Skip Nav Destination
Close Modal
Search Results for
cold chamber die casting
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 283 Search Results for
cold chamber die casting
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005268
EISBN: 978-1-62708-187-0
... Abstract The cold chamber die casting process is used with higher-melting-point alloys such as aluminum and magnesium. This article discusses the component design of the cold chamber high-pressure die casting machine. It reviews the process parameters of cold chamber die casting, incuding...
Abstract
The cold chamber die casting process is used with higher-melting-point alloys such as aluminum and magnesium. This article discusses the component design of the cold chamber high-pressure die casting machine. It reviews the process parameters of cold chamber die casting, incuding the shot profile, intensification phase, and component size.
Image
Published: 01 December 2008
Image
Published: 01 December 1998
Image
Published: 30 November 2018
Image
Published: 30 November 2018
Image
Published: 30 November 2018
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006525
EISBN: 978-1-62708-207-5
... porosity in as-cast parts. It begins by describing a typical cycle for a traditional cold-chamber die casting machine, using detailed illustrations to show how gas can become trapped in the liquid metal. It then presents various remedies, ultimately focusing on vacuum die casting for the production of high...
Abstract
Nearly two-thirds of the aluminum castings made in North America are produced using high-pressure die casting techniques. This article compares and contrasts traditional high-pressure die casting with an improved version that uses a vacuum to pull air out of the die in order to reduce porosity in as-cast parts. It begins by describing a typical cycle for a traditional cold-chamber die casting machine, using detailed illustrations to show how gas can become trapped in the liquid metal. It then presents various remedies, ultimately focusing on vacuum die casting for the production of high-integrity parts. In addition to vacuum technology, the article discusses casting alloys, dies, and cells, and describes some of the benefits of structural die castings.
Image
Published: 01 December 2008
Fig. 5 Schematics showing the principal components of (a) hot chamber and (b) cold chamber die casting machines
More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005267
EISBN: 978-1-62708-187-0
... Abstract This article describes the melting process of casting metals used in hot chamber die casting. It discusses the design and capabilities of injection components, such as gooseneck, plunger, and cylinder. The article reviews the distinctions between hot and cold chamber processes...
Abstract
This article describes the melting process of casting metals used in hot chamber die casting. It discusses the design and capabilities of injection components, such as gooseneck, plunger, and cylinder. The article reviews the distinctions between hot and cold chamber processes. An example of a typical runner, gate and overflow configuration for faucet fixture casting is shown. Temperature control for die casting is also discussed. The article explains some ejection and post-processing techniques used for the hot chamber die casting: robotics, recycling, and fluxing.
Image
Published: 01 December 2008
Fig. 12 The fan housing was cast in a three-plate die with a cold chamber gating system. Shown here is the cover half (left) and ejector half (right) of the die.
More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005266
EISBN: 978-1-62708-187-0
... alloys can also be die cast. Parts produced by the die casting process are shown in Fig. 1 . The primary categories of the conventional die casting process are the hot chamber process and the cold chamber process. These main process variations have been enhanced in recent years to produce high-integrity...
Abstract
This article provides a comprehensive discussion on die casting alloy types and casting processes used in high-pressure die casting. It presents the advantages and disadvantages of high-pressure die casting and describes the product design for the process. The article concludes with information on the metal injection process of high-pressure die casting.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005318
EISBN: 978-1-62708-187-0
...) (a) For short-run zinc castings only. (b) Nitrided. Source: Ref 1 Die Casting Machines Die casting machines are classified by the metal-pumping systems as either hot chamber or cold chamber. If the metal being cast melts at a low temperature or does not attack the injection pump material...
Abstract
The designer of die casting tooling must balance the functional requirements of the part being cast with the cost, speed, and quality requirements of the process. In addition, attention must also be paid to the capacity and operating parameters of the casting machines being used and the need and economics of postprocessing. This article examines how design and materials selection address these diverse requirements of conventional die casting tooling. It focuses on the tooling for high-volume processes where the liquid or semisolid metal is forced into the die with high pressure and speed. The article also describes the functions of the tooling which involves supplying of molten alloy to the casting machine and injecting it into the die.
Image
Published: 01 December 2008
Fig. 4 Schematics showing gating systems for (a) cold chamber and (b) hot chamber die casting machines
More
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006579
EISBN: 978-1-62708-210-5
.... It is, however, subject to abrupt solidification when approaching the setting point and is less suitable for cold-chamber die casting machines than Aluminum 360.0 with lower silicon content. Corrosion The corrosion resistance of alloys 413.0 and A413.0 is very good. Chemical conversion coatings improve...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005292
EISBN: 978-1-62708-187-0
... Two basic types of die casting machines are used for production: the hot chamber and the cold chamber. The hot chamber machine consists of an injection mechanism that is immersed in molten metal in a furnace attached to the machine. These machines are quick in operation and are normally used for lower...
