Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003377
EISBN: 978-1-62708-195-5
... expansion coefficients, moisture swelling coefficients, static and dynamic viscoelastic properties, conductivity, and moisture diffusivity. unidirectional fiber composites aligned continuous fibers analytical method physical properties elasticity thermal expansion coefficients moisture swelling...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003442
EISBN: 978-1-62708-195-5
... of thermal expansion and coefficient of moisture expansion; glass transition temperature; thermal conductivity, diffusivity, and specific heat. lamina nonmechanical testing laminate nonmechanical testing nonmechanical properties composite materials ply thickness density coefficient of thermal...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003378
EISBN: 978-1-62708-195-5
... the development of the relations between mid-surface strains and curvatures and membrane stress and moment resultants. The article discusses the properties, such as thermal expansion, moisture expansion, and conductivity, of symmetric laminates and unsymmetric laminates. It describes the distribution...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003367
EISBN: 978-1-62708-195-5
... free volume. These result in lower moisture absorption, higher diffusivity, low cure shrinkage, low coefficient of thermal expansion (CTE), and low dielectric constant and dielectric loss when compared with epoxy and bismaleimide (BMI) systems. These attributes are particularly attractive for stable...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003023
EISBN: 978-1-62708-200-6
... deflection temperature at 1.82 MPa (0.264 ksi) UL index Thermal conductivity Coefficient of thermal expansion, 10 −6 /°C °C °F °C °F W/m · K Btu/ft · h · °F Acrylonitrile-butadiene-styrene (ABS) 99 210 60 140 0.27 0.16 53 ABS-polycarbonate alloy (ABS-PC) 115 240 60 140 0.25...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003390
EISBN: 978-1-62708-195-5
... changes and moisture absorption can have a significant impact on composite behavior, so laminate programs should be able to handle environmental loads. Engineering constants should include laminate expansion coefficients, and stress/strain calculations should include temperature and moisture components...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001318
EISBN: 978-1-62708-170-2
... the 1980s, a significant level of research activity focused on the protection of high-performance carbon-carbon that used heat-stabilized polyacrylonitrile (PAN) or pitch-based fibers. These composites have higher strength, higher elastic moduli, and lower thermal expansion coefficients than the rayon-based...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003465
EISBN: 978-1-62708-195-5
... are the measurement of both T g and the changes in its coefficient of linear thermal expansion (CTE) with cure. In TMA, the T g is measured as the intersection of the expansion curves in the glassy and rubbery states of the polymer matrix, possible for most polymers because there is a threefold difference...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003428
EISBN: 978-1-62708-195-5
... potential difference of the above materials. A comparison of thermal expansion coefficients is given in Table 2 . The combination of CFRC and aluminum would result in the greatest thermal expansion mismatch, which would increase loads on the fasteners, adhesives, or sealants as the joint is subjected...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006037
EISBN: 978-1-62708-172-6
... are covered subsequently. Thermal Properties Thermal properties, including cure shrinkage, thermal cycling, thermal shock, and temperature limitations, are important properties to quantify and understand for polymer flooring systems. Cure shrinkage and the linear coefficient of thermal expansion (LCTE...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003381
EISBN: 978-1-62708-195-5
... environment has not been ensured. Absorbing moisture induces some degree of volumetric expansion, which can induce warping and other structure-performance effects similar to thermal expansion issues, in addition to the fundamental effects on the base properties of the material. While this is not commonly...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006923
EISBN: 978-1-62708-395-9
... Coefficient of thermal expansion, 10 −6 /°C °C °F °C °F W/m · K Btu/ft · h · °F Acrylonitrile-butadiene-styrene (ABS) 99 210 60 140 0.27 0.16 53 ABS-polycarbonate alloy (ABS-PC) 115 240 60 140 0.25 0.14 35 Diallyl phthalate (DAP) 285 545 130 265 0.36 0.21 27...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003156
EISBN: 978-1-62708-199-3
... Alloys The primary requirements for resistance alloys are uniform resistivity, stable resistance (no time-dependent aging effects), reproducible temperature coefficient of resistance, and low thermoelectric potential versus copper. Properties of secondary importance are coefficient of expansion...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003385
EISBN: 978-1-62708-195-5
... edges by the expansion of the material due to thermal expansion and/or swelling of the matrix from moisture absorption. An interesting aspect of thermal buckling for graphite-fiber composites is that graphite fibers have a negative coefficient of thermal expansion, thus it is possible for plates...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003432
EISBN: 978-1-62708-195-5
... ASTM D 1895 Thermal properties, including glass transition temperature, coefficient of thermal expansion, and weight loss at temperature User defined Chemical exposure to acetone, chlorinated solvents, oils, hydraulic fluids, jet fuel, body fluids, alcohol User defined Moisture effects User...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
... strength Shear modulus Thermal Coefficient of thermal expansion Thermal conductivity Specific heat Elecrical Dielectric constant Dielectric strength Dissipation factor Volume resistivity In-service conditions Service temperature Thermogravimetric analysis...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003032
EISBN: 978-1-62708-200-6
... Compressive modulus Shear strength Shear modulus Thermal Coefficient of thermal expansion Thermal conductivity Specific heat Electrical Dielectric constant Dielectric strength Dissipation factor Volume resistivity In-service conditions Service temperature...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002478
EISBN: 978-1-62708-194-8
..., the solution for curvature stability is obtainable over a wide range of coupling coefficients and is independent of the thermal expansion and moisture swelling coefficients of the individual laminates. Temperature changes warp most metal-, ceramic-, or polymer-matrix, asymmetric composites, while moisture...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003452
EISBN: 978-1-62708-195-5
... induced residual stresses do not normally compromise the design of a composite bonded repair; however, it is important that they be considered during the design phase. Coefficients of thermal expansion of substrates and repair materials Table 2 Coefficients of thermal expansion of substrates...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003066
EISBN: 978-1-62708-200-6
... in predictable ways. For example, for selenides of the type Ge-As-Se, the glass transformation temperature, hardness, Young's modulus, and strength increase, while the thermal expansion coefficient and molar volume decrease with a tighter structure. The properties of these glasses also depend on the type...