1-20 of 235 Search Results for

eddy-current inspection

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003234
EISBN: 978-1-62708-199-3
... Abstract Eddy-current inspection is a nondestructive evaluation method based on the principles of electromagnetic induction. Eddy-current methods are used to identify or differentiate a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006450
EISBN: 978-1-62708-190-0
... Abstract Eddy-current inspection is based on the principles of electromagnetic induction and is used to identify or differentiate among a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic and nonferromagnetic metals and metal parts...
Image
Published: 01 December 1998
Fig. 3 Principal elements of a typical system for eddy current inspection of bar or tubing. See description in text. More
Image
Published: 01 December 1998
Fig. 9 Types and applications of coils used in eddy-current inspection. (a) Probe-type coil applied to a flat plate for crack detection. (b) Horseshoe-shape, or U-shape, coil applied to a flat plate for laminar-flaw detection. (c) Encircling coil applied to a tube. (d) Internal, or bobbin-type More
Image
Published: 01 December 2008
Fig. 3 Eddy current inspection. The presence of a flaw alters the magnitude of current. More
Image
Published: 01 August 2018
Fig. 3 Principal elements of a typical system for eddy-current inspection of bar or tubing. See description in text. More
Image
Published: 01 August 2018
Fig. 5 Simplified equivalent circuit (a) of an eddy-current inspection coil and the part being inspected. (b) to (d) Three impedance diagrams for three conditions of the equivalent circuit. See text for explanation. More
Image
Published: 01 August 2018
Fig. 23 Types and applications of coils used in eddy-current inspection. (a) Probe-type coil applied to a flat plate for detection of a crack. (b) Horseshoe-shaped or U-shaped coil applied to a flat plate for detection of a laminar flaw. (c) Encircling coil applied to a tube. (d) Internal More
Image
Published: 01 August 2018
Fig. 24 Arrangements of multiple coils used in eddy-current inspection, (a) absolute, (b) differential. See text for discussion. More
Image
Published: 01 August 2018
Fig. 33 Setup and encircling coil components for continuous eddy-current inspection of ferromagnetic or nonferromagnetic tubes up to about 75 mm (3 in.) in diameter More
Image
Published: 01 August 2018
Fig. 41 Setup and coil arrangement for the eddy-current inspection of longitudinal welds in ferromagnetic welded tubing More
Image
Published: 01 August 2018
Fig. 45 Low-frequency sliding-type eddy-current inspection probe used to detect cracks in the first or subsurface layers of multilayered structures. Courtesy of J. Pellicer, Staveley Instruments More
Image
Published: 01 August 2018
Fig. 53 Sealant trimming requirements for eddy-current inspection. (a) Sealant buildup that hinders detection of fatigue cracks in spar caps because probe capability is exceeded. (b) Sealant trimmed to dimension thin enough to allow probe to be positioned properly around fastener. Source: Ref More
Image
Published: 01 August 2018
Fig. 54 Eddy-current inspection of cracks located under installed bushings. (a) Schematic of typical assembly employing interference-fit bushings in a clevis/lug attachment assembly. (b) Reference standard incorporating an electrical discharge machined corner notch. (c) Probe coil positioned More
Image
Published: 01 August 2018
Fig. 55 High-frequency eddy-current inspection of surface and subsurface cracks in aircraft splice joints. (a) Calibration procedure involves introducing an electrical discharge machining notch in the reference standard to scan the fastener periphery using a circle template to guide the probe More
Image
Published: 01 August 2018
Fig. 24 Eddy current inspection for hardness testing of PM wedges at 10,000 parts/h. Source: Ref 20 More
Image
Published: 01 August 2018
Fig. 26 Rotary probe unit used for the eddy-current inspection of steel billets, and graph showing effect of position on speed as the probe unit traverses radially over one quadrant of a 102 mm (4 in.) square billet More
Image
Published: 01 August 2018
Fig. 4 Unit used for the probe-type eddy-current inspection of seamless steel tubing. A, outer cover, containing test head ( Fig. 4 ), in open position; B, one of four rotating eddy-current probe coils; C, reference-standard testpiece in position for calibration; D, one of eight paint-spray More
Image
Published: 01 August 2018
Fig. 5 Test head of the eddy-current inspection unit shown in Fig. 4 A, orifice for test pipe or tube; B, one of eight paint-spray guns for marking; C, reference-standard testpiece More
Image
Published: 01 August 2018
Fig. 3 Probability of detection (POD) curve for the automated eddy current inspection of titanium bolt holes More