1-20 of 1772

Search Results for copper base alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005191
EISBN: 978-1-62708-187-0
... Abstract This article provides accessible information on the thermodynamic properties of liquid aluminum-base and copper-base alloys with the help of phase diagrams. It contains tables that compile the thermodynamic data in the form of activities, activity coefficients, partial molar thermal...
Image
Published: 01 December 2008
Fig. 27 Flow rates of copper-base alloys through tapered sprues of varying diameter and height More
Image
Published: 09 June 2014
Fig. 8 Ultimate tensile strength of various age-hardenable copper-base alloys as a function of their electrical conductivity. Five important groups are highlighted: copper titanium (left), copper beryllium (center), copper chromium (bottom right), copper silver (center right) and copper More
Image
Published: 01 January 2002
Fig. 2 Wear surface by cavitation of copper-base alloy in a lubricated gearbox. Courtesy of CETIM More
Image
Published: 31 August 2017
Fig. 4 Liquidus temperature determined for an aluminum-copper-base alloy. Source: Ref 13 More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... and composition of the following types of bearing materials: tin-base alloys, lead-base alloys, copper-base alloys, and aluminum-base alloys. It also briefly discusses the following types of bearing materials: zinc-base alloys, silver-base alloys, gray cast irons, cemented carbides, and nonmetallic bearing...
Book Chapter

Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
..., bimetal systems, and trimetal systems. The article describes the designations, nominal compositions, mechanical properties, and applications of various sliding bearing alloys: tin-base alloys, lead-base alloys, copper-base alloys, aluminum-base alloys, silver-base alloys, zinc-base alloys, additional...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003160
EISBN: 978-1-62708-199-3
... and properties (mechanical and physical) of commercial SMA alloys, namely nickel-titanium alloys and copper-base alloys. applications of shape memory alloys copper base alloys general characteristics mechanical properties nickel-titanium alloys physical properties processing of shape memory alloys...
Book Chapter

By Sabit Ali
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006281
EISBN: 978-1-62708-169-6
... Abstract Bronzes generally are used to describe many different copper-base alloys in which the major alloying addition is neither zinc nor nickel. They are generally classified by their major alloying elements, for example, tin bronzes with phosphorus used as a deoxidizer, aluminum bronzes...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006422
EISBN: 978-1-62708-192-4
... section. It provides a discussion on hot rolling, cold rolling, and warm rolling, as well as lubrication in rolling. The article reviews the lubrication for iron-base and nickel-base materials, light metals, copper-base alloys, and titanium alloys. It discusses the wear mechanism in rolling: abrasion...
Image
Published: 31 December 2017
Fig. 9 Strength retention at elevated temperatures for selected bearing alloys. (a) Copper-base alloys. (b) Aluminum-base alloys. (c) Zinc-base alloys. (d) Lead-base alloys and tin-base alloys More
Book Chapter

By Derek E. Tyler, Richard P. Vierod
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005288
EISBN: 978-1-62708-187-0
.... In a general timeline of developments ( Table 1 ), the breakthrough in continuous casting of nonferrous alloys can be credited to Eldred in 1930 ( Ref 2 ). He developed a machine using graphite as the mold material to cast copper rods and later a number of copper-base alloys. Prior to that, the continuous...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... the intended function is decreased. The article addresses factors that may cause failures in castings for each metal type, starting with gray iron and progressing to ductile iron, steel, aluminum, and copper-base alloys. It describes the general root causes of failure attributed to the casting material...
Image
Published: 01 January 2005
Fig. 35 Alligatoring in a rolled slab. This defect is thought to be caused by nonhomogeneous deformation and nonuniform recrystallization during primary rolling of such metals as zinc alloys, aluminum-magnesium alloys, and copper-base alloys. Courtesy of J. Schey, University of Waterloo More
Book Chapter

By Darel E. Hodgson, Ming H. Wu, Robert J. Biermann
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001100
EISBN: 978-1-62708-162-7
... them using differential scanning calorimeter (DSC) techniques as well as other methods. The article examines the most common shape memory alloys, namely, nickel-titanium and copper-base SMAs, and provides information on their respective properties. biomedical applications copper-base shape...
Image
Published: 01 January 2001
250, Naval brass, and phosphor bronze are copper- based alloys. CA, DA, high-carbon steels. HE 15-W, Duralumin aluminum alloy. Ti 715, titanium alloy More
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005303
EISBN: 978-1-62708-187-0
... as being prone to surface cracking and porosity problems. Casting characteristics of copper can be improved by small additions of elements such as beryllium, silicon, nickel, tin, zinc, chromium, and silver. The copper-base casting alloy family can be subdivided into three groups according...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
... weldability of specific metals and alloys by arc welding processes Base metals welded Welding processes Shielded metal arc Gas tungsten arc Plasma arc Submerged arc Gas metal arc Flux cored arc Aluminum C A A No A No Copper-base alloys   Brasses No C C No C No   Bronzes...
Book Chapter

By David V. Neff
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005353
EISBN: 978-1-62708-187-0
... E.F. , Principles of Magnesium Technology , Pergamon Press , 1966 10. Trojan P.K. , Ostrom T.R. , and Flinn R.A. , Melt Control Variables in Copper Base Alloys , Trans. AFS , 1982 , p 729 ; “High Conductivity Copper Alloys,” Bulletin 43, Foseco, Inc. , 1972 11...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003145
EISBN: 978-1-62708-199-3
... use in alloys, the most important of which are tin-base soft solders and bearing alloys and copper-base bronzes. Tin Production Tin is produced from both primary and secondary resources. Secondary tin is produced from recycled materials (see the Section “Recycling and Life-Cycle Analysis...