Published: 15 January 2021
Fig. 38 Corrosion pits and stress-corrosion cracking in type 316 stainless steel evaporator tubes. (a) View of the rust-stained and pitted area near the top of the evaporator tube. A myriad of fine, irregular cracks is discernible visually, although it is not clear in the photograph. (b) View More