Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004035
EISBN: 978-1-62708-185-6
... is parallel to forging datum plane A, and machine reference planes B and C are parallel to forging datum planes B and C. In this way, tooling points for forging dimensioning provide a means of controlling operations through to the finish-machined part. Dimensional tolerances are applied to both the...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004033
EISBN: 978-1-62708-185-6
... machining. The article presents a graphical summary of the interdependence of corner and fillet dimensions with the dimensions of adjoining ribs and webs. It concludes with information on designer's checklist for corners and fillets. closed-die forging die filling forging forging alloy machining...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0001838
EISBN: 978-1-62708-181-8
... surface area of irregular fracture surfaces. The article reviews the experimental procedures required to obtain profiles and measurements that are made. In addition, fractal equations that linearize all the experimental data and provide constant fractal dimensions are presented in the article. Modified...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003125
EISBN: 978-1-62708-199-3
... shapes; forgings; and impacts. The article provides information on product economics, design and selection, including product dimension and dimension tolerances, and design and use of wrought product capabilities. Finally, it tabulates the specifications and standards for aluminum mill products...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003988
EISBN: 978-1-62708-185-6
... amount required for conventional forgings because of the improved dimensional tolerances, shown in Table 3 . Standard machining operations may be used to achieve final dimensions and surface finish ( Ref 66 ). One of the main economic advantages of powder forging is the reduced amount of machining...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004008
EISBN: 978-1-62708-185-6
... Abstract The drawing process, one of the oldest metal forming operations, allows excellent surface finishes and closely controlled dimensions to be obtained in long products that have constant cross sections. This article discusses the basic mechanics and preparation steps of drawing. It...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003987
EISBN: 978-1-62708-185-6
... dimensions before sizing is attempted. When this is done, sizing by coining can produce workpieces having dimensional tolerances that are acceptable in good machining practice, often with significant savings in material and labor costs. Sizing is used to maintain dimensions to close tolerances and to...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005993
EISBN: 978-1-62708-166-5
... Abstract This article is a comprehensive collection of formulas, tables, and analytical solutions, addressing hundreds of heat-transfer scenarios encountered in science and engineering. With detailed explanations and dimensioned drawings, the article demonstrates how to set up and solve real...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006473
EISBN: 978-1-62708-190-0
... provides information on the dimension-measurement applications of ultrasonic inspection methods. ultrasonic imaging inspection area-amplitude blocks distance-amplitude blocks calibration defects WHEN ULTRASONIC NONDESTRUCTIVE TESTING (NDT) was first applied, it was a workmanship standard and...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005323
EISBN: 978-1-62708-187-0
... Abstract This article begins with an overview of classes and applications of gray iron. It discusses the castability of gray iron in terms of section sensitivity and fluidity. The article provides information on the dimensions of prevailing sections recommended for gray irons and reviews the...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005208
EISBN: 978-1-62708-187-0
... Abstract This article begins with balance equations for mass, momentum, energy, and solute and the necessary boundary conditions for solving problems of interest in casting and solidification. The transport phenomena cover a vast range of length and time scales, from atomic dimensions up to...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005344
EISBN: 978-1-62708-187-0
... Abstract The International Committee of Foundry Technical Associations has identified seven basic categories of casting defects: metallic projections, cavities, discontinuities, defective surfaces, incomplete casting, incorrect dimension, and inclusions or structural anomalies. This article...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006268
EISBN: 978-1-62708-169-6
... precipitates that occur in the natural aging and artificial aging of Al-Mg-Si-(Cu) alloys, Al-Mg-Cu alloys, microalloyed Al-Mg-Cu-(Ag, Si) alloys, aluminum-lithium-base alloys, and Al-Zn-Mg-(Cu) alloys. Crystal structure, composition, dimensions, and aging conditions of precipitates are detailed. Effects of...
Book Chapter

Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006544
EISBN: 978-1-62708-183-2
... crystal structure oxidation unit cell lattice dimensions metal crystals Pearson symbol space-group notation METALLIC MATERIALS normally have atoms or molecules placed in a definite, repeating, three-dimensional geometric pattern forming one of seven crystal structures recognized in...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003159
EISBN: 978-1-62708-199-3
... Abstract Low-expansion alloys are materials with dimensions that do not change appreciably with temperature. Alloys included in this category are various binary iron-nickel alloys and several ternary alloys of iron combined with nickel-chromium, nickel-cobalt, or cobalt-chromium alloying. Low...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003132
EISBN: 978-1-62708-199-3
... tube welding, cold drawing, and tube reducing. The article lists the standard dimensions and tolerances for several kinds of copper tubes and pipes in the ASTM specifications, along with other requirements for the tubular products. cold drawing copper tube alloys copper tubular products...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
... dimensions are averages, and the use of either larger or smaller numerical factors may result in more difficult casting or defects. Source Van Hoen, Vol. III. Table 1 Dimensional limits and tolerances for aluminum castings produced by different processes Sand castings Diameter of cored...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003972
EISBN: 978-1-62708-185-6
... the overall system. Manufacturing process selection and parameters must meet these geometric requirements of overall shape, features, dimensions, and dimensional tolerances, depicted in Fig. 1a . Fig. 1 Connecting rod as a part design example. (a) Typical geometric dimensional requirements. (b...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004030
EISBN: 978-1-62708-185-6
... − ε ˙ 1 ) 2 } Table 3 Formulas for compression testing of isotropic material Variable or quantity Symbol or relation Uniaxial compression under uniform deformation conditions Initial sample dimensions Height ( h 0 ) Diameter ( d 0 ) Area ( A 0 ), A...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003986
EISBN: 978-1-62708-185-6
... Abstract Precision forging is defined as a closed-die forging process in which the accuracy of the shape, dimensional tolerances, and surface finish exceed normal expectations to the extent that some of the postforge operations can be eliminated. This article provides an overview of the key...