1-20 of 316 Search Results for

cutting oils

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003189
EISBN: 978-1-62708-199-3
..., advantages and limitations of cutting and grinding fluids, such as cutting oils, water-miscible fluids, gaseous fluids, pastes, and solid lubricants along with their subtypes. It discusses the factors considered during the selection of cutting fluid, focusing on machinability (or grindability) of the...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001232
EISBN: 978-1-62708-170-2
... Abstract Abrasive finishing is a method where a large number of multipoint or random cutting edges are coupled with abrasive grains as a bond or matrix material for effective removal of material at smaller chip sizes. This article provides a broad overview of the various categories of abrasive...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001231
EISBN: 978-1-62708-170-2
..., stainless. (a) Treatment or condition. A, annealed; B, as-cast; C, as-forged; D, cold finished; E, hot finished; F, stress relieved; G, solution and precipitation treated; H, air quench, furnace temper; I, oil quench, furnace temper; J, salt quench, furnace temper. Source: Metal Cutting: Today's...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003179
EISBN: 978-1-62708-199-3
... variables. Suppliers of cutting equipment provide tables that give approximate gas pressures for various sizes and styles of cutting torches and tips, as well as recommended cutting speeds; these variables are operator controlled. Other variables include type and condition (scale, oil, dirt, flatness) of...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003213
EISBN: 978-1-62708-199-3
... Abstract Metal surfaces must often be cleaned before subsequent operations to remove unwanted substances such as pigmented drawing compounds, unpigmented oil and grease, chips and cutting fluids, polishing and buffing compounds, rust and scale, and miscellaneous contaminants. The article...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001221
EISBN: 978-1-62708-170-2
... Abstract This article describes the basic attributes of the most widely used metal surface cleaning processes to remove pigmented drawing compounds, unpigmented oil and grease, chips, cutting fluids, polishing and buffing compounds, rust and scale from steel parts, and residues and lapping...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... installation of the protective coating/lining system. Prior to beginning surface-preparation operations, many specifications will require a presurface-preparation inspection to verify the correction of fabrication defects and removal of surface contamination such as grease, oil, cutting compounds, lubricants...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003096
EISBN: 978-1-62708-199-3
..., water main pipe, oil country tubular goods, water well pipe, and pressure pipe. Pipes in suitable sizes, and most of the products classified as tubing, both seamless and welded, may be cold finished. Pressure tubes are given a separate classification by both the American Society for Testing and...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
.... 7 Stratified rust/rust scale Visible deposits of grease, oil, cutting compounds, or lubricants used in the fabrication process, or that have become deposited onto existing surfaces, must be removed prior to surface preparation. If not removed, the contamination can be spread around the...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003133
EISBN: 978-1-62708-199-3
..., drawing, production of flat rectangular wire, annealing, and coating, are discussed. The article also provides information on electrical insulation and jacketing techniques, including polymeric insulation, enamel insulation, and paper-and-oil insulation. continuous casting copper cable copper wire...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003048
EISBN: 978-1-62708-200-6
.... It also describes classifications and types, comparing and contrasting sealants made from oil-based caulks, asphalts, coal tar resins, latex acrylic sealants, polyvinyl acetate caulks, solvent acrylics, butyl sealants, polysulfides, polyurethanes, modified silicones, anaerobics, vinyl plastisols, and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... Abstract Stainless steels are iron-base alloys containing minimum of approximately 11% Cr, and owing to its excellent corrosion resistance, are used for wide range of applications. These applications include nuclear reactor vessels, heat exchangers, oil industry tubular, chemical processing...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000610
EISBN: 978-1-62708-181-8
... these steels. The austenitic stainless steel components include spring wires, preheater-reactor slurry transfer lines and gas lines of coal-liquefaction pilot plants, oil feed tubes and suction couch rolls of paper machines, cortical screws and compression hip screws of orthopedic implants, and Jewett...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003202
EISBN: 978-1-62708-199-3
..., austenitizing, quenching, preheating, and tempering commonly employed in certain steels. These are water-hardening tool steels, shock-resisting tool steels, oil-hardening cold-work tool steels, medium-alloy air-hardening cold-work tool steels, high-carbon high-chromium cold-work tool steels, hot-work tool...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005810
EISBN: 978-1-62708-165-8
... changes that occur in stabilizer bars as a result of oil quenching and tempering with those that resulted from austempering. It also discusses the production applications of austempering and the problems encountered in austempering together with their solutions. austempering dimension ferrous...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003806
EISBN: 978-1-62708-183-2
..., namely, oil and gas production, energy conversion systems, marine applications, and chemical processing. Emphasis is placed on the corrosion characteristics of the products, which are used in various applications of each industry. low-alloy steel alloy steel corrosion resistance oil and gas...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005824
EISBN: 978-1-62708-165-8
..., classification, selection, and maintenance are reviewed in detail. The article addresses the various reasons for quench oil variability and complications due to aging and contamination. brine cooling flow velocity heat-transfer coefficient oil quenchants polyacrylates polyalkylene glycol polymer...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004012
EISBN: 978-1-62708-185-6
... affecting die life and explains the effect of thread form on processing. It provides information on various fluids used in thread rolling to cool the dies and the work and to improve the finish on the rolled products. The article provides a comparison between thread rolling and cutting, as well as between...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... size, machining, descaling, cutting to length, and lubricating. It lists the advantages of the cold heading over machining. Materials selection criteria for dies and punches in cold heading are also described. The article provides examples that demonstrate tolerance capabilities and show dimensional...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003194
EISBN: 978-1-62708-199-3
... cutting rate. Other than the deburring or radiusing action, there is little effect of TCM on the surface of the workpiece. Surface stains may result if the workpiece is not clean, dry and free of oil before TCM. There can be a thin recast layer below thick burrs or fins. A thin oxide film is deposited on...