Skip Nav Destination
Close Modal
By
R.G. Buchheit, A.E. Hughes
By
Barry Meyers, Stephen Lynn, Elwin Jang
By
Patrick L. Hagans, Christina M. Haas
By
T.J. Clark, R.C. DeVries
By
James L. Smialek, Charles A. Barrett, Jon C. Schaeffer
By
Tapio Mäntylä, Mikko Uusitalo
By
W. Theisen, A. Röttger
By
Bo Hu
Search Results for
cobalt-base conversion coating
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 298
Search Results for cobalt-base conversion coating
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
... ) seal coat. Cobalt-Base Conversion Coatings A cobalt nitrate [Co(NO 3 ) 2 ] bath produces layers of cobalt oxides over an aluminum substrate. Cobalt-base conversion coatings are being developed for the marine, automotive, and aerospace industries. Molybdenum-Base Conversion Coatings...
Abstract
This article provides a brief discussion on the common types of overlayers that can be used on a metal surface to protect it from corrosion. These overlayers include phosphate, chromate, and chromate-free conversion coatings; hot dip galvanizing; cementitious linings; glass and porcelain enamels; electroplating; thermal spray coatings; and rubber linings.
Book Chapter
Chromate and Chromate-Free Conversion Coatings
Available to PurchaseSeries: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003679
EISBN: 978-1-62708-182-5
... with chromate-free conversion. These include: titanium and zirconium fluorocomplexes; cerium-base, manganese-base, cobalt-base, and molybdate-base conversion coatings; hydrotalcite coatings; and organic coatings. chromate conversion coatings corrosion resistance electrochemical impedance spectroscopy...
Abstract
Chromate conversion coatings (CCCs) are primarily used to improve adhesion of subsequently applied organic coatings or to impart corrosion resistance during atmospheric exposure. This article describes the factors that affect the formation of CCCs. It provides information on the processing sequence, morphology, composition, and properties of CCCs. The article discusses the electrochemical impedance spectroscopy approach used for evaluating conversion coatings. The test methods for various CCCs properties are also reviewed. The article examines the various coatings associated with chromate-free conversion. These include: titanium and zirconium fluorocomplexes; cerium-base, manganese-base, cobalt-base, and molybdate-base conversion coatings; hydrotalcite coatings; and organic coatings.
Book Chapter
Chromium Elimination in Surface Engineering
Available to PurchaseBook: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001323
EISBN: 978-1-62708-170-2
... Abstract This article focuses on alternatives to chromium in both hard chromium plating and chromate conversion coating. These include electroless nickel plating, nickel-tungsten composite electroplating, spray coating applications, and cobalt/molybdenum-base conversion coating. The article...
Abstract
This article focuses on alternatives to chromium in both hard chromium plating and chromate conversion coating. These include electroless nickel plating, nickel-tungsten composite electroplating, spray coating applications, and cobalt/molybdenum-base conversion coating. The article discusses the material and process substitutions that can be used to eliminate the use or emissions of chromium in industrial processes. It describes the physical characteristics of each coating, economics, environmental impacts, advantages, and disadvantages of alternative processes.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006521
EISBN: 978-1-62708-207-5
... a discussion on organic-based coatings. chemical conversion coatings chromate conversion coatings chromate-free conversion coatings phosphate conversion coating aluminum alloys CHEMICAL CONVERSION COATINGS are adherent surface layers of low-solubility oxide, phosphate, chromate, and chromate...
Abstract
Chemical conversion coatings are adherent surface layers of low-solubility oxide, phosphate, chromate, and chromate-free compounds produced by the reaction of suitable reagents with the metallic surface. This article provides an overview on chromate-free coatings, along with coverage on the processes of low-solubility oxide, phosphate, and chromate conversion coating. Some applications using chemical conversion coatings on various aluminum alloys are given in a table. The article also provides information on the advantages and disadvantages of chromate conversion coatings. It concludes a discussion on organic-based coatings.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003120
EISBN: 978-1-62708-199-3
... Abstract Superalloys are nickel, iron-nickel, and cobalt-base alloys generally used for high-temperature applications. Superalloys are used in aircraft, industrial, marine gas turbines, nuclear reactors, spacecraft structures, petrochemical production, orthopedic and dental prostheses...
Abstract
Superalloys are nickel, iron-nickel, and cobalt-base alloys generally used for high-temperature applications. Superalloys are used in aircraft, industrial, marine gas turbines, nuclear reactors, spacecraft structures, petrochemical production, orthopedic and dental prostheses, and environmental protection applications. This article discusses the material characteristics, phases, structures, and systems of superalloys. It describes the processing of superalloys, including primary and secondary melting, deformation processing (conversion), powder processing, investment casting, and joining methods. The article also describes the properties, microstructure, and thermal exposure of superalloys. It further discusses the effects of environmental factors on superalloys, including oxidation and hot corrosion. Protective coatings are also discussed. The article provides information on the mechanical properties and chemical composition of nickel, iron, and cobalt-base superalloys in both the cast and wrought forms.
