Skip Nav Destination
Close Modal
By
Robert Goldstein
By
Murali D. Tumuluru, Hongyang Zhang, R. (Bob) Matteson
Search Results for
continuous seam welds
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 365
Search Results for continuous seam welds
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005607
EISBN: 978-1-62708-174-0
... for ultrasonic metal welding. It details the personnel requirements, advantages, limitations, and applications, namely, wire welds, spot welds, continuous seam welds, and microelectronic welds of ultrasonic metal welding. clamping force coalescence continuous seam welds high-frequency vibratory energy...
Abstract
Ultrasonic metal welding is a solid-state welding process that produces coalescence through the simultaneous application of localized high-frequency vibratory energy and moderate clamping forces. This article discusses the parameters to be considered when selecting a suitable welder for ultrasonic metal welding. It details the personnel requirements, advantages, limitations, and applications, namely, wire welds, spot welds, continuous seam welds, and microelectronic welds of ultrasonic metal welding.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001384
EISBN: 978-1-62708-173-3
... Abstract This article begins with a discussion on the advantages and limitation of ultrasonic welding (USW). It describes variations of the USW process which can produce different weld geometries. These variations are helpful in producing spot welds, line welds, continuous seam welds, ring...
Abstract
This article begins with a discussion on the advantages and limitation of ultrasonic welding (USW). It describes variations of the USW process which can produce different weld geometries. These variations are helpful in producing spot welds, line welds, continuous seam welds, ring welds, and microelectronic welds. The article provides information on the functions of USW personnel and describes the special conditions in USW which include the condition of the surface, the use of an interlayer, and the control of resonance. It concludes with a description on the weld quality, the influencing factors, surface appearance and deformation, and metallographic examination.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005608
EISBN: 978-1-62708-174-0
... together under pressure by circular electrodes. The resulting weld is a series of overlapping spot welds made progressively along a joint by rotating the electrodes.” Seam welding machines are capable of making two types of lap joint. A continuous, pressure-tight joint ( Fig. 1 ) is produced...
Abstract
This article describes the process applications, advantages, and limitations of resistance seam welding. The fundamentals of lap seam welding are also reviewed. The article details the types of seam welds, namely, lap seam welds and mash seam welds, and the processing equipment used for lap seam welding. The primary factors used to determine the selection of electrodes, including alloy type and wheel configuration, are reviewed. The article also describes weld quality and process control procedures.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005583
EISBN: 978-1-62708-174-0
... of butt joints in pipe. Pipes as large as 305 mm (12 in.) in diameter with wall thicknesses up to 8 mm (5/16 in.) were welded. The pipe ends were fitted and pressed together, then were induction heated to the forge-welding temperature in approximately 60s. 1949—Forge welding of continuous seams...
Abstract
High-frequency resistance welding (HFRW) is a process that uses high-frequency currents to concentrate the welding heat at the desired location. This article focuses on the fundamentals, advantages, limitations, and applications of HFRW. It discusses the personnel and equipment requirements as well as safety considerations necessary for the process. The article concludes with a discussion on the techniques for inspection and quality control of HFRW.
Book Chapter
Contour Roll Forming
Available to PurchaseSeries: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005126
EISBN: 978-1-62708-186-3
... the tubes as they are produced on the machine. It describes the roll design for tube rolling and reviews the seam welding operations of pipe and tubing. The article discusses cross-sectional tolerances, the reshaping of round tubing, and factors that affect the quality, accuracy, and surface finish...
Abstract
Contour roll forming is a continuous process for forming metal from sheet, strip, or coiled stock into desired shapes of uniform cross section by feeding the stock through a series of roll stations equipped with contoured rolls. This article discusses the materials, roll-forming machines, tooling, and auxiliary equipment used in contour roll forming and its process variables. Tooling used in roll forming includes forming rolls and dies for punching and cutting off the material. The article discusses the additional tooling required in tube mills to weld, size, and straighten the tubes as they are produced on the machine. It describes the roll design for tube rolling and reviews the seam welding operations of pipe and tubing. The article discusses cross-sectional tolerances, the reshaping of round tubing, and factors that affect the quality, accuracy, and surface finish.
Book Chapter
Procedure Development and Practice Considerations for Resistance Welding
Available to PurchaseSeries: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001443
EISBN: 978-1-62708-173-3
... either continuously or intermittently. Additional information is available in the article “Resistance Seam Welding” in this Volume. Seam Welding Machines A seam welding machine is similar in construction to a spot welding machine, except that one or two electrode wheels are substituted...
