1-20 of 579 Search Results for

corrosion rate

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003794
EISBN: 978-1-62708-183-2
... Abstract This article contains a corrosion rate conversion table, and a figure, that illustrate relationships among some of the units commonly used for corrosion rates of metals. corrosion rate Table 1 Relationships among some of the units commonly used for corrosion rates d is...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003819
EISBN: 978-1-62708-183-2
... Abstract The rate and form of corrosion that occur in a particular situation depend on many complex variables. This article discusses the rate of corrosion of lead in natural and domestic water depending on the degree of water hardness caused by calcium and magnesium salts. Lead exhibits...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003811
EISBN: 978-1-62708-183-2
... considered, by alloy casting users, in material selection. It presents compositions of cast steels tested in atmospheric corrosion in a tabular form. The rate of corrosion of a material in an environment can generally be estimated with confidence only from long-term tests. The article graphically presents...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003137
EISBN: 978-1-62708-199-3
... series of metals and alloys valid for dilute aqueous solutions, such as seawater and weak acids. It provides useful information on the effects of alloy compositions, selection for specific environments, and atmospheric corrosion of selected copper alloys. The article also tabulates the corrosion ratings...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003816
EISBN: 978-1-62708-183-2
... Abstract This article discusses the identifying characteristics of the forms or mechanisms of corrosion that commonly attack copper metals, as well as the most effective means of combating each. It tabulates corrosion ratings of wrought copper alloys in various corrosive media. The article...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003829
EISBN: 978-1-62708-183-2
... corrosion resistance; and corrosion applications of these precious metals. The article also tabulates the corrosion rates of these precious metals in corrosive environment, namely, acids, salts, and halogens. corrosion resistance fabricability gold iridium mechanical properties osmium oxidation...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003830
EISBN: 978-1-62708-183-2
... brass and other alloys, wrought zinc alloys, zinc oxide, and zinc chemicals. It discusses the corrosion and electrochemical behavior of zinc and its alloys in various environments, particularly in atmospheres in which they are most widely used. The article tabulates the corrosion rates of zinc and zinc...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003805
EISBN: 978-1-62708-183-2
..., chromium, nickel, and/or phosphorus, do produce significant reductions in the atmospheric corrosion rate in certain environments. See the article “Corrosion of Weathering Steels” in this Volume. At the levels present in low-alloy steels, the usual impurities have no significant effect on corrosion rate...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... alloy interface. The most widely used clad metal corrosion barrier material is copper-clad stainless steel (Cu/430 SS/Cu) for telephone and fiber optic cable shielding. In environments in which the corrosion rate of copper is high, such as acidic or sulfide-containing soils, the stainless steel acts...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... the parent coating may occur during induction preheat operations. Blistering sometimes happens after a sustained period of rainy weather or during early morning (following exposure to dew). If this happens, the heat-up rate must be slowed to prevent the blistering problem. While it is possible to...