1-1 of 1 Search Results for

counterflow equilibrium powder classification

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006115
EISBN: 978-1-62708-175-7
... and the process variables of the sieving process. An appendix reviews dispersion of powders in liquids. counterflow equilibrium powder classification crossflow powder classification powder classification powder dispersion in liquids powder sampling powder sieving methods WHEN POWDER is analyzed...