Skip Nav Destination
Close Modal
Search Results for
discontinuously reinforced composites
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 342 Search Results for
discontinuously reinforced composites
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004002
EISBN: 978-1-62708-185-6
... Abstract Discontinuously reinforced aluminum (DRA) alloy metal-matrix composites (MMCs) represent an advanced aluminum materials concept whereby ceramic particles, or whiskers, are added to aluminum-base alloys through the use of either ingot-melting or casting and/or powder-metallurgy (P/M...
Abstract
Discontinuously reinforced aluminum (DRA) alloy metal-matrix composites (MMCs) represent an advanced aluminum materials concept whereby ceramic particles, or whiskers, are added to aluminum-base alloys through the use of either ingot-melting or casting and/or powder-metallurgy (P/M) techniques. This article begins with a summary of general observations on the forging of discontinuously reinforced composites. It provides information on some of the specific experimental results obtained on various DRA systems, including 2xxx DRA alloys and cast DRA alloys. The article reviews the efforts on the modeling of behavior of specific alloy systems, with a comparison of experimental results to the modeling attempts. It concludes with information on the properties of deformation-processed DRA alloys.
Image
Published: 01 January 2001
Fig. 8 Cyclic stress-strain loops for a discontinuously reinforced composite compared to unreinforced matrix alloy. (a) Stress-controlled conditions. (b) Strain-controlled conditions. Source: Ref 45
More
Image
Published: 01 December 2008
Fig. 25 Discontinuously reinforced aluminum metal-matrix composites. (a) Multi-inlet SiC p -Al truss node. (b) Gr p -Al composite components for electronic packaging applications
More
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003358
EISBN: 978-1-62708-195-5
... Abstract This article focuses on the production of particulate reinforcements that are used in discontinuously reinforced metal-matrix composite (DRMMC) materials systems, their physical and materials properties, and the particle shape and overall morphology. The most common DRMMC materials...
Abstract
This article focuses on the production of particulate reinforcements that are used in discontinuously reinforced metal-matrix composite (DRMMC) materials systems, their physical and materials properties, and the particle shape and overall morphology. The most common DRMMC materials systems used for aerospace structural applications are silicon carbide and boron carbide particulate reinforcement in an aluminum alloy matrix. The article concludes with information on reinforcement chemistry for designing DRMMC materials systems.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003399
EISBN: 978-1-62708-195-5
... of unidirectional fiber reinforced metal matrix composites (MMCs). It discusses the elastic deformation and elastic-plastic deformation analysis of discontinuously reinforced MMCs. The article provides an overview of analysis of strength, fatigue, and fracture toughness for macromechanics fiber-reinforced...
Abstract
The goal of micromechanics and analysis is to use the predictive methodology to develop tailored composites and also to make accurate predictions of their performance in service. This article reviews results derived from micromechanics analyses, based on finite-element method of unidirectional fiber reinforced metal matrix composites (MMCs). It discusses the elastic deformation and elastic-plastic deformation analysis of discontinuously reinforced MMCs. The article provides an overview of analysis of strength, fatigue, and fracture toughness for macromechanics fiber-reinforced and discontinuous reinforced composites.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
..., discontinuously reinforced composites and continuous-fiber-reinforced composites. Processing methods include cold pressing, sintering, hot pressing, reaction bonding, melt infiltration, directed metal oxidation, sol-gel and polymer pyrolysis, self-propagating high-temperature synthesis and joining. A table...
Abstract
Ceramic-matrix composites (CMCs) are being developed for a number of high-temperature and high-performance applications in industrial, aerospace, and energy conservation sectors. This article focuses on processing, fabrication, testing, and characterization methods of CMCs, namely, discontinuously reinforced composites and continuous-fiber-reinforced composites. Processing methods include cold pressing, sintering, hot pressing, reaction bonding, melt infiltration, directed metal oxidation, sol-gel and polymer pyrolysis, self-propagating high-temperature synthesis and joining. A table summarizes the properties of various ceramic reinforcements and industrial applications of these composites.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003371
EISBN: 978-1-62708-195-5
.... The reinforcements are either in the form of continuous fibers or discontinuous reinforcements, such as chopped fibers, whiskers, particulates, or platelets. Metal-matrix composites can contain either continuous or discontinuous or a combination of both these reinforcements. The main advantage of discontinuously...
