Skip Nav Destination
Close Modal
By
Bennett P. Boffardi
By
George Y. Lai
By
S.R. Freeman
By
Greg Courval
By
Barbara A. Shaw, Wilford W. Shaw, Daniel P. Schmidt
Search Results for
corrosion protection method
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1341
Search Results for corrosion protection method
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 January 2001
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003672
EISBN: 978-1-62708-182-5
... Abstract This article discusses the factors affecting corrosion behavior. It describes galvanic corrosion and its protection methods. The article also provides information on coatings and inhibitors, which are used in corrosion protection. corrosion galvanic corrosion coatings...
Abstract
This article discusses the factors affecting corrosion behavior. It describes galvanic corrosion and its protection methods. The article also provides information on coatings and inhibitors, which are used in corrosion protection.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004220
EISBN: 978-1-62708-184-9
... Abstract This article discusses the generic situation of steel reacting with the environments found in structures. Two environments are specifically discussed: atmospheric and cementitious. The article describes the utility of different corrosion protection methods for atmospheric corrosion...
Abstract
This article discusses the generic situation of steel reacting with the environments found in structures. Two environments are specifically discussed: atmospheric and cementitious. The article describes the utility of different corrosion protection methods for atmospheric corrosion and cementitious systems. It presents examples of problems that have arisen in the corrosion performance of steel.
Book Chapter
Corrosion Inhibitors in the Water Treatment Industry
Available to PurchaseSeries: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003701
EISBN: 978-1-62708-182-5
... pretreatment methods of the incoming water and preboiler corrosion protection methods. It analyzes internal treatment and condensate treatment of boilers. The article discusses three types of cooling systems: once-through systems, open recirculating systems, and closed recirculating systems. The corrosion...
Abstract
The corrosion process that occurs in industrial systems is often difficult to discern until extensive deterioration has occurred. For boilers to function properly, the incoming water must be processed to meet the water quality required for the boiler. This article discusses pretreatment methods of the incoming water and preboiler corrosion protection methods. It analyzes internal treatment and condensate treatment of boilers. The article discusses three types of cooling systems: once-through systems, open recirculating systems, and closed recirculating systems. The corrosion processes which occur in water-recirculating systems and the effect of dissolved gases, temperature, pH, suspended solids, dissolved salts, and scale deposition on corrosivity of water, are also reviewed. The article also considers anodic and cathodic inhibitors and the control of corrosion in municipal water systems.
Book Chapter
General Introduction to Surface Engineering
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003212
EISBN: 978-1-62708-199-3
... specific processes that can be used to replace cadmium coatings, chromium coatings, and chromate conversion coatings, as well as alternatives to vapor degreasing and wipe solvent cleaners. Selected References Selected References • Corrosion Protection Methods , Corrosion , Vol 13 , ASM Handbook...
Abstract
This article is a general introduction to surface engineering of engineering components, providing an overview of the applications of surface treatments and the environmental protection regulations directly or indirectly related to surface engineering processes.
Book Chapter
High-Temperature Corrosion in Waste-to-Energy Boilers
Available to PurchaseSeries: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004157
EISBN: 978-1-62708-184-9
... wastage rates. Superheaters One of the very common corrosion protection methods for superheaters is the use of bimetallic tubes with alloy 625 cladding on the outer diameter of the carbon or chromium-molybdenum steel tube. The 625 cladding can be fabricated by overlay welding ( Ref 13...
Abstract
This article describes the corrosion modes in a waste-to-energy boiler. It discusses the corrosion protection and alloy performance with an emphasis on two main areas of the boiler: furnace water walls and super heaters.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004120
EISBN: 978-1-62708-184-9
... in a contract specification to provide a better definition of dissimilar metals and to provide guidance for corrosion-protection methods that can be used when galvanic couples cannot be avoided. The dissimilar metals charts in ASM Handbook , Vol 13B, 2005, are based on this standard. MIL-DTL-53072: Chemical...
Abstract
This article provides a perspective on United States (U.S.) Department of Defense (DOD) specifications, standards, handbooks, and related documents, as well as their role in the corrosion prevention and control activities in the U.S. military.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003698
EISBN: 978-1-62708-182-5
...-phase-corrosion inhibitors, or volatile corrosion inhibitors (VCIs) are discussed in this article. Practical methods of using VCIs for corrosion protection of ferrous and nonferrous alloys are discussed with some specific examples. Definition and Classification The definition of an inhibitor used...
