Skip Nav Destination
Close Modal
By
David L. Bourell, Joseph J. Beaman, Jr., Donald Klosterman, Ian Gibson, Amit Bandyopadhyay
Search Results for
data infiltration
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 183 Search Results for
data infiltration
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006962
EISBN: 978-1-62708-439-0
... AM-using organization. It discusses the following threat categories: technical data theft, sabotage, illegal part manufacturing, and data infiltration and exfiltration. The article also presents a detailed discussion on countermeasures against threat categories. additive manufacturing...
Abstract
Additive manufacturing (AM) security is considered an integral part of several broader security fields, including supply chain security and critical infrastructure security. This article presents a general guide to the types of data and locations of data as they may exist in a typical AM-using organization. It discusses the following threat categories: technical data theft, sabotage, illegal part manufacturing, and data infiltration and exfiltration. The article also presents a detailed discussion on countermeasures against threat categories.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006076
EISBN: 978-1-62708-175-7
... 1100 159 510 74 36 HRC 58 HRC 190 27 7.3 Note: All data based on single-pass infiltration. (a) Suffix numbers represent minimum strength values in ksi; yield in the as-sintered condition and ultimate in the heat treated condition. (b) Mechanical property data derived from laboratory...
Abstract
The two most important classes of materials that are manufactured via infiltration methods are copper- and silver-infiltrated refractory metals and refractory carbides, and copper-infiltrated steels. This article focuses on copper-infiltrated steels and discusses the basic requirements for infiltration, which is a technique that is only applicable to material systems that meet certain requirements. It addresses these requirements and describes the conventional (partial) infiltration process of powder metallurgy (PM) steel. The materials used in the process, such as matrix and infiltrant, are discussed. The article also details several criteria used to evaluate the performance of an infiltration process. It concludes with information on alloy steels and fully infiltrated steels.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006488
EISBN: 978-1-62708-207-5
... Abstract In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two...
Abstract
In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two main methods of MMC solidification processing. It describes the MCC casting methods, such as sand and permanent mold casting, centrifugal casting, compocasting, and high-pressure die casting. The article discusses the MMC infiltration processes in terms of pressure infiltration casting and liquid metal infiltration. It reviews the powder metallurgy processing of aluminum MMCs and deformation processing of discontinuously reinforced aluminum composites. The article concludes with a discussion on the processing of fiber-reinforced aluminum.
Image
Published: 01 January 2005
generated by the mixed-potential theory (MPT) and that of the P100 Gr/6061-T6 Al MMC is due to microstructural chlorides. Also, notice data (closed circle data points) from Gr (65 vol% fiber)/1100 Al MMC fabricated by pressure infiltration ( Ref 34 ) exposed to 0.5 M Na 2 SO 4 at 30 °C (86 °F); scan rate
More
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006091
EISBN: 978-1-62708-175-7
... ” in this article. Properties of composites for electrical make-break contacts Table 2 Properties of composites for electrical make-break contacts Nominal composition, % Manufacturing method (a) Density, g/cm 3 Electrical conductivity, % IACS Hardness Tensile strength Modulus of rupture Data...
Abstract
Electrical contacts are made of elemental metals, composites, or alloys that are made by the melt-cast method or manufactured by powder metallurgy (PM) processes. PM facilitates combinations of metals that ordinarily cannot be achieved by alloying. This article describes the processing, properties, and performance of electrical contacts based on PM or hybrid composite technologies with refractory metals and compounds. These metals and compounds include tungsten, molybdenum, carbide-based composites, and silver-base composites. The article explains composite manufacturing methods, namely, PM methods, internal oxidation, and hybrid consolidation. The availability of the refractory metals and compounds in various product forms are also reviewed.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006101
EISBN: 978-1-62708-175-7
... 1 21.0 0.24 7 156 70 90 HRB N/D 23 7.3 FX-2008-90HT … 90 100 (a) <1 21.0 0.24 5 159 74 36 HRC 58 HRC 27 7.3 All data based on single-pass infiltration. HT, heat treated; N/D, not determined for the purposes of this standard. Suffix numbers represent minimum...
