DOI: 10.31399/asm.hb.v18.a0006360
EISBN: 978-1-62708-192-4
...Abstract Abstract This article describes two variations of carbon-base coatings: diamondlike carbon (DLC) coatings and polycrystalline diamond (PCD) coatings. It discusses the basics of a few deposition methods as they apply to industrially relevant coatings. The methods include deposition...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001320
EISBN: 978-1-62708-170-2
... coating on a cobalt-enriched cemented carbide insert Fig. 8 Diamond coating on a cemented carbide insert Fig. 3 Chemical vapor deposition coatings. (a) Cemented carbide insert with TiC coating. Note eta phase at the coating-substrate interface. (b) 73WC-19(Ti,Ta,Nb)C-8Co alloy...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003424
EISBN: 978-1-62708-195-5
..., diamond plated, brazed diamond, diamond coated carbide, and polycrystalline cutting tools. The article also describes cutting tool materials that are used for peripheral milling, face milling, and the trimming of polymer-matrix composites. machining carbon fiber-reinforced epoxy epoxy thermoset...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006547
EISBN: 978-1-62708-290-7
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006434
EISBN: 978-1-62708-192-4
... and discuses the characteristics and fundamental aspects of solid lubricants. It describes the material categories of solid lubricant coatings, including graphite, graphite fluoride, transition metal dichalcogenides, diamond-like-carbon, polymeric materials, and metallic films. The article presents...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003563
EISBN: 978-1-62708-180-1
... and diamond-like carbon coatings. It presents an insight into the design considerations of coating-substrate material properties, coating thickness, and coating processes to combat RCF failure in TS coatings. References References 1. Suh N.P. , An Overview of the Delamination Theory of Wear...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003218
EISBN: 978-1-62708-199-3
...Abstract Abstract Chemical vapor deposition (CVD) involves the formation of a coating by the reaction of the coating substance with the substrate. Serving as an introduction to CVD, the article provides information on metals, ceramics, and diamond films formed by the CVD process. It further...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003218
EISBN: 978-1-62708-199-3
... Abstract Chemical vapor deposition (CVD) involves the formation of a coating by the reaction of the coating substance with the substrate. Serving as an introduction to CVD, the article provides information on metals, ceramics, and diamond films formed by the CVD process. It further discusses...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002177
EISBN: 978-1-62708-188-7
... tool performance and workpiece machinability. It provides a brief description of cutting tool materials, such as high-speed steels, uncoated and coated carbides, cermets, ceramics, cubic boron nitride, and polycrystalline diamond. The article considers the matrices that represent the range of tests...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009073
EISBN: 978-1-62708-177-1
... silicon carbide papers or diamond-coated (continuous and discontinuous) disks. In some cases, such as hand polishing, rough polishing may be performed using deagglomerated alumina suspensions. In the grinding and rough polishing steps, the abrasive may be adhered to the surface of a disk, pad, or paper...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001291
EISBN: 978-1-62708-170-2
... in an electrically neutral state. Adjusting the deposition energy can produce coatings that have greater density, purity, and adhesion. Under favorable circumstances, the quenching of ions can produce coatings with structures that have unusual properties, such as the extremely hard and smooth amorphous diamond...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002194
EISBN: 978-1-62708-188-7
...Parameters for composite trimming Table 1 Parameters for composite trimming Operation Equipment Cutter type Speed m/s sfm Straight-line cuts Pneumatic saw Diamond-coated circular saw (a) 60–90 12,000–18,000 Hand router Diamond router (b) Carbide router (c) 10–15...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003152
EISBN: 978-1-62708-199-3
... Vapor Deposition (PVD or CVD) Plasma-Assisted CVD Coatings CVD/PVD Coatings Diamond Coatings Almost 50% of the total production of cemented carbides is now used for nonmetal cutting applications such as metalforming dies, punches, and rolls, transportation and construction, mining, oil...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003042
EISBN: 978-1-62708-200-6
.... Research and development of other machining techniques and procedures for composites is ongoing but limited. Cutting tools used to trim composites are of three basic types: circular saws, router cutters, and abrasive tools. Diamond-coated circular saw blades used in portable equipment are useful...
Book Chapter

By Koji Kato
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006394
EISBN: 978-1-62708-192-4
.... Source: Ref 49 . (b) Mechanochemical polishing (MCP) of diamond coating on silicon wafer with iron polisher in vacuum. Source: Ref 50 Fig. 27 Tribochemical effect of abrasive particles and liquid media on polishing rate of silicon single-crystal wafer in polishing with porous polyurethane...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006418
EISBN: 978-1-62708-192-4
... , Surface and Coatings Technology , Vol 124 , 2000 , p 235 – 242 10.1016/S0257-8972(99)00653-2 • Mallika K. and Komanduri R. , Diamond Coatings on Cemented Tungsten Carbide Tools by Low-Pressure Microwave CVD , Wear , Vol 224 , 1999 , p 245 – 266 10.1016/S0043-1648(98)00337-8...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006064
EISBN: 978-1-62708-175-7
.... Alternatively, additives such as TaC or NbC improve thermal properties of the WC-Co system. Coated grades are used for a large majority of WC-Co cutting tools today. Ceramic and diamond coatings provide cutting tools with increased wear resistance and thermal insulation. The high elastic modulus of the WC...
Book Chapter

By Dongyang Li
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006382
EISBN: 978-1-62708-192-4
... 11 . (b) Brittle features of worn surface of quenched steel. Source: Ref 12 . (c) Worn surface of 304 steel showing considerable plastic deformation. Source: Ref 13 Fig. 12 (a) Nanostructured diamond coating for temporomandibular joints. Source: Ref 21 . (b) Multilayered coating...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006433
EISBN: 978-1-62708-192-4
... on carbon steel as well as CVD coatings of diamond (20 µm thick) on WC-Ni and B4C (15 µm thick) on WC-Co. E k at 90° jet angle for water-sand jet and air-sand jet impingement erosion tests. Source: Ref 16 Fig. 6 Plot of erosion resistance versus static hardness for selected materials. Erosion...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003480
EISBN: 978-1-62708-195-5
... Commercial pitch-based and vapor-grown carbon fibers with higher thermal conductivities, perhaps approaching 2000 W/m · K Commercial diamond and diamond-coated carbon fibers with thermal conductivities also approaching 2000 W/m · K Reinforcement coatings to promote adhesion, reduce reinforcement-matrix...