Skip Nav Destination
Close Modal
Search Results for
cutting tool material
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1394
Search Results for cutting tool material
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003188
EISBN: 978-1-62708-199-3
... Abstract Selecting the proper cutting tool material for a specific machining application can provide substantial advantages, including increased productivity, improved quality, and reduced costs. This article begins with a description of the factors affecting the selection of a cutting tool...
Abstract
Selecting the proper cutting tool material for a specific machining application can provide substantial advantages, including increased productivity, improved quality, and reduced costs. This article begins with a description of the factors affecting the selection of a cutting tool material. This is followed by a schematic representation of their relative application ranges in terms of machining speeds and feed rates. The article provides a detailed account of chemical compositions of various tool materials, including high-speed tool steels, cobalt-base alloys, cemented carbides, cermets, ceramics, cubic boron nitride, and polycrystalline diamond. It compares the toughness, and wear resistance for these cutting tool materials. Finally, the article explains the steps for selecting tool material grades for specific application.
Image
Published: 01 January 1994
Image
Published: 01 December 1998
Image
Published: 01 December 1998
Fig. 3 Comparison of toughness and wear resistance for various cutting tool materials. Source: Metcut Research Associates, Inc.
More
Image
Published: 01 January 1989
Fig. 5 Cutting tool materials yield strength as a function of temperature. Lower curve is high-speed steel. Upper two curves are tungsten carbide. Source: Ref 1
More
Image
Published: 01 January 1989
Fig. 10 Abrasion resistance of PCD, PCBN, and other cutting tool materials. Machining parameters: depth of cut = 1.0 mm (0.040 in.); feed rate = 0.32 mm/rev (0.013 in./rev); approach angle = 45°; top rake = 0°; clearance = 6°; tool nose radius = 0.8 mm (0.030 in.); dry, no coolant. Workpiece
More
Image
Published: 01 January 1989
Fig. 1 Approximate speed ranges and applications of various cutting tool materials. Source: GTE Valenite Corporation
More
Image
Published: 31 August 2017
Fig. 28 Hardness and toughness of cutting tool materials. PCD, polycrystalline diamond; DLC, diamond-like carbon; PCBN, polycrystalline cubic boron nitride; PM HSS, powder metallurgy high-speed steel. Source: Ref 29
More
Image
Published: 31 August 2017
Fig. 33 Approximate speed ranges and applications of various cutting tool materials. PCD, polycrystalline diamond; CBN, cubic boron nitride; HSS, high-speed steel
More
Image
Published: 01 January 1989
Fig. 4 Effect of cutting speed and tool material in turning β-forged Ti-6Al-4V having 331 HB hardness. High-speed tool steel materials: A, M2; B, T15; and C, M42. Feed rate was 0.25 mm (0.010 in.). Depth of cut was 0.25 mm/rev (0.010 in./rev). Cutting fluid was phosphated oil. Tool life end
More
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002177
EISBN: 978-1-62708-188-7
... Abstract This article discusses the factors to be considered in selecting and evaluating machining tests for the purpose of evaluating cutting tool performance and workpiece machinability. It provides a brief description of cutting tool materials, such as high-speed steels, uncoated and coated...
Abstract
This article discusses the factors to be considered in selecting and evaluating machining tests for the purpose of evaluating cutting tool performance and workpiece machinability. It provides a brief description of cutting tool materials, such as high-speed steels, uncoated and coated carbides, cermets, ceramics, cubic boron nitride, and polycrystalline diamond. The article considers the matrices that represent the range of tests performed on candidate cutting tool materials: the workpiece matrix, the property matrix, and the operation matrix. Various machine tests used to evaluate cutting tools, including the impact test, turning test, and facing test, are described. The article lists the factors to be taken into consideration in measuring the machinability of a material. The article presents general recommendations for proper chip groove selection on carbide tools and concludes with information on machining economics.
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006306
EISBN: 978-1-62708-179-5
... on cutting tool life, and the importance of as-cast surface integrity on the machining variation. It presents examples of cutting tool materials selection for different cast iron grades, and describes the effects of coolants on the machining of cast irons. A chart showing different cutting materials...
Abstract
Machining of cast iron involves removing metal from the cast part, usually by cutting with a power-driven machine tool. This article discusses the factors that influence machinability, the methods used to evaluate machinability of cast irons, the effects of cast iron microstructure on cutting tool life, and the importance of as-cast surface integrity on the machining variation. It presents examples of cutting tool materials selection for different cast iron grades, and describes the effects of coolants on the machining of cast irons. A chart showing different cutting materials and cutting speed ranges for selected iron-carbon alloys is also presented. Different types of cutting tool wear observed during turning are schematically illustrated.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001320
EISBN: 978-1-62708-170-2
... productivity of carbide, cermet, and ceramic cutting tool materials used in machining operations. The useful life of cutting tools may be limited by a variety of wear processes, such as crater wear, flank wear or abrasive wear, builtup edge, depth-of-cut notching, and thermal cracks. The article provides...