Abstract
Resistance welding (RW) encompasses a group of processes in which the heat for welding is generated by the resistance to the flow of electrical current through the parts being joined. The three major resistance welding processes are resistance spot welding (RSW), resistance seam welding (RSEW), and projection welding (PW). This article addresses the considerations for using these processes to join specific types of materials. It discusses the process variations, applicability, advantages, and limitations of these resistance welding processes. The article provides information on flash welding, high-frequency resistance welding, and capacitor discharge stud welding. It concludes with a discussion on resistance welding of stainless steels, aluminum alloys, and copper and copper alloys.
Book Chapter
Magnetic Flux Controllers in Induction Heating and Melting
Available to PurchaseSeries: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005846
EISBN: 978-1-62708-167-2
..., and linear coils. It provides information on the role of magnetic flux controllers for whole-body and local area mass-heating applications, continuous induction tube welding, seam-annealing inductors, and various induction melting systems, namely, channel-type, crucible-type, and cold crucible systems...
Abstract
Magnetic flux controllers are materials other than the copper coil that are used in induction systems to alter the flow of the magnetic field. This article describes the effects of magnetic flux controllers on common coil styles, namely, outer diameter coils, inner diameter coils, and linear coils. It provides information on the role of magnetic flux controllers for whole-body and local area mass-heating applications, continuous induction tube welding, seam-annealing inductors, and various induction melting systems, namely, channel-type, crucible-type, and cold crucible systems. The article also describes the benefits of the flux controllers for induction heat treating processes such as single-shot and scanning.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001365
EISBN: 978-1-62708-173-3
... ), or a wire-feed system in which a copper wire is fed into a groove on the wheel. This wire-feed process continuously provides a new copper surface for contact with the work metal ( Fig. 4 ). Fig. 3 Setup for foil butt seam welding of a table leg made of low-carbon steel. Dimensions given in inches...
Abstract
Resistance seam welding (RSEW) is a process in which the heat generated by resistance to the flow of electric current in the work metal is combined with pressure to produce a welded seam. This article discusses the various classes of the RSEW process, namely roll spot welding, reinforced roll spot welding, and leak-tight seam welding. It provides information on the applications of lap seam weld, mash seam weld, and butt seam weld. The article reviews the advantages and limitations of seam welding compared to resistance spot welding, projection welding, and laser welding. It describes the four basic types of resistance seam weld machines: circular, longitudinal, universal, and portable. The article concludes with a discussion on weld quality and process control for seam welding.
Book Chapter
Procedure Development and Practice Considerations for Resistance Welding
Available to PurchaseSeries: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005640
EISBN: 978-1-62708-174-0
... with seam welding. It concludes with a discussion on the welding equipment and other factors associated with resistance spot and seam welding. aluminum alloys copper alloys electrode force low-carbon steel resistance spot welding seam welding stainless steel surface preparation weld lobe weld...
Abstract
This article describes the significance of the three variables that affect the resistance spot welding process: welding current, electrode force, and welding time. It presents the effects of weld spacing and surface preparation on weld quality. The article elaborates the typical sequence of steps for determining the satisfactory conditions for spot welding and the mechanical aspects that affect this process. It considers the effects of process variables on the weld lobe. The article reviews surface preparation, part fit-up, electrode drives, weld parameters, and tests associated with seam welding. It concludes with a discussion on the welding equipment and other factors associated with resistance spot and seam welding.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006514
EISBN: 978-1-62708-207-5
...) Leaktight seam welding (nugget overlap) Seam welding consists of a series of overlapping weld nuggets capable of forming a gastight or liquidtight seam along the length of a joint. The weld may be made with overlapping weld nuggets, a continuous weld nugget, or by forging the joint as it is heated...
Abstract
The resistance welding processes commonly employed for joining aluminum are resistance spot welding, resistance seam welding, resistance roll welding, upset and flash welding for butt joining welding, and high-frequency resistance welding. This article discusses the general factors affecting resistance welding: electrical and thermal conductivities, rising temperature, plastic range, shrinkage, and surface oxide. It reviews the weldability of base materials such as Alclad alloys and aluminum metal-matrix composites. The article describes the joint design and welding procedures for resistance spot welding, as well as the joint type, equipment, and welding procedures for seam and roll spot welding. It concludes with information on flash welding, high-frequency welding, and cross-wire welding.
Book Chapter
Solid-State Welding Processes
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003209
EISBN: 978-1-62708-199-3
..., essentially parallel to the weld interface, while static force is applied perpendicular to the interface. Spot welding and continuous seam welding can be accomplished by this method. In spot welding, the duration of the ultrasonic pulse (usually 1 s or less) is selected according to the thickness...