Abstract
Metallic matrices are essential constituents for the fabrication of metal-matrix composites (MMCs). This article describes three different classes of aluminum alloys, namely, commercial aluminum alloys, low-density and high-modulus alloys, and high temperature alloys. It presents typical tensile properties and fracture toughness of the selected heat treatable aluminum alloys in a table. Titanium alloys are very attractive for MMC applications, due to their higher strength and temperature capability compared to aluminum alloys. The article tabulates the effect of heat treatment on room-temperature properties and tensile properties of Ti-25Al-17Nb alloy sheet.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003448
EISBN: 978-1-62708-195-5
... Abstract Metal-matrix composites (MMCs) are used in structural applications, and in applications requiring wear resistance, thermal management, and weight savings. This article summarizes the mechanical and thermal properties of discontinuously reinforced aluminum MMCs, laminated metallic...
Abstract
Metal-matrix composites (MMCs) are used in structural applications, and in applications requiring wear resistance, thermal management, and weight savings. This article summarizes the mechanical and thermal properties of discontinuously reinforced aluminum MMCs, laminated metallic composites, and continuously aligned fiber reinforced MMCs.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001101
EISBN: 978-1-62708-162-7
... an overview of the status of MMCs, and provides information on physical and mechanical properties, processing methods, distinctive features, and various types of continuously and discontinuously reinforced aluminum, magnesium, titanium, copper, superalloy, and intermetallic-matrix composites. It further...
Abstract
Metal-matrix composites (MMCs) are a class of materials with potential for a wide variety of structural and thermal management applications. They are nonflammable, do not outgas in a vacuum, and suffer minimal attack by organic fluids, such as fuels and solvents. This article presents an overview of the status of MMCs, and provides information on physical and mechanical properties, processing methods, distinctive features, and various types of continuously and discontinuously reinforced aluminum, magnesium, titanium, copper, superalloy, and intermetallic-matrix composites. It further discusses the property prediction and processing methods for MMCs.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003480
EISBN: 978-1-62708-195-5
... true for silicon carbide particle-reinforced aluminum (often called Al/SiC in the electronic packaging industry and discontinuously reinforced aluminum, or DRA, in the aerospace industry), which is one of the most important of the new composite packaging materials. In the following sections...
Abstract
This article presents an overview of advanced composites, namely, polymer matrix composites, metal-matrix composites, ceramic-matrix composites, and carbon-matrix composites. It also provides information on the properties and applications of the composites in thermal management and electronic packaging.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006488
EISBN: 978-1-62708-207-5
... Abstract In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two...
Abstract
In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two main methods of MMC solidification processing. It describes the MCC casting methods, such as sand and permanent mold casting, centrifugal casting, compocasting, and high-pressure die casting. The article discusses the MMC infiltration processes in terms of pressure infiltration casting and liquid metal infiltration. It reviews the powder metallurgy processing of aluminum MMCs and deformation processing of discontinuously reinforced aluminum composites. The article concludes with a discussion on the processing of fiber-reinforced aluminum.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
..., such as the aluminides of titanium, nickel, and iron, are also under development. Reinforcements, characterized as either continuous or discontinuous, may constitute from 10 to 70 vol% of the composite. Continuous fiber or filament (f) reinforcements include graphite, silicon carbide (SiC), boron, aluminum oxide (Al 2 O...
Abstract
Metal-matrix composites (MMCs) are a class of materials with potential for a wide variety of structural and thermal applications. This article discusses the mechanical properties of MMCs, namely aluminum-matrix composites, titanium-matrix composites, magnesium-matrix composites, copper-matrix composites, superalloy-matrix composites, and intermetallic-matrix composites. It describes the processing methods of discontinuous aluminum MMCs which include casting processes, liquid-metal infiltration, spray deposition and powder metallurgy. The article provides useful information on aluminum MMC designation system and also describes the types of continuous fiber aluminum MMCs, including aluminum/boron MMC, aluminum/silicon carbide MMC, aluminum/graphite MMC, and aluminum/alumina MMC.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003350
EISBN: 978-1-62708-195-5
... polymers, where the discontinuous phase is more compliant and more ductile than the polymer, resulting in improved toughness. Similarly, steel wires have been used to reinforce gray cast iron in truck and trailer brake drums. Composites are commonly classified at two distinct levels. The first level...