Abstract
The classes of tool materials for machining operations are high-speed tool steels, carbides, cermets, ceramics, polycrystalline cubic boron nitrides, and polycrystalline diamonds. This article discusses the expanding role of surface engineering in increasing the manufacturing productivity of carbide, cermet, and ceramic cutting tool materials used in machining operations. The useful life of cutting tools may be limited by a variety of wear processes, such as crater wear, flank wear or abrasive wear, builtup edge, depth-of-cut notching, and thermal cracks. The article provides information on the applicable methods for surface engineering of cutting tools, namely, chemical vapor deposited (CVD) coatings, physical vapor deposited coatings, plasma-assisted CVD coatings, diamond coatings, and ion implantation.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006494
EISBN: 978-1-62708-207-5
... Abstract The horsepower requirements to cut various metal alloys provide an indication of the relative ease and cost of machining, but several other important factors include cutting tool material, chip formation, cutting fluids, cutting tool wear, surface roughness, and surface integrity...
Abstract
The horsepower requirements to cut various metal alloys provide an indication of the relative ease and cost of machining, but several other important factors include cutting tool material, chip formation, cutting fluids, cutting tool wear, surface roughness, and surface integrity. This article reviews these general machining factors as well as specific cutting tool and cutting parameters for the six basic chip-forming processes of turning, shaping, milling, drilling, sawing, and broaching. Best practices for each of the six chip-forming processes are suggested for optimized machining of aluminum alloys. The article lists the inherent disadvantages of machining processes that involve compression/shear chip formation. It discusses the machining of aluminum metal-matrix composites and nontraditional machining of aluminum, such as abrasive jet, waterjet, electrodischarge, plasma arc, electrochemical, and chemical machining.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003424
EISBN: 978-1-62708-195-5
... Abstract This article describes the machining operations of carbon fiber-reinforced epoxy, or carbon/epoxy thermoset composite materials, such as drilling, reaming, routing, trimming, end milling, slot milling, and facing. It reviews cutting tools for machining, including solid carbide, diamond...
Abstract
This article describes the machining operations of carbon fiber-reinforced epoxy, or carbon/epoxy thermoset composite materials, such as drilling, reaming, routing, trimming, end milling, slot milling, and facing. It reviews cutting tools for machining, including solid carbide, diamond plated, brazed diamond, diamond coated carbide, and polycrystalline cutting tools. The article also describes cutting tool materials that are used for peripheral milling, face milling, and the trimming of polymer-matrix composites.
Book Chapter
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002178
EISBN: 978-1-62708-188-7
... Abstract This article discusses the factors influencing cast iron machining and selection of cutting fluid and cutting tool materials. It presents a comparison of machinability of different types of cast iron, namely, gray cast iron, ductile cast iron, and malleable cast iron. In addition...
Abstract
This article discusses the factors influencing cast iron machining and selection of cutting fluid and cutting tool materials. It presents a comparison of machinability of different types of cast iron, namely, gray cast iron, ductile cast iron, and malleable cast iron. In addition, the article provides an overview of different methods used in the machining of cast iron, namely, turning, boring, broaching, planing and shaping, drilling, reaming, counterboring and spotfacing, tapping, milling, grinding, and honing and lapping. Nominal speeds and feeds for the machining of cast iron with single-point and box tools, ceramic tools, high-speed steel, and carbide tools are also tabulated.
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001033
EISBN: 978-1-62708-161-0
... Abstract The machinability of carbon and alloy steels is affected by many factors, such as the composition, microstructure, and strength level of the steel; the feeds, speeds, and depth of cut; and the choice of cutting fluid and cutting tool material. This article describes the influence...
Abstract
The machinability of carbon and alloy steels is affected by many factors, such as the composition, microstructure, and strength level of the steel; the feeds, speeds, and depth of cut; and the choice of cutting fluid and cutting tool material. This article describes the influence of the various attributes of carbon and alloy steels on machining characteristics. It lists the relative machinability ratings for some plain carbon steels, standard resulfurized steels, and several alloy steels. The addition of lead to carbon steels is one of the means of increasing the machinability of the steel and improving the surface finish of machined parts. Low carbon content of carburizing steels may be beneficial to tool life and production rate. The sulfur content of through-hardening alloy steels can significantly affect machining behavior. Cold drawing generally improves the machinability of steels containing less than about 0.2% carbon.
Book Chapter
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002173
EISBN: 978-1-62708-188-7
... Abstract High removal rate (HRR) machining involves the use of extremely rigid, high-power, high-precision machines, such as roll turning lathes, to achieve material removal rates far beyond the capacity of conventional machine tools. This article reviews the machine requirements and cutting...
Abstract
High removal rate (HRR) machining involves the use of extremely rigid, high-power, high-precision machines, such as roll turning lathes, to achieve material removal rates far beyond the capacity of conventional machine tools. This article reviews the machine requirements and cutting parameters of HRR machining. Machine components such as the lathe bed, tailstock, headstock, carriage, and tooling are detailed. The article also discusses the applications of HRR machining.
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002116
EISBN: 978-1-62708-188-7
... Abstract This article provides an overview of the independent and dependent variables of a machining process. Independent variables include workpiece material, specific machining processes, and tool materials and geometry. Cutting force and power, surface finish, and tool wear and failure...
Abstract
This article provides an overview of the independent and dependent variables of a machining process. Independent variables include workpiece material, specific machining processes, and tool materials and geometry. Cutting force and power, surface finish, and tool wear and failure are some dependent variables discussed. The article also describes the relations between the input variables and process behavior.
Image
Published: 01 January 1990
Fig. 23 Tool nose deformation versus vanadium carbide content of cutting tool materials containing 0 or 5% Al in the binder. Material cut was 4340 steel with a hardness of 300 HB. Source: Ref 33