Abstract
This article summarizes the general classification, mechanical properties, and applications of ferrous powder metallurgy (PM) materials for parts production. It discusses four principal ferrous PM alloy types: admixed elemental alloys, diffusion alloys, prealloys, and hybrid alloys. The article reviews the benefits and disadvantages as well as the effect of processing on the properties and material microstructure of these alloys. It contains tables that list the mechanical properties of various iron-copper and copper steels.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
...-matrix composites, superalloy-matrix composites, and intermetallic-matrix composites. It describes the processing methods of discontinuous aluminum MMCs which include casting processes, liquid-metal infiltration, spray deposition and powder metallurgy. The article provides useful information on aluminum...
Abstract
Metal-matrix composites (MMCs) are a class of materials with potential for a wide variety of structural and thermal applications. This article discusses the mechanical properties of MMCs, namely aluminum-matrix composites, titanium-matrix composites, magnesium-matrix composites, copper-matrix composites, superalloy-matrix composites, and intermetallic-matrix composites. It describes the processing methods of discontinuous aluminum MMCs which include casting processes, liquid-metal infiltration, spray deposition and powder metallurgy. The article provides useful information on aluminum MMC designation system and also describes the types of continuous fiber aluminum MMCs, including aluminum/boron MMC, aluminum/silicon carbide MMC, aluminum/graphite MMC, and aluminum/alumina MMC.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001044
EISBN: 978-1-62708-161-0
...) All data based on single-pass infiltration. (m) Codes for the stainless steel designations: N1, nitrogen alloyed, with good strength and low elongation; N2, nitrogen alloyed, with high strength and medium elongation; L, low carbon, with lower strength and highest elongation; HT, martensitic grade...
Abstract
Certain metal products can be produced only by powder metallurgy; among these products are materials whose porosity is controlled. Successful production by powder metallurgy depends on the proper selection and control of process variables: powder characteristics; powder preparation; type of compacting press; design of compacting tools and dies; type of sintering furnace; composition of the sintering atmosphere; choice of production cycle, including sintering time and temperature; and secondary operations and heat treatment. When the application of a powder metallurgy part requires high levels of strength, toughness, or hardness, the mechanical properties can be improved or modified by infiltration, heat treatment, or a secondary mechanical forming operation such as cold re-pressing or powder forging. The article also discusses the effect of the secondary processes on P/M mechanical properties.
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003397
EISBN: 978-1-62708-195-5
... Curing (SGC) ( Ref 13 ), a process developed by Cubital in Israel, also fabricates parts from photopolymer resins but in a different way than stereolithography ( Fig. 5 ). Resin is spread onto a platform, which is then exposed to ultraviolet light through a mask, which is printed from the layer data onto...
Abstract
This article reviews various rapid prototyping (RP) processes such as stereolithography, powder sintering, hot melt extrusion, sheet lamination, solid ground curing, and three-dimensional printing. It discusses the various material prototypes produced by RP technology. The list of materials includes particulate and fiber-reinforced polymers, ceramic-matrix composites, and metal-matrix composites. The article also provides information on freeform-fabrication techniques for composite part lay-up.
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003420
EISBN: 978-1-62708-195-5
... infiltration casting, liquid metal infiltration, spray deposition, and powder metallurgy methods. It describes the processing of continuous fiber-reinforced aluminum, discontinuously, reinforced titanium, and continuous fiber-reinforced titanium. The article concludes with information on work done to develop...
Abstract
Metal-matrix composites (MMCs) are a class of materials with a wide variety of structural, wear, and thermal management applications. This article discusses the primary processing methods used to manufacture discontinuous aluminum MMCs, namely, high-pressure die casting, pressure infiltration casting, liquid metal infiltration, spray deposition, and powder metallurgy methods. It describes the processing of continuous fiber-reinforced aluminum, discontinuously, reinforced titanium, and continuous fiber-reinforced titanium. The article concludes with information on work done to develop magnesium, copper, and superalloy MMCs.
