Published: 01 August 2018
Fig. 32 Cold shut (at arrow) in the flange of a machined cast drum. Magnetic-particle inspection revealed faint indications of the cold shut in the rough casting. More
Image
Published: 01 January 1997
Fig. 17 Submerged arc welding setup for steam-drum shell course. Based metal: carbon steel, 0.35% max C (ASTM A 515, grade 70), normalized. Filler metals: low-carbon steel (E7018) for root passes (shielded metal arc welding); 0.5% Mo steel for remaining passes (submerged arc welding). Source More
Image
Published: 01 January 1989
Fig. 2 Typical electron beam drilling unit with a tensioning drum More
Image
Published: 01 January 2006
Fig. 24 Brake-drum back that was produced in two press operations, in a blank-and-notch die and in a restrike-and-form die. Dimensions given in inches More
Image
Published: 01 January 2000
Fig. 3 Schematic diagram of the pin-on-drum wear apparatus. Source: Ref 23 , 28 More
Image
Published: 01 January 2000
Fig. 10 Schematic diagram of impeller-in-drum impact-abrasion wear apparatus. Source: Ref 61 More
Image
Published: 01 January 1989
Fig. 14 Planetary action and cutter path of an eccentric-drum miller. (a) Internal work. (b) External work. Cutter is shown in neutral position for loading (left), in radial feed to depth (center), and in planetary feed around work (right). More
Image
Published: 01 January 2002
Fig. 4 Crack path in a failed utility boiler drum. More
Image
Published: 30 August 2021
Fig. 1 Corrosion mapping of ultrasonic thickness scans at bottom of knockout drum More
Image
Published: 30 August 2021
Fig. 27 Tubular shaft (drum tube) cut to reveal one representative disc (web plate) More
Image
Published: 30 August 2021
Fig. 6 Crack path in a failed utility boiler drum More
Image
Published: 30 August 2021
Fig. 3 Three reeving diagrams for double-drum hoists More
Image
Published: 01 January 2002
Fig. 3 Three reeving diagrams for double-drum hoists. More
Book Chapter

Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006416
EISBN: 978-1-62708-192-4
.... Gray cast iron is the dominant material for both brake drums and disk brake rotors. The article reviews brake lining chemistry effects, graphite morphology effects, and external abrasive effects on brake drums. It concludes with information on cast iron grinding balls. abrasive wear adhesive...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006374
EISBN: 978-1-62708-192-4
... conditions. The morphology effect of graphite on automotive brake drum and disk is explained. The article also describes the characteristics of specific wear rates for both normal and local cast iron in automotive brake drums and disk rotors. It provides information on noises, vibrations, and harshness...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006823
EISBN: 978-1-62708-329-4
...Abstract Abstract This article illustrates the use of the American Petroleum Institute (API) 579-1/ASME FFS-1 fitness-for-service (FFS) code (2020) to assess the serviceability and remaining life of a corroded flare knockout drum from an oil refinery, two fractionator columns affected...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005930
EISBN: 978-1-62708-166-5
..., and drive and idler drums. The article also reviews the material characteristics of silicon/silicon carbide composite and reaction-bonded silicon carbide as used in radiant tubes. chemical composition furnace parts heat-resistant alloys heat-treating furnaces high-temperature corrosion industrial...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006568
EISBN: 978-1-62708-290-7
.../Carney flow test, bulk/tap density, rheometer, and the revolving or rotating drum technique. The three categories of powder properties that are available from rheometer experiments are discussed: bulk, dynamic flow, and shear properties. The article also describes the basic principles and applications...
Book Chapter

Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006348
EISBN: 978-1-62708-179-5
... cast iron wear, local cast iron wear, and external abrasive effects on brake drums and disk brake rotors made of gray cast iron. The article concludes with a discussion on the application of cast iron for grinding balls. abrasive wear adhesive wear brake drums cast iron compacted gray iron...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006830
EISBN: 978-1-62708-329-4
...Abstract Abstract The types of metal components used in lifting equipment include gears, shafts, drums and sheaves, brakes, brake wheels, couplings, bearings, wheels, electrical switchgear, chains, wire rope, and hooks. This article primarily deals with many of these metal components of lifting...