Published: 30 September 2014
Fig. 34 Continuous furnace with central recuperator More
Image
Published: 30 September 2014
Fig. 25 Continuous furnace, using additional impeller agitation More
Image
Published: 01 January 1994
Fig. 12 Coating and firing installation using a U-type continuous furnace. Personnel stations: A, loader and stoner; B, spray operator; C, brusher; D, loader; E, unloader and inspector More
Image
Published: 01 August 2013
Fig. 35 Schematic view of a multichamber continuous furnace. Courtesy of Nitrex Metal Inc., Canada More
Image
Published: 01 December 1998
Fig. 2 Continuous furnace More
Image
Published: 01 February 2024
Fig. 69 Continuous furnace application with chute quenching More
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003198
EISBN: 978-1-62708-199-3
... Abstract Batch furnaces and continuous furnaces are commonly used in heat treating. This article provides a detailed account of various heat treating equipment and its furnace types, including salt bath equipment (externally heated, immersed-electrode and submerged-electrode furnaces...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005529
EISBN: 978-1-62708-197-9
... and continuous furnaces. The heating methods, such as direct-fired heating, radiant-tube heating, and electrical heating, are also discussed. Furnace temperature control is essential to ensure quality heat treatment. The article explains the operating procedure of the automatic temperature controllers used...
Book Chapter

By Satyam S. Sahay
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005787
EISBN: 978-1-62708-165-8
... and time cycles for annealing of alloy steels and carbon steel forgings. Different combinations of annealed microstructure and hardness are significant in terms of machinability. Furnaces for annealing are of two basic types, batch furnaces and continuous furnaces. The article concludes with a description...
Book Chapter

By Jon Dossett
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005762
EISBN: 978-1-62708-165-8
... atmosphere in batch and continuous furnaces. It discusses the most important considerations in the selection of carbonitriding temperature. The article also describes the processing factors for minimizing retained austenite in the carbonitrided case. Hardness testing and carbonitriding of powder metallurgy...
Book Chapter

By Toshi Oyama, Howard Mizuhara
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001386
EISBN: 978-1-62708-173-3
... and reviews three types of furnaces: continuous, semi-continuous, and batch. It presents three examples of the industrial applications of the furnace brazing: vacuum devices, jet engines, and automotive industries. The health and safety guidelines to be followed during the furnace brazing are also discussed...
Book Chapter

By Alexey Sverdlin
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005957
EISBN: 978-1-62708-166-5
... Abstract Furnaces are one of the most versatile types of industrial appliances that span many different areas of use. This article discusses the classification of various furnaces used in heat treating based on the mode of operation (batch-type furnaces and continuous-type furnaces...
Image
Published: 30 September 2014
Fig. 25 Continuous mesh belt furnace. Courtesy of Thermal Lining Services More
Image
Published: 30 September 2014
Fig. 26 Continuous strand wire annealing-type furnace. Courtesy of Thermal Engineering & Controls More
Image
Published: 01 August 2013
Fig. 12 (a) Schematic diagram of a continuous annealing furnace. (b) Typical continuous annealing thermal profile More
Image
Published: 09 June 2014
Fig. 29 Scheme of inductor-crucible furnace for continuous production More
Image
Published: 01 June 2016
Fig. 10 Continuous conveyor furnace for heat treating copper alloys in a controlled atmosphere More
Image
Published: 01 August 2013
Fig. 14 Typical multichamber continuous pusher-type furnace More
Image
Published: 01 January 1993
Fig. 6 Continuous-type brazing furnace with water-jacketed cooling chamber for use in air or controlled atmospheres More
Image
Published: 31 August 2017
Fig. 19 Schematic of horizontal continuous casting machine. 1, furnace; 2, water-cooled open-ended die; 3, supporting rollers; 4, traction system; 5, cutting saw; 6, breaking unit More