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006569
EISBN: 978-1-62708-290-7
... , Dec . 2015 . 10.1063/1.4937809 61. “ 316 Stainless Steel Infiltrated with Bronze ,” ExOne , 2013 . [Online]. Available: http://www.hasmak.com.tr/yeni/dosyalar/images/Material-Data-316SS_EN.pdf . 62. Mortensen A. and Llorca J. , “ Metal Matrix Composites ,” Annu. Rev. Mater...
Abstract
This article focuses on binder-jetting technologies in additive manufacturing (AM) that produce metal artifacts either directly or indirectly. The intent is to focus on the most strategic and widespread uses of the binder jetting technology and review some of the challenges and opportunities for that technology. The discussion includes a historical overview and covers the major steps involved and the advantages of using the binder jetting process. The major steps of the process covered include printing, curing, de-powdering, and sintering.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
..., discontinuously reinforced composites and continuous-fiber-reinforced composites. Processing methods include cold pressing, sintering, hot pressing, reaction bonding, melt infiltration, directed metal oxidation, sol-gel and polymer pyrolysis, self-propagating high-temperature synthesis and joining. A table...
Abstract
Ceramic-matrix composites (CMCs) are being developed for a number of high-temperature and high-performance applications in industrial, aerospace, and energy conservation sectors. This article focuses on processing, fabrication, testing, and characterization methods of CMCs, namely, discontinuously reinforced composites and continuous-fiber-reinforced composites. Processing methods include cold pressing, sintering, hot pressing, reaction bonding, melt infiltration, directed metal oxidation, sol-gel and polymer pyrolysis, self-propagating high-temperature synthesis and joining. A table summarizes the properties of various ceramic reinforcements and industrial applications of these composites.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005227
EISBN: 978-1-62708-187-0
... and melt infiltration, used in the synthesis of MMCs. The article also considers the fundamentals of the process and presents a computational modeling of particle/solidification front interactions in metal-ceramic systems. The article concludes with information on nanocomposites. casting melt...
Abstract
This article discusses the solidification of a matrix alloy in cast metal matrix composites (MMCs). It begins with a discussion on the mixing techniques in reinforcement incorporation and wettability of reinforcement. It describes the solidification processes, such as stir mixing and melt infiltration, used in the synthesis of MMCs. The article also considers the fundamentals of the process and presents a computational modeling of particle/solidification front interactions in metal-ceramic systems. The article concludes with information on nanocomposites.
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006972
EISBN: 978-1-62708-439-0
..., and the nature of the L-PBF process all contribute to the potential of defect formation. All records, files, and data associated with each stage, including field performance, combine to form a digital thread. Steps performed before L-PBF typically include part design, CAD (of new or scanned geometry), materials...
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003112
EISBN: 978-1-62708-199-3
... with the mechanical and physical properties of ferrous P/M materials, which may depend on certain factors, namely microstructure, porosity, density, infiltration, re-pressing, chemical composition, and heat treatment. carbonyl iron powders compaction electrolytic iron powders ferrous powders mechanical...
Abstract
Iron powders are the most widely used powder metallurgy (P/M) material for structural parts. This article reviews low to medium density iron and low-alloy steel parts produced by the pressing and sintering technology. It explains different powder production methods, including Hoeganaes process, Pyron process, atomization of liquid metal, thermal decomposition and the electrodeposition process for carbonyl and electrolytic iron powders. It describes the types of compaction and sintering, explaining their effects of processing with designations. Further, the article deals with the mechanical and physical properties of ferrous P/M materials, which may depend on certain factors, namely microstructure, porosity, density, infiltration, re-pressing, chemical composition, and heat treatment.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003135
EISBN: 978-1-62708-199-3
... and nickel silver P/M parts, copper-nickel P/M parts, copper-lead P/M parts, copper-base P/M friction materials, copper-base P/M electrical contact materials, copper-base P/M brush materials, infiltrated parts, and oxide-dispersion-strengthened copper P/M materials. copper alloy powders copper powders...
