spray was also patented by Schoop in approximately 1908, which enabled more metals to be sprayed. Steel, stainless steel, and zinc by wire-arc metallizing advanced...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005756
EISBN: 978-1-62708-171-9
... also be required to mitigate lung hazards from respiratory dust. Light and/or ultraviolet radiation Electric arc, plasma spray, and welding Optical radiation Welding helmets or welding shields. Typical shades: 10–14. Autodimming shades as suitable Note: Skin protection to prevent...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006364
EISBN: 978-1-62708-192-4
... , 3 Nickel-base alloys Ni-Cr (Al), Ni-Al Plasma spraying Buffer layers, repair of worn surfaces 2 , 4 NiBSi/NiCrBSi Deposition welding (PTAW, FCAW, GMAW, SAW, GTMW), electric arc spraying Oil drilling equipment, piston rings, rollers, caterpillar teeth, excavator shovels, high wear...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005725
EISBN: 978-1-62708-171-9
... Flame wire X X Flame powder X X APS X X High-velocity plasma X X VPS X X Electric wire arc X X High-velocity oxyfuel X X Detonation gun X X Cold spray X X (a) Particle speed ranges from a high of approximately...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003832
EISBN: 978-1-62708-183-2
... sprayed onto large structures using flame and electric arc-based processes, and with the coating material supplied in wire form to the spray gun. There are standards for the composition and diameter of these wires: ISO 14919 ( Ref 1 ) and AWS C2.25/C2.25M ( Ref 2 ). Among these, four classes of materials...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005746
EISBN: 978-1-62708-171-9
... Produced by Various Thermal Spray Processes M. Shibata, S. Kuroda, M. Watanabe, H. Murakami, M. Ode, and Y. Sakamoto Proceedings of the 2006 International Thermal Spray Conference 2006 Scientific, Technological and Economic Aspects of Rapid Tooling by Electric Arc Spray Forming P.S. Grant, S.R...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001487
EISBN: 978-1-62708-173-3
... operations. adhesive bonding arc welding brazing compressed gas handling cutting electric shock electrical safety electron-beam welding explosion welding eye protection face protection friction welding high-frequency welding laser-beam welding oxyfuel gas welding protective clothing...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.9781627081719
EISBN: 978-1-62708-171-9
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005759
EISBN: 978-1-62708-171-9
..., dBA Detonation gun 145 High-velocity oxyfuel (HVOF) liquid fuel 133 HVOF gaseous fuel 125–135 High-velocity air fuel 133 Wire flame spray 118–122 Powder flame spray 90–125 Rod flame spray gun 125 Electric arc 105–119 Air plasma spray 110–125 Vacuum plasma...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005635
EISBN: 978-1-62708-174-0
... and explosion. adhesive bonding arc welding brazing compressed gas cutting electrical safety electromagnetic radiation electron beam welding explosion prevention explosion protection explosion welding fire prevention fire protection friction welding fumes gas high-frequency welding laser...