Book Chapter
Chromate Conversion Coatings
Available to PurchaseBook: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001275
EISBN: 978-1-62708-170-2
... by chromate coatings. The article also discusses the development of replacement technologies in response to environmental constraints that have developed around the use of chromium-base compounds. chromate conversion coatings coating deposits coating performance environmental constraints substrate...
Abstract
This article briefly describes the basic attributes of chromate conversion coatings and the processes for applying them. It provides information on the influence of substrate microstructure on the performance of coating deposits and on the mechanism of substrate protection supplied by chromate coatings. The article also discusses the development of replacement technologies in response to environmental constraints that have developed around the use of chromium-base compounds.
Book Chapter
Compatibility Guide
Available to PurchaseBook: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006541
EISBN: 978-1-62708-183-2
...+paint or resin seal C Cadmium, beryllium Chromate conversion coating+paint or resin seal D Aluminum, Al-Mg, Al-Zn Anodic coating+paint or resin seal E Aluminum-copper Anodic coating+paint or resin seal F Steel, carbon and low alloy Metallic coating, sacrificial (Zn) or nonsacrificial...
Abstract
This guide rates the compatibility of dissimilar structural materials joined together for service in seawater, marine atmosphere, or industrial atmosphere. It contains a table that indicates the material code and most generally effective surface treatment typically used to reduce corrosion of bare metals.
Book Chapter
Superabrasives and Ultrahard Tool Materials
Available to PurchaseSeries: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001106
EISBN: 978-1-62708-162-7
... oxide layer no longer prevents further degradation. Back conversion is not significant until temperatures reach about 1700 °C (3100 °F). Because the reactivity of CBN with iron-, cobalt-, and nickel-base alloys is much less than that of diamond, CBN fills an important gap in the use of ultrahard...
Abstract
Synthetic diamond and cubic boron nitride are among a class of superhard materials from the boron-carbon-nitrogen-silicon family of elements. This article focuses on the two materials, the forms in which they are produced, and their respective properties. Synthetic diamond and cubic boron nitride compounds are available in the form of grit and sintered polycrystalline blanks of various size, shape, and composition. The article explains how superabrasive grains made from these materials can be used in lapping, polishing, and grinding applications, and how diamond and boron nitride blanks can be mounted to suitable substrates to form ultrahard cutting edges and tools.
Book Chapter
Cutting Tool Materials
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003188
EISBN: 978-1-62708-199-3
... material. This is followed by a schematic representation of their relative application ranges in terms of machining speeds and feed rates. The article provides a detailed account of chemical compositions of various tool materials, including high-speed tool steels, cobalt-base alloys, cemented carbides...
Abstract
Selecting the proper cutting tool material for a specific machining application can provide substantial advantages, including increased productivity, improved quality, and reduced costs. This article begins with a description of the factors affecting the selection of a cutting tool material. This is followed by a schematic representation of their relative application ranges in terms of machining speeds and feed rates. The article provides a detailed account of chemical compositions of various tool materials, including high-speed tool steels, cobalt-base alloys, cemented carbides, cermets, ceramics, cubic boron nitride, and polycrystalline diamond. It compares the toughness, and wear resistance for these cutting tool materials. Finally, the article explains the steps for selecting tool material grades for specific application.
Book Chapter
Design for Oxidation Resistance
Available to PurchaseSeries: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002473
EISBN: 978-1-62708-194-8
... in Lai ( Ref 11 ). Supplementary information on superalloy oxidation, corrosion, and coatings is present in Ref 1 , 12 , 13 , 14 , 15 , and 16 and in the review of high-temperature oxidation of iron-, nickel-, and cobalt-base alloys in Ref 17 . Performance Characteristics of Superalloys...
Abstract
Alloys intended for use in high-temperature environments rely on the formation of a continuous, compact, slow-growing oxide layer for oxidation, and hot corrosion resistance. This article focuses on the issues related to high-temperature oxidation of superalloys used in gas turbine engine applications. It discusses the general methodologies used to evaluate oxidation resistance of materials. The article describes the performance characteristics of superalloys, single-crystal superalloys, and other high-temperature materials such as refractory metals and ceramics. It discusses hot corrosion of superalloys and airfoil degradation due to deposits resulting from ingested particles or sand. The article concludes with a discussion on the limitations of testing techniques and life prediction.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006418
EISBN: 978-1-62708-192-4
... serve as grain-growth inhibitors, particularly in very fine (<1 μm) particle sizes. Cobalt (Co) Cobalt (Co) is the most widely used binder in WC-base hardmetals. Cobalt is the preferred binder due to its outstanding wetting and adhesion characteristics. As shown in Table 1 , cobalt has a low...
Abstract
Cemented carbides, best known for their superior wear resistance, have a range of industrial uses more diverse than that of any other powder metallurgy product including metalworking and mining tools and wear-resistant components. This article discusses raw materials and manufacturing methods used in the production of cemented carbides, the physical and mechanical properties of carbides, and wear mechanisms encountered in service. Emphasis is placed on tungsten carbide-cobalt (WC-Co) or tungsten carbide-nickel (WC-Ni) materials as used in nonmachining applications. Nominal composition and properties of representative cemented carbide grades and their applications are listed in a table.
