1-20 of 55 Search Results for

dip infiltration

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006099
EISBN: 978-1-62708-175-7
...Abstract Abstract This article provides information on the infiltration mechanism of carbide structures. It reviews the basic techniques used for metal infiltration, including dip infiltration, contact filtration, gravity feed infiltration, and external-pressure infiltration. The article...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004220
EISBN: 978-1-62708-184-9
... these circumstances, the use of stainless steel becomes a highly advantageous proposition. One of the principal methods of preventing these problems has been to place cover concrete of sufficient quality and thickness over the steel to dramatically reduce any infiltration of chloride or CO 2 to the steel surface...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004024
EISBN: 978-1-62708-185-6
... Tool steel Technique Vacuum degassing Mixing of slurry Vacuum cast Hot isostatic pressing Spray forming Post processing Curing Sintering and infiltration Thermal curing Decanning Cooling to room temperature Tensile strength … 100 ksi >70 ksi … 239 ksi Operating temperature...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001306
EISBN: 978-1-62708-170-2
... 6.0–8.0 2.0 max 87.4–93.7 … P/M nickel steel FN-0708 … … 0.6–0.9 6.0–8.0 2.0 max 87.1–93.4 … P/M infiltrated steel FX-1000 B 783 … 0–0.3 … 8.0–14.9 82.8–92.0 … P/M infiltrated steel FX-1005 B 783 … 0.3–0.6 … 8.0–14.9 80.5–91.7 … P/M infiltrated steel FX-1008 B...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001269
EISBN: 978-1-62708-170-2
... of these variables as a function of temperature versus the water/hydrogen ratio. Another concern is the infiltration of free oxygen into this atmosphere. Oxygen levels between 50 and 100 ppm have been shown to be detrimental to proper surface preparation for hot-dip coatings. Wet chemical precleaning...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006576
EISBN: 978-1-62708-290-7
... energy deposition. On the other hand, binder jet-based AM is a powder bed-based technology that uses a binder to fabricate a green component that can be subsequently sintered or infiltrated to full density. The different AM technologies are briefly described in this section. Laser powder bed fusion...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001318
EISBN: 978-1-62708-170-2
... impregnation, vapor phase carbon infiltration, or combinations of the two to achieve pore filling ( Ref 3 , 4 , 5 , 6 , 7 , 8 , 9 , 10 ). High-temperature pyrolysis is used to convert liquid impregnants to carbon while vapor phase infiltration is conducted in reduced-pressure reactors where flowing...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003688
EISBN: 978-1-62708-182-5
... ) Soil description Soil corrosivity Coating life, years Poor drainage, low resistivity High 1–2 Poor drainage, high salt content Moderate 4–6 Good drainage, high resistivity, low salt content Low 18–25 Source: Ref 7 Common coating weight categories for hot-dip galvannealed...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003773
EISBN: 978-1-62708-177-1
... Etchant Bearing material NH 4 OH and H 2 O 2 (a) Commercial bronze liner Copper-lead alloy liner Copper-lead-tin alloy liner High-leaded tin bronze liner Leaded tin bronze liner Lead-tin-copper overlay on copper-lead alloy liner Nickel bronze infiltrated with lead-base babbitt Nickel-tin bronze...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003430
EISBN: 978-1-62708-195-5
...) in several different areas of postprocessing. Fig. 3 Illustrations of various SiC and SiC composites joined using melt infiltration, a reaction-forming process to make various components. Courtesy of M. Singh, NASA Glenn Research Center Fig. 4 Heat exchanger subassembly (left...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
..., namely, discontinuously reinforced composites and continuous-fiber-reinforced composites. Processing methods include cold pressing, sintering, hot pressing, reaction bonding, melt infiltration, directed metal oxidation, sol-gel and polymer pyrolysis, self-propagating high-temperature synthesis...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006571
EISBN: 978-1-62708-290-7
... on Porous Surfaces , Langmuir , Vol 18 , 2002 , p 2980 – 2984 10.1021/la0117810 20. Holman R.K. , Cima M.J. , Uhland S.A. , and Sachs E. , Spreading and Infiltration of Inkjet-Printed Polymer Solution Droplets on a Porous Substrate , J. Colloid Interface Sci. , Vol 248...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003422
EISBN: 978-1-62708-195-5
.... The article discusses matrix precursor impregnants, liquid impregnation, and chemical vapor infiltration (CVI) for densification of CCCs. It presents various coating approaches for protecting CCCs, including pack cementation, chemical vapor deposition, and slurry coating. Practical limitations of coatings...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003245
EISBN: 978-1-62708-199-3
...% picral or 2% nital. Etchants for microscopic examination of cast irons Table 3 Etchants for microscopic examination of cast irons Etchant Composition Etching technique Applications Picral 4% picric acid, 96% ethanol Dip etch for 2–10 s General-purpose etching of all pearlitic gray...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003245
EISBN: 978-1-62708-199-3
... with either 4% picral or 2% nital. Table 3 Etchants for microscopic examination of cast irons Etchant Composition Etching technique Applications Picral 4% picric acid, 96% ethanol Dip etch for 2–10 s General-purpose etching of all pearlitic gray, malleable, and ductile cast irons. Best...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006492
EISBN: 978-1-62708-207-5
... 1.5 8 Resistance to humid atmospheres ISO 3231 After 24 cycles. No infiltration exceeding 1 mm (0.04 in.) on both sides of the scratch, and no change in color or blisters in excess of 2 (S2) according to ISO 4628-2 Same as class 1 Same as class 1 Same as class 1 9 Acetic acid saltspray...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003350
EISBN: 978-1-62708-195-5
... or lower copper ( Ref 6 ). Infiltration casting also often uses aluminum-silicon alloys, such as A356, and this is common for materials used in thermal management. However, wrought alloy compositions, including common 2 xxx and 6 xxx alloys, can also be used for infiltration casting. For pressureless...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001097
EISBN: 978-1-62708-162-7
... Circuit breakers (a) PSR, press-sinter-re-press; INF, press-sinter-infiltrate; PS, press-sinter; PSE, press-sinter-extrude; IO, internal oxidation; PPSE, preoxidize-press-sinter-extrude; SF, oxidized from one direction. (b) A: Advance Metallurgy, Inc., McKeesport, PA. C: Contacts, Materials...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006421
EISBN: 978-1-62708-192-4
... Contains metallic glass as predominant coating component Composite coatings with crystalline phases in amorphous matrix possible Very high surface hardness and wear resistance in various environments Must control process kinetics (heating and cooling rates) and dilution Ceramic Infiltration process...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
... A. , Infiltration of A6063 Aluminium Alloy into SiC-B 4 C Hybrid Preforms using Vacuum Assisted Block Mould Investment Casting Technique , Trans. Nonferrous Met. Soc. China , Vol 22 ( No. 7 ), July 2012 , p 1563 – 1567 10.1016/S1003-6326(11)61356-3 • Browne D.J. and O'Mahoney D...