Skip Nav Destination
Close Modal
Search Results for
eddy current
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 323 Search Results for
eddy current
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003234
EISBN: 978-1-62708-199-3
...Abstract Abstract Eddy-current inspection is a nondestructive evaluation method based on the principles of electromagnetic induction. Eddy-current methods are used to identify or differentiate a wide variety of physical, structural, and metallurgical conditions in electrically conductive...
Abstract
Eddy-current inspection is a nondestructive evaluation method based on the principles of electromagnetic induction. Eddy-current methods are used to identify or differentiate a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic and nonferromagnetic metals and metal parts. Giving a brief introduction on the uses of eddy-current inspection, this article discusses the operating principles and the principal operating variables encountered in eddy-current inspection, including coil impedance, electrical conductivity, magnetic permeability, lift-off and fill factors, edge effect, and skin effect. It further describes different aspects of eddy current testing such as the selection of inspection frequencies and the types and configurations of inspection coils. The article also deals with the eddy current instrumentation and the discontinuities that are detectable by eddy-current methods.
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006450
EISBN: 978-1-62708-190-0
...Abstract Abstract Eddy-current inspection is based on the principles of electromagnetic induction and is used to identify or differentiate among a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic and nonferromagnetic metals and metal...
Abstract
Eddy-current inspection is based on the principles of electromagnetic induction and is used to identify or differentiate among a wide variety of physical, structural, and metallurgical conditions in electrically conductive ferromagnetic and nonferromagnetic metals and metal parts. This article discusses the advantages and limitations of eddy-current inspection, as well as the development of the eddy-current inspection process. It reviews the principal operating variables encountered in eddy-current inspection: coil impedance, electrical conductivity, magnetic permeability, lift-off and fill factors, edge effect, and skin effect. The article illustrates some of the principal impedance concepts that are fundamental to understanding of and effective application of eddy-current inspection. It discusses various types of eddy-current instruments, such as the resistor and single-coil system, bridge unbalance system, induction bridge system, and through transmission system. The article concludes with a discussion on the inspection of aircraft structural and engine components.
Image
in Nondestructive Inspection of Steel Bar, Wire, and Billets[1]
> Nondestructive Evaluation of Materials
Published: 01 August 2018
Fig. 25 Schematics of eddy-current flow. (a) Eddy-current flow around a probe coil for a sound billet. (b) Eddy currents flowing around the seam in a defective billet, thus altering the electrical loading on the probe coil
More
Image
Published: 31 October 2011
Fig. 12 Example of array eddy current examination for a friction stir weld in an aluminum plate. (a) Photo showing friction stir weld in an aluminum specimen with locations of flaws. (b) Test results at 20 kHz. (c) Test results at 480 kHz
More
Image
Published: 01 January 2006
Image
Published: 01 August 2018
Fig. 37 Example of automated ultrasonic and eddy-current phased array system for bar inspection. Used with permission of Olympus
More
Image
Published: 01 August 2018
Fig. 1 Two common types of inspection coils and the patterns of eddy current flow generated by the exciting current in the coils. Solenoid-type coil is applied to cylindrical or tubular parts; pancake-type coil, to a flat surface.
More
Image
Published: 01 August 2018
Image
Published: 01 August 2018
Fig. 3 Principal elements of a typical system for eddy-current inspection of bar or tubing. See description in text.
More
Image
Published: 01 August 2018
Fig. 5 Simplified equivalent circuit (a) of an eddy-current inspection coil and the part being inspected. (b) to (d) Three impedance diagrams for three conditions of the equivalent circuit. See text for explanation.
More
Image
Published: 01 August 2018
Fig. 10 Variation in density of eddy current as a function of depth below the surface of a conductor—a variation commonly known as skin effect
More
Image
Published: 01 August 2018
Fig. 23 Types and applications of coils used in eddy-current inspection. (a) Probe-type coil applied to a flat plate for detection of a crack. (b) Horseshoe-shaped or U-shaped coil applied to a flat plate for detection of a laminar flaw. (c) Encircling coil applied to a tube. (d) Internal
More
Image
Published: 01 August 2018
Fig. 24 Arrangements of multiple coils used in eddy-current inspection, (a) absolute, (b) differential. See text for discussion.
More
Image
Published: 01 August 2018
Image
Published: 01 August 2018
Fig. 27 Four types of eddy current instruments. (a) A simple arrangement, in which voltage across the coil is monitored. (b) Typical impedance bridge. (c) Impedance bridge with dual coils. (d) impedance bridge with dual coils and a reference sample in the second coil
More
Image
Published: 01 August 2018
Fig. 32 Eddy current signals obtained with an internal rotating probe operating at 250 kHz for the discontinuities shown. (a) 2 mm (0.08 in.) diam radial hole. (b) OD surface narrow slit. (c) OD surface longitudinal groove. Source: Ref 9
More
Image
Published: 01 August 2018
Fig. 33 Setup and encircling coil components for continuous eddy-current inspection of ferromagnetic or nonferromagnetic tubes up to about 75 mm (3 in.) in diameter
More
Image
Published: 01 August 2018
Fig. 34 Absolute bobbin probe with flexible wafer guides used for the eddy current evaluation of heat exchanger tubesheet rolled joints
More
Image
Published: 01 August 2018
Fig. 40 Eight possible coil combinations employed in the eddy current reflection and transmission methods of inspecting nonmagnetic tubes. See text for description.
More
Image
Published: 01 August 2018
Fig. 41 Setup and coil arrangement for the eddy-current inspection of longitudinal welds in ferromagnetic welded tubing
More