Abstract
This article discusses the definitions, classifications, structural features, vapor pressure values, corrosion inhibition mechanisms, and methods of evaluation of vapor-phase-corrosion inhibitors or volatile corrosion inhibitors (VCIs). Practical methods of using VCIs for corrosion protection of aluminum, ferrous, and nonferrous alloys are discussed with specific examples. The article contains tables that summarize the applications of different VCIs used for protecting ferrous metals, copper and its alloys, and silver.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003696
EISBN: 978-1-62708-182-5
... recently developed electrochemical methods of corrosion control. The method was first used to protect plant-sized equipment in the late 1950s and became commercially successful in the early 1970s. It is currently used on a smaller scale than other corrosion control techniques due to the fundamental...
Abstract
This article presents a brief history and the uses of the anodic protection technique. It compares anodic and cathodic protection and describes the design considerations of the anodic protection system. The article discusses the specific requirements of equipment required for anodic protection. It also explains the applications and economic aspects of anodic protection, with examples.
Book Chapter
Selected Color Images
Available to PurchaseSeries: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004221
EISBN: 978-1-62708-184-9
... protection, where the object to be protected is made electrically negative or cathodic, has been a tool for preventing or at least reducing corrosion of large structures such as bridges, piers, ships, and buried pipelines. Evaluation of Corrosion Protection Methods Besides manipulating the electric...
Abstract
This article includes a collection of color images that aid in the identification and classification of forms of corrosion in industries and environments. It emphasizes the negative aspects of corrosion and examines the cost and the effort to test, evaluate, simulate, and prevent corrosion. The ability of corrosion to undo the best complex engineered systems has been documented.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004122
EISBN: 978-1-62708-184-9
... by the procurement contract, existing or new corrosion-control technologies used in a vehicle system need to be evaluated to determine their benefit. Accelerated corrosion test methods can demonstrate differences in performance of competing alternatives, identify areas requiring additional corrosion protection...
Abstract
This article presents a discussion on the U.S army's position on corrosion control for wheeled tactical vehicles. It addresses the army requirement for corrosion control. The U.S. Army Tank-automotive and Armaments Command (TACOM) defines the corrosion prevention and control requirements in the procurement document. The article summarizes requirements from a procurement document. As required by the procurement contract, corrosion-control technologies used in a vehicle system need to be evaluated to determine their benefit. The article provides information on testing systems, which help to meet the army's needs. It includes information on supplemental corrosion protection, which improves the corrosion resistance of a material.
Book Chapter
Analysis and Prevention of Corrosion-Related Failures
Available to PurchaseSeries: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003549
EISBN: 978-1-62708-180-1
... to clean adherent corrosion deposits. In cases where the protection of the fracture features is critical, softened acetate tape can be used to remove adherent deposits. This method also retains the deposits removed for further examination if necessary. If the failure analysis does not involve...
Abstract
This article provides an overview of the electrochemical nature of corrosion and analyzes corrosion-related failures. It describes corrosion failure analysis and discusses corrective and preventive approaches to mitigate corrosion-related failures of metals. These include: change in the environment; change in the alloy or heat treatment; change in design; use of galvanic protection; use of inhibitors; use of nonmetallic coatings and liners; application of metallic coatings; use of surface treatments, thermal spray, or other surface modifications; corrosion monitoring; and preventive maintenance.
Book Chapter
Simulated Service Corrosion Testing in Water
Available to PurchaseSeries: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003650
EISBN: 978-1-62708-182-5
... on crevice corrosion can be found in the articles “Crevice Corrosion” and “Evaluating Crevice Corrosion” in this Volume. NACE standards TM 0174 Laboratory Methods for the Evaluation of Protective Coatings Used as Lining Materials in Immersion Service This standard gives guidelines to assist...
Abstract
Simulated service testing includes exposures of either structural components or test specimens in environments that are representative of many general service situations. This article discusses the selection criteria of test specimens and methods of assessing the corrosion effects. The ASTM International and NACE International standards that are directly or indirectly applicable to simulated service corrosion testing in water are tabulated. The article also describes the effects of variable concentrations of dissolved carbonates, such as calcium, magnesium, and/or sodium, in water on corrosion.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004113
EISBN: 978-1-62708-184-9
.... Cathodic Protection Cathodic protection is a proven method of controlling corrosion of buried or submerged metallic structures. Design, installation, and maintenance of CP for the exterior bottoms of carbon steel ASTs and the external surfaces of USTs can mitigate corrosion. Cathodic protection...
