Published: 01 January 2005
Fig. 4 Influence of deformation rate on hot-twist characteristics of low-carbon steels at 1095 °C (2000 °F). Source: Ref 27 More
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003292
EISBN: 978-1-62708-176-4
... Abstract Studies on mechanical behavior of superplasticity at or above 50" of the melting point lead to the understanding of superplasticity as a creep phenomenon. This article provides a discussion on the four relationships that define the basic deformation characteristics associated...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003024
EISBN: 978-1-62708-200-6
... Abstract This article discusses the deformation and viscoelastic characteristics of plastics as polymeric materials, focusing on the test methods used for the evaluation of their mechanical properties, methods available for analytically predicting the deformation response of polymers...
Image
Published: 01 October 2014
Fig. 6 Scanning electron micrograph of plastically deformed surface of a low-temperature carburized 316 stainless steel tensile specimen. Because the treated material retains its austenitic structure, it also retains its ductile deformation characteristics, as shown by the intersecting slip More
Image
Published: 01 December 1998
in.) in diameter, was made of 6118 steel and had a hardness of 23 HRC. Being made of a ductile metal, it was twisted in pure torsion with a single overload, yielding the fracture on the transverse shear plane shown in (b). (b) Fracture surface of the shaft, showing the rotary deformation characteristic of a single More
Book Chapter

By Howard A. Kuhn
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003265
EISBN: 978-1-62708-176-4
... Abstract Compression tests are used for subscale testing and characterizing the mechanical behavior of anisotropic materials. This article discusses the characteristics of deformation during axial compression testing, including deformation modes, compressive properties, and compression-test...
Book Chapter

By Sammy Tin
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005404
EISBN: 978-1-62708-196-2
... materials using expressions known as constitutive equations that relate the dependence of stress, temperature, and microstructure on deformation. The article reviews the characteristics of creep deformation and mechanisms of creep, such as power-law creep, low temperature creep, power-law breakdown...
Book Chapter

By Scott M. Olig
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006941
EISBN: 978-1-62708-395-9
... of a material. This includes assessing the extent of stress decay in materials that are pre-stressed, the noise and vibration transmission characteristics of a material, the amount of heat build-up in a material subjected to cyclic deformation, and the extent a material can recover from any prior deformation...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003541
EISBN: 978-1-62708-180-1
... Abstract This article reviews the mechanical behavior and fracture characteristics that discriminate structural polymers from metals. It provides information on deformation, fracture, and crack propagation as well as the fractography involving the examination and interpretation of fracture...
Book Chapter

By A.R. Shah, D.B. Edwards
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006865
EISBN: 978-1-62708-395-9
... Abstract This article reviews the mechanical behavior and fracture characteristics that discriminate structural polymers from metals, including plastic deformation. It provides overviews of crack propagation and fractography. The article presents the distinction between ductile and brittle...
Book Chapter

By Jack W. Bray
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001059
EISBN: 978-1-62708-162-7
... Abstract Aluminum mill products are those that have been subjected to plastic deformation by hot- and cold-working mill processes such as rolling, extruding, and drawing, either singly or in combination. Microstructural changes associated with the working and with any accompanying thermal...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003258
EISBN: 978-1-62708-176-4
... hydrostatic pressure effects material characteristics tension test plane-strain tension test compression test plane-strain compression test partial-width indentation test torsion test bulk deformation formability sheet-metal forming mechanical properties sample preparation quality control...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003114
EISBN: 978-1-62708-199-3
... steels, and precision-cast tool steels. It describes the effects of surface treatments on the basic properties of tool steels, including hardness, resistance to wear, deformation, and toughness. The article provides information on fabrication characteristics of tool steels, including machinability...
Book Chapter

Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003720
EISBN: 978-1-62708-177-1
..., and fatigue fracture with illustrations. It discusses microanalysis with a focus on the method of light microscopy and includes information of scanning electron microscope in fractography. The article also explains the characteristics of solidification, transformation, deformation structures...
Book Chapter

By Vladimir Segal
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004016
EISBN: 978-1-62708-185-6
... Abstract This article describes the mechanics and processing characteristics of equal-channel angular extrusion (ECAE). Tool design considerations for the ECAE are discussed. During ECAE, severe plastic strains and simple shear deformation mode contribute to strong, sometimes unusual effects...
Book Chapter

By Howard A. Kuhn
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009008
EISBN: 978-1-62708-185-6
... geometry and friction conditions; strain measurements; crack detection; and material inhomogeneities, which are to be considered for performing cold upset testing. It describes test characteristics in terms of deformation, free-surface strains, and stress states for performing cylindrical compression tests...
Book Chapter

By P. Dadras
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003262
EISBN: 978-1-62708-176-4
... Abstract A characteristic feature of bending is the inhomogeneous (nonuniform) nature of the deformation. Therefore, in a bent specimen, the strain and stress at a given point are dependent on the location of the point with respect to the neutral axis of the cross-sectional area of the specimen...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003184
EISBN: 978-1-62708-199-3
... requiring a high degree of metal displacement. Materials also are rated according to forgeability—the amount of deformation possible before failure ( Fig. 1 ). Both these characteristics vary with forging temperatures ( Table 1 ). Classification of alloys in order of increasing forging difficulty Table...
Book Chapter

By Matthew J. Donachie, Stephen J. Donachie
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003120
EISBN: 978-1-62708-199-3
..., and environmental protection applications. This article discusses the material characteristics, phases, structures, and systems of superalloys. It describes the processing of superalloys, including primary and secondary melting, deformation processing (conversion), powder processing, investment casting, and joining...
Book Chapter

By Jennifer Hoffman, Tao Xu, Suresh Donthu
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005676
EISBN: 978-1-62708-198-6
... that develops from molecular architecture and ordering. Due to their molecular nature, polymers exhibit both liquid- and solid-like characteristics. Similar to liquids, polymers deform slowly with time under stress (i.e., creep). Polymers also store some elastic energy when subjected to stress and may recover...