Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006059
EISBN: 978-1-62708-172-6
... copper copper alloys corrosion control ductile iron ferrous metals localized corrosion microbiologically influenced corrosion municipal wastewater systems protective coatings reinforced concrete pipes wastewater treatment THE PURPOSE OF THIS ARTICLE is to acquaint the reader with useful...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... Abstract This article describes the principal cladding processes and methods for calculating properties of clad metals. It reviews the designing processes of clad metals to achieve specific requirements. The article discusses six categories of clad metal systems designed for corrosion control...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005925
EISBN: 978-1-62708-166-5
... Abstract Temperature control in heat treating is of paramount importance in maintaining the quality and achieving the desired metallurgical results. This article provides a detailed account of the factors affecting temperature control in heat treating furnaces, with information on temperature...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... Abstract This article discusses the concepts of quality control (QC) and quality assurance (QA), and clarifies the differences and similarities in the roles and responsibilities of QC and QA personnel. It describes the inspection procedures used to verify proper surface preparation and...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003199
EISBN: 978-1-62708-199-3
... Abstract Control of temperature and furnace atmospheres has become increasingly critical to successful heat treating. Temperature instrumentation and control systems used in heat treating include temperature sensors, controllers, final control elements, measurement instruments, and set-point...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006286
EISBN: 978-1-62708-169-6
... Abstract Quenching is a widely used technique to strengthen titanium alloys. This article presents the metallurgical and structural background underlying the specific techniques applied in the quenching of various titanium alloys, and the ways to control and reduce residual stresses induced...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005968
EISBN: 978-1-62708-166-5
... Abstract The heat treatment of steel involves a number of processes (such as stress relieving, normalizing, annealing etc) to condition the microstructure and obtain desired properties. This article discusses typical heat treating process control procedures for carbon and low-alloy steels, as...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003839
EISBN: 978-1-62708-183-2
... concludes with a description on the corrosion control of MMCs using protective coatings and inhibitors. aluminum chemical degradation copper corrosion control depleted uranium metal matrix composites galvanic corrosion lead magnesium metal matrix composites processing-induced corrosion...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003823
EISBN: 978-1-62708-183-2
...-corrosion, and fretting corrosion. The article explains the effects of tin content in zirconium and effects of fabrication on corrosion. Corrosion control measures for all types of corrosion are also highlighted. The article concludes with information on the safety precautions associated with handling of...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006782
EISBN: 978-1-62708-295-2
... Abstract Corrosion is the deterioration of a material by a reaction of that material with its environment. The realization that corrosion control can be profitable has been acknowledged repeatedly by industry, typically following costly business interruptions. This article describes the...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003805
EISBN: 978-1-62708-183-2
... them, the Hoar method, estimated for 1997 that the cost was 5258 billion yen (40.5 billion U.S. dollars), which was equivalent to 1.02% of the gross national product of Japan. The estimated total was doubled when indirect cost was taken into consideration ( Ref 2 ). Corrosion control methods are...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... quality-control checks, such as thickness measurements and holiday tests. An alternative is to use a welded internal coupling that becomes an integral part of the pipeline ( Ref 61 ). The coupling is precoated and uses O-ring seals to prevent corrosive materials from reaching the uncoated weld area...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005654
EISBN: 978-1-62708-198-6
... stage I and stage II. Fractographically, more or less featureless facets were observed, but at higher magnification there was a complex topography with crystallographically controlled propagation and striations in some locations. Obstacles in the crack path were said to provide barriers that could stop...