Abstract
This article discusses the characteristics, properties, and production methods of copper powders and copper alloy powders. Bulk of the discussion is devoted to production and applications of powder metallurgy (P/M) parts, including pure copper P/M parts, bronze P/M parts, brass and nickel silver P/M parts, copper-nickel P/M parts, copper-lead P/M parts, copper-base P/M friction materials, copper-base P/M electrical contact materials, copper-base P/M brush materials, infiltrated parts, and oxide-dispersion-strengthened copper P/M materials.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003486
EISBN: 978-1-62708-195-5
... optimized for applications requiring slurry erosion resistance ( Ref 16 , 17 ). Processing was carried out by directed metal oxidation (see the article “Processing of Ceramic-Matrix Composites” in this Volume for details). Wear test data for the Al 2 O 3 -SiC p composite and other ceramic and metallic...
Abstract
The applications of discontinuously reinforced ceramic-matrix composites (CMCs) fall into four major categories, namely, cutting tool inserts; wear-resistant parts; aerospace and military applications; and other industrial applications, including engines and energy-related applications. This article provides examples for these four categories, with an emphasis on those applications/materials that have achieved commercial viability. The applications for continuous fiber ceramic composites are also summarized.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003374
EISBN: 978-1-62708-195-5
... no quantitative models are available for interphase optimization, various thermodynamic and materials science principles coupled with a growing body of experimental data allow us to understand the interphase as well as to qualitatively design the interphase. The tools available for analysis and design include...
Abstract
Fiber-matrix adhesion is a variable to be optimized in order to get the best properties and performance in composite materials. This article schematically illustrates fiber matrix interphase for composite materials. It discusses thermodynamics of interphase in terms of surface energy, contact angle, work of adhesion, solid surface energy, and wetting and wicking. The article describes the change in interphase depending on the reinforcing fiber such as glass fiber, polymeric fiber, and carbon fiber. It emphasizes fiber-matrix adhesion measurements by direct methods, indirect methods, and composite laminate tests. The effects of interphase and fiber-matrix adhesion on composite mechanical properties, such as composite on-axis properties, composite off-axis properties, and composite fracture properties, are also discussed.
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002465
EISBN: 978-1-62708-194-8
.... and Fiberite Inc. for resin-matrix composites, and as developed in-house for carbon- and metal-matrix products by other manufacturers, for various processing cycles. The following discussion provides data on matrix composition, manufacturing, and mechanical properties. Composition of Composites...
Abstract
This article describes the interaction of composition, manufacturing process, and composite properties of composites. The manufacturing process includes resin-matrix, metal-matrix, and carbon/carbon matrix processing. The article discusses various mechanical properties of composites. It explores how variations in the composition, manufacturing, shop process instructions, and loading/environmental conditions can affect the use of a composite product in a performance/service life operation.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003789
EISBN: 978-1-62708-177-1
... equipment and techniques and provides data on etchants and etching procedures. specimen grinding liquid-phase sintering macroexamination metallographic examination microstructure particle size analysis powder metallurgy alloys particle shape analysis specimen polishing specimen preparation...
Abstract
This article provides information on the microstructure of powder metal alloys and the special handling requirements of porous materials. It covers selection, sectioning, mounting, grinding, and polishing, and describes procedures, such as washing, liquid removal, and impregnation, meant to preserve pore structures and keep them open for analysis. The article compares and contrasts the microstructures of nearly 50 powder metal alloys, using them to illustrate the effect of consolidation and compaction methods as well as particle size, composition, and shape. It discusses imaging equipment and techniques and provides data on etchants and etching procedures.