Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006085
EISBN: 978-1-62708-175-7
... loading Fig. 17 Conform continuous extruder Fig. 5 Extrusion pressure as function of ram travel Fig. 10 Effect on distribution of flow caused by use of dies of different conicity. Small-scale experiments with cylindrical tin samples. Source: Ref 6 Fig. 9 Typical...