Abstract
High-pressure die casting is a fast method for the net shape manufacturing of parts from nonferrous alloys. This article reviews the automation technologies for the different stages or steps of the process. These steps include liquid metal pouring, injection, solidification, die open, part extraction, die lubrication, insert loading, and die close. Some manual aspects of the operations, together with automation options, are discussed. The article describes finishing steps, such as finish trimming, detailed deflashing, shot blast cleaning, and quality checks. Automation of the postcasting process is also discussed.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005187
EISBN: 978-1-62708-187-0
... … Counterpressure casting/pressure-counterpressure casting Aluminum 3 Yes Medium … Countergravity casting All 3 … Small … High-pressure die casting (HPDC) Conventional HPDC Hot chamber Zn and Mg 5 No Small Outstanding Cold chamber Nonferrous 5 No Small to medium...
Abstract
This article discusses the categories and subcategories of shape casting processes. These include single-use processes such as sand, plaster, ceramic, and graphite molding; essentially unpressurized multiuse processes, such as permanent mold; and high-pressure metal mold methods, such as die casting, squeeze casting, and semisolid processing. The article contains tables that compare some of the typical capabilities of shape casting processes.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005334
EISBN: 978-1-62708-187-0
... alloys, may employ a larger bulk melting unit from which the molten alloy for the casting operation is distributed to holding crucible furnaces. Metal treatments are carried out, and the metal is either poured directly from the crucible or hand ladled to the casting molds. In cold-chamber die-casting...
Abstract
This article focuses on the variety of alloys, furnaces, and associated melting equipment as well as the casting methods available for manufacturing magnesium castings. These methods include sand casting, permanent mold casting, die casting, thixomolding, and direct chill casting. The article discusses the flux process and fluxless process for the melting and pouring of magnesium alloys. It describes the advantages and disadvantages of green sand molding and tabulates typical compositions and properties of magnesium molding sands. The article provides information on the machining characteristics of magnesium and the applications of magnesium alloys.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... that use ceramic molds include investment casting, and plaster casting. Metallic molds are used in permanent mold casting, die casting, semisolid casting, and centrifugal casting. centrifugal casting ceramic molds CO2 process cold box process die casting hot box process investment casting lost...
Abstract
This article discusses classification of foundry processes based on the molding medium, such as sand molds, ceramic molds, and metallic molds. Sand molds can be briefly classified into two types: bonded sand molds, and unbonded sand molds. Bonded sand molds include green sand molds, dry sand molds, resin-bonded sand molds, and sodium silicate bonded sand. The article describes the casting processes that use these molds, including the no-bake process, cold box process, hot box process, the CO2 process, lost foam casting process and vacuum molding process. The casting processes that use ceramic molds include investment casting, and plaster casting. Metallic molds are used in permanent mold casting, die casting, semisolid casting, and centrifugal casting.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
... in die casting is the formation of complex intermetallics that are insoluble at melt-holding temperatures and/or precipitate under holding conditions or during transfer to and injection from the hot or cold chamber. These intermetallics (sludge) affect furnaces, transfer systems, and, by inclusion...
Abstract
Aluminum casting alloys are the most versatile of all common foundry alloys and generally have the highest castability ratings. This article provides an overview of the common methods of aluminum shape casting. These include gravity casting, die casting, sand casting, lost foam casting, shell mold casting, plaster casting, investment casting, permanent mold casting, squeeze casting, semisolid forming, centrifugal casting, and pressure die casting. The article presents several different factors on which the selection of a casting process depends. It discusses gating and risering principles in casting. The article concludes with information on premium engineered castings that provide higher levels of quality and reliability than in conventionally produced castings.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005333
EISBN: 978-1-62708-187-0
..., are always cast in hot-chamber zinc die casting machines. ZA-8 can be hot-chamber die cast and is also permanent mold cast. As a pressure die casting, it has excellent properties, especially creep, compared with other zinc alloys. ZA-12 and ZA-27 are cold-chamber die cast and can be sand cast, too. ZA-12...
Abstract
Die casting is the process most often used for shaping zinc alloys. This article tabulates the compositions of zinc casting alloys and comparison of typical mechanical properties of zinc casting alloys. It discusses additions of alloys to the zinc, including aluminum, magnesium, copper, and iron. The article illustrates a characteristic five-layer microstructure of zinc alloy casings. It discusses the various methods of finishing of zinc alloy die castings, including chromium plating, polishing, painting, and electropainting. The article describes the casting of inserts and their uses in the zinc. It concludes with information on the applications of zinc die castings.