Abstract
This article describes the mechanism, advantages and disadvantages, fundamentals, capabilities, variations, equipment used, and weldability of metals in solid-state welding processes, including diffusion bonding, explosion welding, friction welding, ultrasonic welding, upset welding, and deformation welding.
Book Chapter
Other Fusion Welding Processes
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003208
EISBN: 978-1-62708-199-3
... before welding have a major influence in determining the current flow and concentration in continuous seam welding by both processes. The depth to which current flows depends on the frequency and the resistive and magnetic properties of the workpiece. At higher frequencies, current flow is shallower...
Abstract
This article discusses the principles of operation, equipment needed, applications, and advantages and disadvantages of various fusion welding processes, namely, oxyfuel gas welding, electron beam welding, stud welding, laser beam welding, percussion welding, high-frequency welding, and thermite welding.
Book Chapter
Resistance Welding
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003207
EISBN: 978-1-62708-199-3
... of spot welds is made without retracting the electrode wheels or releasing the electrode force between spots, although the electrode wheels may advance either continuously or intermittently. Advantages and Limitations Advantages Advantages of seam welding, compared to resistance spot welding...
Abstract
This article presents a detailed account of the welding parameters, equipment needed, applications, advantages, limitations, and the process variables affecting various types of resistance welding operations, namely, resistance spot welding, resistance seam welding, resistance projection welding, and flash welding.
Book Chapter
Steel Tubular Products
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003096
EISBN: 978-1-62708-199-3
... temperature. The heated stock is roll formed into cylindrical shape as it emerges from the furnace; additional heat is usually provided by an oxygen or air jet impinging on the seam edges, and the tube passes through constricting rolls where the seam edges are welded by the pressure of the rolls. Continuous...
Abstract
This article discusses the classifications, specifications, applications and methods for producing welded and seamless steel tubular products, including pipes and tubes. Common types of pipes include standard pipe, conduit pipe, piling pipe, pipe for nipples, transmission or line pipe, water main pipe, oil country tubular goods, water well pipe, and pressure pipe. Pipes in suitable sizes, and most of the products classified as tubing, both seamless and welded, may be cold finished. Pressure tubes are given a separate classification by both the American Society for Testing and Materials (ASTM) and producers. The term tube covers three groups, including pressure tubes, structural tubing, and mechanical tubing.
Image
Schematic of a continuous high-frequency induction longitudinal seam tube-w...
Available to Purchase
in Magnetic Flux Controllers in Induction Heating and Melting
> Induction Heating and Heat Treatment
Published: 09 June 2014
Fig. 21 Schematic of a continuous high-frequency induction longitudinal seam tube-welding system. Source: Ref 13
More
Image
Resistance seam welding of an aircraft integral wing fuel tank using contin...
Available to PurchasePublished: 30 November 2018
Fig. 9 Resistance seam welding of an aircraft integral wing fuel tank using continuous electrode motion. Dimensions given in inches
More
Image
Setup for foil butt seam welding of a table leg made of low-carbon steel. D...
Available to PurchasePublished: 01 January 1993
Fig. 3 Setup for foil butt seam welding of a table leg made of low-carbon steel. Dimensions given in inches Equipment specifications and welding parameters Power supply 440 V, single phase Welding machine Automatic, longitudinal, with movable carriage for upper electrode
More
Image
Examples of how design and assembly can affect localized corrosion by creat...
Available to PurchasePublished: 01 January 2002
on the concrete support. (i) Continuous welding is necessary for horizontal stiffeners to prevent the formation of traps and crevices. (j) Square sections formed from two L-shaped members require continuous welding to seal out the external environment. Source: Ref 5
More
Image
Examples of how design and assembly can affect localized corrosion by creat...
Available to PurchasePublished: 01 January 2003
liquid to run off, rather than impinge directly on the concrete support. (i) Continuous weld for horizontal stiffeners prevents traps and crevices from forming. (j) Square sections formed from two L-shape members need to be continuously welded to seal out the external environment.
More
Image
Examples of how design and assembly can affect localized corrosion by creat...
Available to Purchase
in Analysis and Prevention of Environmental- and Corrosion-Related Failures
> Failure Analysis and Prevention
Published: 15 January 2021
on the concrete support. (i) Continuous welding is necessary for horizontal stiffeners to prevent the formation of traps and crevices. (j) Square sections formed from two L-shaped members require continuous welding to seal out the external environment. Source: Ref 12
More
1