Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
..., bronze, beryllium-copper, nickel-plate, steel, rubber, plastic, metal-filled plastic, plaster, and combinations of these. All of these are suitable for wax patterns, but plastic patterns usually require steel or beryllium-copper tooling. Soft metals and nonmetallics are often used for temporary tooling...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006026
EISBN: 978-1-62708-172-6
... testing procedures: falling abrasive and Taber abrasion. The latter is less costly and generally more repeatable/reproducible. The falling sand test is conducted according to ASTM D968, “Standard Test Methods for Abrasion Resistance of Organic Coatings by Falling Abrasive” ( Fig. 3 ). Test plates...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001277
EISBN: 978-1-62708-170-2
... Abstract Painting is a generic term for the application of a thin organic coating to the surface of a material for decorative, protective, or functional purposes. This article provides a detailed account of the types and selection factors of paints and the various application methods, including...