Abstract
This article begins with a brief history of composite materials and discusses its characteristics. It presents an introduction to the constituents, product forms, and fabrication processes of composite materials. The article concludes with a discussion on the applications of organic-matrix, metal-matrix, and ceramic-matrix composites.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003472
EISBN: 978-1-62708-195-5
... Abstract This article focuses on the techniques used in recycling of aluminum metal matrix composites (MMCs) such as discontinuous SiC reinforced aluminum MMCs and continuous reinforced aluminum MMCs. It provides a discussion on the properties of recycled aluminum MMCs and disposal of aluminum...
Abstract
This article focuses on the techniques used in recycling of aluminum metal matrix composites (MMCs) such as discontinuous SiC reinforced aluminum MMCs and continuous reinforced aluminum MMCs. It provides a discussion on the properties of recycled aluminum MMCs and disposal of aluminum MMCs.
Image
Published: 01 January 1989
Fig. 1 Cross sections of typical fiber-reinforced MMCs. (a) Continuous fiber reinforced graphite/aluminum composites. (b) Discontinuous silicon carbide/aluminum composite. (c) Continuous-fiber silicon carbide/aluminum composite
More
Image
in Metal-Matrix Composites
> Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Published: 01 January 1990
Fig. 1 Cross sections of typical fiber-reinforced MMCs. (a) Continuous-fiber-reinforced boron/aluminum composite. Shown here are 142 μm diam boron filaments coated with B 4 C in a 6061 aluminum alloy matrix. (b) Discontinuous graphite/aluminum composite. Cross section shows 10 μm diam chopped
More
Image
Published: 01 January 2001
) A fluid manifold end gland currently used in F-18 E/F aircraft as part of the subsystem that controls the rudder and aileron. The material is a powder metallurgy discontinuously reinforced aluminum, 2009/SiC/15p. Dimensions for the end gland are provided in the text. Courtesy of DWA Aluminum Composites
More
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
... magnesium, copper, and superalloy MMCs. metal-matrix composites high-pressure die casting pressure infiltration casting liquid metal infiltration spray deposition powder metallurgy continuous fiber-reinforced aluminum composite discontinuously reinforced titanium composites continuous fiber...
Abstract
Metal-matrix composites (MMCs) are a class of materials with a wide variety of structural, wear, and thermal management applications. This article discusses the primary processing methods used to manufacture discontinuous aluminum MMCs, namely, high-pressure die casting, pressure infiltration casting, liquid metal infiltration, spray deposition, and powder metallurgy methods. It describes the processing of continuous fiber-reinforced aluminum, discontinuously, reinforced titanium, and continuous fiber-reinforced titanium. The article concludes with information on work done to develop magnesium, copper, and superalloy MMCs.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
... for their structural properties, the definition can be restricted to include only those materials that contain a reinforcement (such as fibers or particles) supported by a binder (matrix) material. Thus, composites typically have a discontinuous fiber or particle phase that is stiffer and stronger than...
Abstract
This article discusses the types, properties, and uses of continuous-fiber-reinforced composites, including glass, carbon, aramid, boron, continuous silicon carbide, and aluminum oxide fiber composites. While polyester and vinyl ester resins are the most used matrix materials for commercial applications, epoxy resins, bismaleimide resins, polyimide resins, and thermoplastic resins are used for aerospace applications. The article addresses design considerations as well as product forms and fabrication processes.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005339
EISBN: 978-1-62708-187-0
.... It illustrates the three broad categories of MMCs depending on the aspect ratio of the reinforcing phase. The categories include continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. The article discusses the two main classes...
Abstract
Metal matrix composites (MMCs) can be synthesized by vapor phase, liquid phase, or solid phase processes. This article emphasizes the liquid phase processing where solid reinforcements are incorporated in the molten metal or alloy melt that is allowed to solidify to form a composite. It illustrates the three broad categories of MMCs depending on the aspect ratio of the reinforcing phase. The categories include continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. The article discusses the two main classes of solidification processing of composites, namely, stir casting and melt infiltration. It describes the effects of reinforcement present in the liquid alloy on solidification. The article examines the automotive, space, and electronic packaging applications of MMCs. It concludes with information on the development of select cast MMCs.