Abstract
Steel storage tanks are the primary means for storing large volumes of liquids and gaseous products. The stored fluid could be water, but it could also be volatile, corrosive, and flammable fluid requiring special precautions for storage as well. Corrosion is generally worst where the tank is in contact with the soil. This article describes the soil characteristics and addresses cathodic protection (CP) criteria for submerged metallic piping systems. It provides information on the data required for designing a CP system, alone or in conjunction with a protective coating system. These data are collected from predesign site assessments, tank electrical characteristics, and soil-resistivity measurements. The article addresses NACE Standard RP0169, which gives requirements and desired characteristics for coating in conjunction with CP. It also explains the methods of protecting aboveground storage tanks and underground storage tanks.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004210
EISBN: 978-1-62708-184-9
... materials of construction, cathodic protection, inhibitors, and other methods has evolved into a science in its own right and has created industries devoted solely to corrosion control in specific areas. This article discusses the particular corrosion problems encountered and the methods of control used...
Abstract
This article discusses the particular corrosion problems encountered and the corrosion control methods used in petroleum production (i.e., upstream) and the storage and transportation of oil and gas (i.e., midstream) up to the refinery (i.e., downstream). These control methods include proper material selection, protective coatings, cathodic protection systems, use of inhibitors, use of nonmetallic materials, and control of the environment. The article reviews the aspects of corrosion that tend to be unique to corrosion as encountered in applications involving oil and gas exploration and production. It discusses corrosion problems that are specific to the various types of environments or equipment used in secondary recovery, including producing wells, producing flow lines, and injection wells. Corrosion mitigation methods and guidelines are also discussed for each type of environment.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003577
EISBN: 978-1-62708-182-5
..., localized corrosion, and stress-corrosion cracking, on corrosion testing and evaluation, and finally on the methods of corrosion protection. ...
Abstract
This article provides a summary of the concepts discussed in the articles under the Section “Fundamentals of Corrosion” in ASM Handbook, Volume 13A: Corrosion: Fundamentals, Testing, and Protection. In this section, the thermodynamic aspects of corrosion are descried first followed by a group of articles discussing the fundamentals of aqueous corrosion kinetics. The fundamentals of gaseous corrosion are addressed next. The fundamental electrochemical reactions of corrosion and their uses are finally described.
Book Chapter
Corrosion of Aluminum Components in the Automotive Industry
Available to PurchaseSeries: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004166
EISBN: 978-1-62708-184-9
... to be examined on a case-by-case basis. There are many unique features of any particular component or assembled module that dictate the methods that can be used to provide good corrosion protection. The guidelines offered are therefore of a general nature, and great care to detail and field experience must...
Abstract
This article provides an overview of the principle forms of corrosion that can occur on automotive aluminum components and offers general guidelines on how best to avoid these situations. It discusses the most common forms of aluminum corrosion such as stress-induced corrosion, cosmetic corrosion, crevice corrosion, and galvanic corrosion.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003687
EISBN: 978-1-62708-182-5
... of predicting the corrosion performance of a plated part. It reviews the designs of coating systems for optimal protection of the substrate. The article also discusses controlled weathering tests and accelerated tests used to predict and determine the relative durability of the coating. electroplated...
Abstract
This article discusses the various factors that affect the corrosion performance of electroplated coatings. It describes the effects of environment and the deposition process on substrate coatings. The article provides a discussion on the electrochemical techniques capable of predicting the corrosion performance of a plated part. It reviews the designs of coating systems for optimal protection of the substrate. The article also discusses controlled weathering tests and accelerated tests used to predict and determine the relative durability of the coating.
Book Chapter
Corrosion of Metallic Coatings
Available to PurchaseSeries: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004107
EISBN: 978-1-62708-184-9
... discusses thermal spray, hotdipping, and electroplating processes used to apply coatings in steel structures. It describes the corrosion attributes of the resulting coatings and discusses the methods of protecting steel from corrosion using aluminum and zinc coatings. corrosion corrosion protection...
Abstract
A sacrificial coating applied to a steel substrate can add 20 years or more of life to the substrate, depending on its thickness and composition. Different techniques to apply sacrificial coatings offer various characteristics that contribute to corrosion resistance. This article discusses thermal spray, hotdipping, and electroplating processes used to apply coatings in steel structures. It describes the corrosion attributes of the resulting coatings and discusses the methods of protecting steel from corrosion using aluminum and zinc coatings.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003809
EISBN: 978-1-62708-183-2
... methods of protecting steels from corrosion using paints: barrier coatings, passivation of the steel surface, and galvanic protection. In barrier protection, the paint film retards the diffusion of water, oxygen, or salts to the steel substrate. In 1952, the permeability of water and oxygen through...
Abstract
This article describes the paint systems generally used to protect steel structures, steel sheet, and bridges from corrosion, and how they deter corrosion. It provides a discussion on the basic design criteria of steel structures for corrosion protection. The article also explains the differences between prepaint and postpaint, and the steps involved in prepaint processing of steel. It presents the selection guideline for paint system evaluation. The advantages of corrosion protection are also discussed.