Book Chapter

By Karl K. Chang
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0009242
EISBN: 978-1-62708-195-5
... filament yarns, rovings, woven fabrics, discontinuous staple and spun yarns, fabrics, and pulp. Key representative properties of para-aramid fibers are listed in a table. The article reviews the properties of aramid fibers, including tensile modulus, tensile strength, creep and fatigue, compressive...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001101
EISBN: 978-1-62708-162-7
... has a lower thermal conductivity, which is sometimes a factor in its selection. Three types of magnesium MMCs are currently under development: continuous fiber Gr/Mg for space structures ( Ref 43 ), short staple fiber Al 2 O 3 /Mg for automotive engine components ( Ref 44 ), and discontinuous SiC or B...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
... 7 P120 Gr/Al 60 2.41 150 419 242 −0.32 −0.17 P120 Gr/Cu 60 4.90 306 522 302 −0.07 −0.04 Matrix alloys for discontinuous reinforced aluminum metal-matrix composites Table 2 Matrix alloys for discontinuous reinforced aluminum metal-matrix composites Alloy...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003033
EISBN: 978-1-62708-200-6
...Abstract Abstract This article addresses the types, properties, forms, and applications of fibers that are available for use in fiber-reinforced polymeric matrix composites, including glass, graphite, carbon, aramid, boron, silicon carbide, ceramic, continuous oxide and discontinuous oxide...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
... for space structures, short staple fiber Al 2 O 3 /Mg for automotive engine components, and discontinuous SiC or B 4 C/Mg for engine components and low-expansion electronic packaging materials. Matrix alloys include AZ31, AZ91, ZE41, QE22, and EZ33. Processing methods parallel those used for the aluminum...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005674
EISBN: 978-1-62708-198-6
... cages that become larger as the patient grows Implantable fixation devices such as bone screws, plates, rods, hooks, nails, cables, and staples Prosthetics for support of soft tissue Bone conduction hearing aids Reconstructive plate, mesh, and acrylic that supports broken bones or helps...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.9781627081955
EISBN: 978-1-62708-195-5
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003687
EISBN: 978-1-62708-182-5
... Limitations Inhospitable Substrates Limitations of Design Size Limitations Environmental Issues Zinc and cadmium deposits will protect steel at pores and other discontinuities by cathodic protection. Observation of the emf series ( Table 1 ) shows that zinc is electronegative to steel...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005707
EISBN: 978-1-62708-171-9
..., and tubing Coating Product Sheet Wire Tubing Zinc and Zn-5Al Roofing, siding, doors, culvert, ductwork, housings, appliances, autobody panels and structural components Nails, staples, guy wires, strand, tension members, rope, utility wire, fencing Electrical conduit Zinc-iron Autobody...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003415
EISBN: 978-1-62708-195-5
... squeegee each is used to apply the resin paste to the surface of films, which enclose the chopped glass reinforcing fibers from above and below. The fiber rovings are metered according to the drawing speed of the cutter and cut to a length of 25 or 50 mm (1 or 2 in.). The two-dimensional, unoriented staple...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002481
EISBN: 978-1-62708-194-8
... of continuous-fiber-reinforced composites follows techniques used for polymer-matrix composite manufacture (infiltration, pultrusion) or metalworking (investment casting, hot isothermal rolling, diffusion bonding). Discontinuous-fiber reinforcement allows casting, squeeze casting, hot extrusion, hot forging...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006527
EISBN: 978-1-62708-207-5
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003067
EISBN: 978-1-62708-200-6
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... Stitching wire Stapling wire Carbon steel pipe Structural tubing Line pipe Oil country tubular goods Steel specialty tubular products Pressure tubing Mechanical tubing Aircraft tubing Hot-rolled carbon steel wire rods Industrial...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
...  structural 178 0.2 180 0.2  pipe for piling 74 0.1 (c) …  stainless 55 0.1 42 0.1 Wire  drawn 1,073 1.3 800 1.0  nails and staples (a) … 218 0.3  barbed and twisted (a) … 49 0.1 woven wire fence (a) … 13 …  bale ties and baling wire...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.9781627081719
EISBN: 978-1-62708-171-9
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003065
EISBN: 978-1-62708-200-6
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7