1-20 of 774

Search Results for draw rolls

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005744
EISBN: 978-1-62708-171-9
... cylinders, corona rolls, and draw rolls. blanket cylinders corona rolls draw rolls engraver rolls plate cylinders printing machines TODAY (2013), SEVERAL PRINTING TECHNIQUES are available, including offset, letterpress (flexo), and gravure printing ( Fig. 1 ). These techniques are different...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001011
EISBN: 978-1-62708-161-0
..., commercial quality, drawing quality, and drawing quality, special killed. The surface texture of low-carbon cold-rolled steel sheet and strip can be varied between rather wide limits. The modified low-carbon steel grades discussed in the article are designed to provide sheet and strip products having...
Image
Published: 01 January 2006
Fig. 13 Limit drawing ratios in dependence on as-rolled conditions. d 0 =50 mm (2 in.). Source: Ref 20 More
Image
Published: 01 January 2005
Fig. 2 Drawing of a bar through undriven rolls More
Image
Published: 01 January 2005
Fig. 25 Slip-line fields for rolling (a), drawing (b), and side pressing (c). These fields are similar to those for double indentation shown in Fig. 24 . More
Image
Published: 01 January 2005
Fig. 21 Slip-line fields for (a) rolling, (b) drawing, and (c) side pressing. These fields are similar to those for double indentation shown in Fig. 20 . More
Image
Published: 01 December 2009
Fig. 11 Slip-line fields for (a) rolling, (b) drawing, and (c) side pressing. These fields are similar to those for double indentation of a thick slab shown in Fig. 9 . More
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004030
EISBN: 978-1-62708-185-6
.... The article also provides formulas for flat rolling, conical-die extrusion, wire drawing, deep drawing of cups from sheet metal, and bending, and formulas for anisotropic sheet materials. bending conical-die extrusion deep drawing flat rolling sheet metal forming strain strain rate stress...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005181
EISBN: 978-1-62708-186-3
... yield function Yld2000-2d for plane-stress deformation of sheet material. It also contains formulas related to flat (sheet) rolling, conical-die extrusion, wire drawing, bending, and deep drawing of cups from sheet metal. arbitrary coordinates Barlat's anisotropic yield function compression...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005122
EISBN: 978-1-62708-186-3
.... The hydraulic presses ordinarily used in stretch draw forming have capacities of 1800 to 7100 kN (200 to 800 tonf). Accessory Equipment Grippers and wiping shoes or rollers are made to conform to the rolled or extruded shape that is to be stretch formed. Jaws used for gripping sheet in stretch draw...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003178
EISBN: 978-1-62708-199-3
... Abstract This article discusses the mechanics, surface preparation and principles of metal forming operations such as drawing, bending (draw bending, compression bending, roll bending, and stretch bending), spinning, and straightening of bars, tubes, wires, rods and structural shapes...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001378
EISBN: 978-1-62708-173-3
... Abstract Cold pressure welding can be accomplished by deforming in a lap or butt configuration, drawing, extrusion, and rolling. This article provides a discussion on cold pressure lap welding, cold pressure butt welding and cold pressure welding in drawing process with illustrations...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005542
EISBN: 978-1-62708-197-9
... Abstract This article is a comprehensive collection of tables containing formulas for metals processing, namely, casting and solidification, flat (sheet) rolling, conical-die extrusion, wire drawing, bending, and deep drawing. Formulas for compression, tension, and torsion testing of isotropic...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005139
EISBN: 978-1-62708-186-3
..., press-brake forming, press forming, multiple-slide forming, deep drawing, spinning, rubber-pad forming, drop hammer forming¸ three-roll forming, contour roll forming, stretch forming, and bending of tubing. bending blanking contour roll forming deep drawing drop hammer forming formability...
Book Chapter

By R.J. Glodowski
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001016
EISBN: 978-1-62708-161-0
... Abstract Wire rod is a semifinished product rolled from billet on a rod mill and is used primarily for the manufacture of wire. Steel wire rod is usually cold drawn into wire suitable for further drawing; for cold rolling, cold heading, cold upsetting, cold extrusion, or cold forging...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001059
EISBN: 978-1-62708-162-7
... Abstract Aluminum mill products are those that have been subjected to plastic deformation by hot- and cold-working mill processes such as rolling, extruding, and drawing, either singly or in combination. Microstructural changes associated with the working and with any accompanying thermal...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003177
EISBN: 978-1-62708-199-3
... or nonferrous metals. The article reviews the various types of forming processes such as blanking, piercing, fine-edge blanking, press bending, press forming, forming by multiple-slide machines, deep drawing, stretch forming, spinning, rubber-pad forming, three-roll forming, contour roll forming, drop hammer...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004031
EISBN: 978-1-62708-185-6
... Abstract This article is a comprehensive collection of terms related to metalworking operations that produce shapes from forging, extrusion, drawing, and rolling operations. drawing extrusion forging rolling ASM Handbook, Volume 14A: Metalworking: Bulk Forming Copyright © 2005 ASM...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
... requirements and applications. bending blanking contour roll forming copper alloys drawing high-velocity metal forming hydraulic forming piercing rubber-pad forming spinning stretch forming swaging COPPER AND MOST COPPER ALLOYS are readily formed at all sheet gages. The copper alloys...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005141
EISBN: 978-1-62708-186-3
... used in the forming. It also analyzes the various forming processes of aluminum alloys. The processes include blanking and piercing, bending, press-brake forming, contour roll forming, deep drawing, spinning, stretch forming, rubber-pad forming, warm forming, superplastic forming, explosive forming...