1-20 of 1249

Search Results for contamination removal

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003694
EISBN: 978-1-62708-182-5
... contaminants, removal of invisible contaminants, and roughening of the surface. Solvent or chemical washing, steam cleaning, hand tool cleaning, power tool cleaning, water blasting, and abrasive blast cleaning, are some preparation methods discussed. The article describes the most common application techniques...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003220
EISBN: 978-1-62708-199-3
... including metallic contaminant removal, tarnish removal, oxide and scale removal, finishing, and coating processes. abrasive blast cleaning coating process electropolishing heat-resistant alloys passivation salt bath descaling stainless steel surface treatment tarnish removal Surface...
Book Chapter

By Om S. Kolluri
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001319
EISBN: 978-1-62708-170-2
... on contamination removal, plasma surface modification, plasma-induced grafting, and plasma film deposition. contamination removal plasma discharge reactions plasma film deposition plasma processing equipment plasma surface modification plasma-induced grafting plastic plasma treatment plastics surface...
Image
Published: 01 December 2004
Fig. 1 Extractor-condenser used for washing P/M specimens to remove contaminants from pores More
Image
Published: 01 December 1998
Fig. 6 Extractor-condenser used to wash P/M specimens to remove contaminants from pores More
Book Chapter

By F.S. Pettit
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001307
EISBN: 978-1-62708-170-2
... Abstract This article describes the methods for removing metallic contaminants, tarnish, and scale resulting from hot-working or heat-treating operations on nickel-, cobalt-, and iron-base heat-resistant alloys. It provides a brief description of applicable finishing and coating processes...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001269
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the various techniques for removing contaminants in the surface preparation of steel for hot-dip coatings: wet cleaning methods, including alkaline cleaning, electrolytic cleaning, chemical pickling, and electrolytic pickling; flame cleaning and furnace...
Book Chapter

By Jeff Hancock
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001226
EISBN: 978-1-62708-170-2
... Abstract Ultrasonic cleaning involves the use of high-frequency sound waves that is above the upper range of human heating, or about 18 kHz, to remove a variety of contaminants from parts immersed in aqueous media. This article describes the process, design considerations and the equipment...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... and installation of the protective coating/lining system. Prior to beginning surface-preparation operations, many specifications will require a presurface-preparation inspection to verify the correction of fabrication defects and removal of surface contamination such as grease, oil, cutting compounds, lubricants...
Book Chapter

By Ted Kostilnik
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001228
EISBN: 978-1-62708-170-2
... Abstract Mechanical cleaning systems are used to remove contaminants of work surface by propelling abrasive materials through any of these three principal methods: airless centrifugal blast blade- or vane-type wheels; compressed air, direct-pressure dry blast nozzle systems; or compressed-air...
Book Chapter

By Ken Trimber, Bill Corbett
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... Abstract This article reviews the steps involved in presurface-preparation inspection: substrate replacement; removal of weld spatter, rounding of sharp edges, and grinding of slivers/laminations; and removal of rust scale, grease, oil, and chemical (soluble salt) contamination. It focuses...
Book Chapter

By Mark T. Carroll
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001326
EISBN: 978-1-62708-170-2
... Abstract Wipe solvents are used to remove contaminants from a workpiece before it undergoes manufacturing operations that require clean surfaces, such as bonding, sealing, painting, welding, plating, specialized surface treatment procedures, and others. This article describes the evaluation...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003213
EISBN: 978-1-62708-199-3
... Abstract Metal surfaces must often be cleaned before subsequent operations to remove unwanted substances such as pigmented drawing compounds, unpigmented oil and grease, chips and cutting fluids, polishing and buffing compounds, rust and scale, and miscellaneous contaminants. The article...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005777
EISBN: 978-1-62708-165-8
... is difficult; it consumes time and money and may not be feasible. The barrier contaminant layers may have to be removed mechanically, for example, by grinding or blasting, which may create other problems, such as a change in dimensions of the workpiece and the roughness of the surface. Afterwards, the parts...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001324
EISBN: 978-1-62708-170-2
... by removing the soils or contaminants (oils) from the cleaning solution. Oils that float to the surface of a wash tank can often be removed by manual or automatic skimming. Parts being pulled up through a floating oil or foam patch run the risk of having the soil redeposited. Agitation systems can be designed...
Book Chapter

By Kenneth B. Tator
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006070
EISBN: 978-1-62708-172-6
... of the hurricane (coastal or inland). Salt concentrations in such localized areas may change seasonally or even daily, because precipitation may wash and remove contaminating salts from the surface or leach salts from soils. On the other hand, acid rain precipitation may again deposit new salts onto a surface...
Book Chapter

By David Eisenmann
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006440
EISBN: 978-1-62708-190-0
... the lipophilic emulsifier; therefore, it is easier to control the cleaning action. In addition to the emulsifier application, method D also requires a prerinse. Using a coarse water spray, the prerinse helps remove the excess penetrant to minimize contamination of the emulsifier. Of greater significance, only...
Book Chapter

By Rick Huntley
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006043
EISBN: 978-1-62708-172-6
... at the edge of the coating. This method of coating removal can be performed on steel, concrete, wood, and most other substrates. However, in examining the surface after the coating removal, it should be remembered that in some cases surface contaminants are removed by the coating and adhere to the back...
Book Chapter

By Reginald K. Asher, Sr.
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001256
EISBN: 978-1-62708-170-2
... density too high Lower rectifier settings. Temperature of plating solution too high Check and adjust to 19-21 °C (66-70 °F). Lack of solution circulation Check to be sure all circulating pumps are operating. Excessive copper in plating solution Analyze and remove contamination by dummy...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001223
EISBN: 978-1-62708-170-2
... Regulation of Surface Engineering” and “Vapor Degreasing Alternatives” in this volume. Cold Cleaning Cold cleaning is a process for removing oil, grease, loose metal chips, and other contaminants from the surfaces of metal parts. Common organic solvents such as petroleum distillate fractions...