1-20 of 220 Search Results for

draw panel analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006801
EISBN: 978-1-62708-329-4
.../loose metal, and springback/dimensional. It discusses the processes involved in analytical tools that aid in characterizing the state of a formed part. In addition, information on draw panel analysis and troubleshooting of sheet forming failures is also provided. draw panel analysis fractures...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005182
EISBN: 978-1-62708-186-3
... to help limit problems during production. Although parts on day one may “hold water,” strain analysis can highlight those areas that may need some tooling work to ensure that the ordered steel or aluminum grade and the forming process, together, are sufficiently robust to produce a split-free panel over...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005150
EISBN: 978-1-62708-186-3
... material and processing variation Short die-change time (where the first part made after a die set is a good part) Work-hardening drawing steel (180 MPa, or 26 ksi, yield strength) to 350 MPa (51 ksi) yield strength on the vehicle Size consistency (to fit the panel to the subsequent dies...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003223
EISBN: 978-1-62708-199-3
.... It also discusses the concept of life-cycle analysis (LCA), a quantitative accounting of the environmental and economic costs of using a given material and the energy required to make, distribute, operate, and eventually dispose of the host product and its constituent materials. An important but often...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005151
EISBN: 978-1-62708-186-3
... analysis (including meshing, setup, calculation, and visualizing the results) of one panel (based on a front fender from Mazda) was reduced from 50 days in 1990 to approximately 10 days in 2002. Fig. 4 Reduction in lead time for simulating the stamping of an automotive panel The total...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001031
EISBN: 978-1-62708-161-0
...Abstract Abstract Steel sheet is widely used for industrial and consumer products, partly because it is relatively strong, easily joined, and readily available at moderate cost. This article discusses the mechanical properties and formability of steel sheet, the use of circle grid analysis...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002176
EISBN: 978-1-62708-188-7
...Abstract Abstract This article describes the basic functions that should be included when considering the relationship of computer-aided design (CAD)/computer-aided manufacturing (CAM) and machining. These include design, analysis, drafting, process planning, part programming, program...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005163
EISBN: 978-1-62708-186-3
... and are formed by deep drawing. High-strength steels used for this application have tensile strength of 260 to 390 MPa (38 to 57 ksi). This may include BH and HSLA grades. However, because of the limited formability of HSS, complicated inner panels cannot be formed successfully using traditional forming methods...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005141
EISBN: 978-1-62708-186-3
...Abstract Abstract This article discusses the general formability considerations of aluminum alloys. To conduct a complete analysis of a formed part, the required mechanical properties, as determined by several standard tests, must be considered. The article describes tension testing and other...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002447
EISBN: 978-1-62708-194-8
... Implementation of 3-D Tolerance Analysis , International Congress and Exposition, Instrument Panel Design Issues , SP-1068, 950858, Society of Automotive Engineers, Inc. , 1995 , p 51 – 102 10.4271/950858 • Staif J. , Dimensional Management Process Applied to Body-to-Frame Marriage...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003455
EISBN: 978-1-62708-195-5
...Abstract Abstract This article discusses the requirements for designing repairable composite structures such as a honeycomb sandwich panel construction and integrally stiffened co-cured composite structures. It reviews the general and specific design guidelines for bolted or riveted repairs...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005118
EISBN: 978-1-62708-186-3
... is necessary. Formed parts other than those produced from fully developed blanks also must undergo some trimming before they are brought to final size. Analysis of Parts to be Trimmed Trimming of a part is usually performed immediately after a drawing operation. Therefore, it is necessary to consider...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005129
EISBN: 978-1-62708-186-3
... such as the orientation of weld relative to metal movement in dies, the formability of TWB materials, die and press considerations, and specific factors for the drawing, stretching, and bending of steel tailor-welded blanks. bending drawing formability forming stretching tailor-welded blanks welding...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005168
EISBN: 978-1-62708-186-3
... alloy sheets. It explains testing procedures and analysis methods that are used to measure the relevant data needed to identify the material coefficients. The article describes the various formulations of finite element methods used in sheet metal forming process simulations. Stress-integration...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003045
EISBN: 978-1-62708-200-6
...Abstract Abstract Ultrasonic inspection is a nondestructive technique that is useful in both quality control and research applications for flaw detection in fiber-reinforced composite materials. This article describes ultrasonic nondestructive analysis by outlining its three basic types...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005540
EISBN: 978-1-62708-197-9
... efficiency and accuracy, or between locking and hourglassing, as mentioned subsequently. For forming and springback analysis, the procedure consists of applying boundary conditions (i.e., the motion of a punch or die, the action of draw beads, frictional constraints, and so on), stopping at the end...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005162
EISBN: 978-1-62708-186-3
... steels low-carbon steels metal thickness surface finish FABRICATION of sheet products includes various forming operations such as press forming, press bending, press-brake forming, stretch forming, and deep drawing. Fabrication of sheet products may also include cutting operations...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006527
EISBN: 978-1-62708-207-5
... of strain that can occur without splitting. The article reviews various bending methods, such as draw, compression, ram and press, roll, and stretch or tension bending. It describes the process variations of incremental sheet forming (ISF), such as single-point incremental forming, two-point incremental...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005149
EISBN: 978-1-62708-186-3
... testing, and simulative tests such as bending tests, stretching tests, the Ohio State University test, the drawing test, and stretch-drawing tests. It extends the correlation between simulative tests and materials properties using forming limit diagrams and circle grid analysis, and discusses...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005100
EISBN: 978-1-62708-186-3
... typically involve multidirectional deformation throughout the volume of a worked mass, as in the cases of forging, extrusion drawing, rolling, coining, sizing, and thread forming. In bulk forming, the input material is in billet, rod, or slab form, and the surface-to-volume ratio in the formed part...