1-20 of 283 Search Results for

copper tubular products

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003132
EISBN: 978-1-62708-199-3
...Abstract Abstract This article discusses the applications and tensile properties of selected copper tube alloys, as well as the methods for producing copper tubular products, namely extrusion and rotary piercing. It explains the methods available for the finishing of copper tubular products...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001066
EISBN: 978-1-62708-162-7
... of fabrication, and good heat-transfer properties. This article describes the manufacturing processes used to produce wrought copper and copper alloys in the form of sheet and strip products, tubular products, and wire and cable. Common processes include melting, casting, hot and cold rolling, milling...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003096
EISBN: 978-1-62708-199-3
..., and by the refrigeration industry for refrigerant lines. It is made by forming copper-coated strip into a tubular section with double walls, using either single-strip or double strip construction. The tubing is then heated in a reducing atmosphere to join all mating surfaces completely. The resulting product is thus...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004005
EISBN: 978-1-62708-185-6
... or shearing is generally used to produce solid slugs. Machining (as in a lathe) or cold forming in auxiliary equipment is seldom used unless a hole in the slug, or some other modification, is required. The following examples describe typical production practice for extruding parts from copper and brass...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001020
EISBN: 978-1-62708-161-0
... of the manufacturer. (f) Electric resistance or electric flash. (g) Nickel, chromium, and copper combined shall not exceed 0.5%. (h) Alloys are typically added in various amounts, even though it is not specified in API Specification 5CT. (i) Carbon content may be increased to 0.55% max if the product...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006449
EISBN: 978-1-62708-190-0
... of nondestructive examination methods based on flaw type and product stage is presented in a table. The article also discusses in-service inspection of tubular products and presents an example that illustrates the importance of nondestructive testing (NDT) for welds in austenitic stainless steel tubing...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001119
EISBN: 978-1-62708-162-7
... occupational exposures have since been well documented, particularly in the last 20 years. Available data suggest a dose-response relationship ( Ref 40 ). Workers engaged in the production of arsenic-containing pesticides showed increased lung cancer mortality ( Ref 42 ), and workers involved in copper...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001376
EISBN: 978-1-62708-173-3
..., flyer plate mass, standoff distance, and/or preset angle. These process variables are normally controlled to provide: Transition joint components are produced by explosion welders at their production facilities and then provided in the form of blocks, strips, or tubular couplings to equipment...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001442
EISBN: 978-1-62708-173-3
..., these may drop out, having played only a small role in resisting abrasion. Several tungsten carbide composites are available in a variety of tubular product forms. Popular compositions are 40, 50, 55, and 60 wt% tungsten carbide, with a carbon steel tube making up the balance. For each composition...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004014
EISBN: 978-1-62708-185-6
... and in-line flow-forming process. Typical mechanical properties of flow-formed materials in various conditions are summarized in a table. Proper process controls and subsequent product qualification tests are critical to assure optimal performance of the flow-formed tubular component. The article discusses...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005891
EISBN: 978-1-62708-167-2
... of the workpiece is widely used to selectively heat tubular products. Applications such as localized stress relieving, brazing, preheating prior to parting, induction welding, bending, and annealing of welds can benefit from the ability of induction to heat selective areas. Stress relieving of steel tube/pipe...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005135
EISBN: 978-1-62708-186-3
... on copper and brass. Tubular sections are converted into a variety of products. One or more forming processes can be used, including press forming, contour roll forming, tube spinning, rotary swaging, hydraulic bulging, explosive forming, electromagnetic forming, and electrohydraulic forming...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003983
EISBN: 978-1-62708-185-6
...′ and 0.13 mm (0.005 in.) ovality. The production rate was increased to 750 pieces per hour. Blades for high-voltage switches were swaged from annealed copper tubes ( Fig. 22 ) in three operations using a two-die rotary machine. Each die was 195 mm (7 3 4 in.) long, 180 mm (7 1 8...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005257
EISBN: 978-1-62708-187-0
... spinning. Horizontal centrifugal casting is mainly used to cast pieces with a high length-to-diameter ratio or with a uniform internal diameter. Products include pipe, tubes, bushings, cylinder sleeves (liners), and cylindrical or tubular castings that are simple in shape. On the other hand, vertical...
Book Chapter

Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003990
EISBN: 978-1-62708-185-6
... portion of the workpiece at any one time. Fig. 6 Schematic of rotary forging setup for the forming of a copper alloy seal fitting used in high-pressure piping Abstract Abstract Radial forging is a hot- or cold-forming process that uses two or more radially moving anvils or dies...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003162
EISBN: 978-1-62708-199-3
... in a variety of tubular product forms. Popular compositions are 38, 50, 55, and 60 wt% tungsten carbide, with the carbon steel tube making up the balance. For each composition, several carbide size ranges are available. As an example, for the 60% WC oxyacetylene welding consumable, four mesh size ranges...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005834
EISBN: 978-1-62708-167-2
..., is the most common induction heat treating operation, improving the strength, wear, and fatigue properties of steels. Steel tubular products, for example, lend themselves quite readily to hardening by induction in continuous line operations. Tempering of steel by induction, although not as common as induction...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006527
EISBN: 978-1-62708-207-5
... Handbook , Altan T. , Ed., Springer , 1998 10.1007/978-3-642-58857-0 46. Mills Products, Tubular Hydroforming Aluminum: 5 Things to Keep in Mind . https://millsproducts.com/tubular-hydroforming-aluminum/ 47. Hirt G. and Bambach M. , Incremental Sheet Forming , Sheet...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003662
EISBN: 978-1-62708-182-5
... the investigator some control over the test design. In contrast, the testing of tubular products may be dictated by the available mill-produced OD and whether the products are formed to English or metric dimensions. The combination of product form and selected crevice device can accurately reproduce or closely...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006813
EISBN: 978-1-62708-329-4
... the cited references. New installations are particularly vulnerable to crevice corrosion because of insufficient time for a protective film or scale to form on the surface before the onset of corrosion. Copper alloys are also susceptible to crevice corrosion, forming similar corrosion products...