Book Chapter
Diffusion Coatings
Available to PurchaseBook: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001293
EISBN: 978-1-62708-170-2
...- and cobalt-base superalloys, steels (including carbon, alloy, and stainless steels), and refractory metals and alloys. This article is divided into two major Sections. The first Section describes the widespread use of diffusion coatings for elevated-temperature protection of turbine components...
Abstract
This article describes the widespread use of diffusion coatings for elevated-temperature protection of the turbine components for aircraft engines and gas turbines. The principles of pack diffusion coating, namely, aluminizing, chromizing, and siliconizing, are discussed. The article presents information on the coating formation mechanism of superalloys and explains the steps involved in a typical pack cementation process. It concludes with information on the processing procedures and properties of pack aluminized steels.
Book Chapter
Hardfacing Alloys
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003162
EISBN: 978-1-62708-199-3
... hardfacing alloys can be divided into pearlitic steels, austenitic (manganese) steels, martensitic steels, high-alloy irons, and austenitic stainless steel. The types of nonferrous hardfacing alloys include cobalt-base/carbide-type alloys, laves phase alloys, nickel-base/boride-type alloys, and bronze type...
Abstract
Hardfacing is defined as the application of a wear-resistant material, in depth, to the vulnerable surfaces of a component by a weld overlay or thermal spray process Hardfacing materials include a wide variety of alloys, carbides, and combinations of these materials. Iron-base hardfacing alloys can be divided into pearlitic steels, austenitic (manganese) steels, martensitic steels, high-alloy irons, and austenitic stainless steel. The types of nonferrous hardfacing alloys include cobalt-base/carbide-type alloys, laves phase alloys, nickel-base/boride-type alloys, and bronze type alloys. Hardfacing applications for wear control vary widely, ranging from very severe abrasive wear service, such as rock crushing and pulverizing to applications to minimize metal-to-metal wear. This article discusses the types of hardfacing alloys, namely iron-base alloys, nonferrous alloys, and tungsten carbides, and their applications and advantages.
Book Chapter
Surface Engineering of Stainless Steels and Heat-Resistant Alloys
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003220
EISBN: 978-1-62708-199-3
... that has been successful in Diffusion coatings via pack cementation of Electropolishing is applicable to all stainless removing brass, lead, zinc, bismuth, and tin from steel grades, hot or cold finished, cast or nickel-base and cobalt-base alloys involves vapor aluminum, chromium, silicon, or combinations...
Abstract
Although stainless steel is naturally passivated by exposure to air and other oxidizers, additional surface treatments are needed to prevent corrosion. Passivation, pickling, electropolishing, and mechanical cleaning are important surface treatments for the successful performance of stainless steel. This article describes the surface treatment of stainless steels including abrasive blast cleaning, acid pickling, salt bath descaling, passivation treatments, electropolishing, and the necessary coating processes involved. It also describes the surface treatment of heat-resistant alloys including metallic contaminant removal, tarnish removal, oxide and scale removal, finishing, and coating processes.
Book Chapter
Hand Lay-Up, Spray-Up, and Mechanical Lay-Up
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003036
EISBN: 978-1-62708-200-6
..., % Gel time starting at room temperature, min Approximate time at 21–24 °C (70–75 °F) for development of Barcol Hardness = 35 Gel coats MEKP 1.5 (a) , cobalt naphthenate 0.4 (b) (accessory promoters usually omitted because of tendency to discolor) 30 (high filler content) 6–8 (can proceed...
Abstract
Wet lay-up using hand or spray techniques is one of the simplest methods of combining a fiber reinforcement with a solidifying resin to form a composite structure. This article describes several wet lay-up processes - including contact molding, spray molding, vacuum bag molding, and autoclave molding - suited for making parts on open-faced molds using polyester and vinyl ester resins. The article also provides information on mechanically assisted lay-up which can be automated to alleviate some of the manual work.
Book Chapter
Corrosion of Thermal Spray Coatings at High Temperatures
Available to PurchaseBook: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0004050
EISBN: 978-1-62708-183-2
... of MCrAl X -base alloy coatings has been developed for oxidation protection of gas turbines. The early MCrAlY coatings were alloys based on cobalt containing 20 to 40% Cr, 12 to 20% Al, and ∼0.5% Y, a typical example being Co-25Cr-14Al-0.5Y. The most recent coatings are more complex, in which M is nickel...
Abstract
This article describes the specific features and mechanisms of oxidation in thermal spray coatings. It discusses the two forms of hot corrosion in sulfur-containing combustion, namely high-temperature hot corrosion and low-temperature hot corrosion. The article reviews the behavior of corrosion-resistant coatings in boilers. The effects of high-temperature corrosion in waste incinerators are detailed. The article also examines the effects of erosion-corrosion in fluidized bed combustion boilers.
Book Chapter
Carbide- and Boride-Based Thick Coatings for Abrasive Wear-Protection Applications
Available to PurchaseSeries: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006364
EISBN: 978-1-62708-192-4
...-resistant coatings, namely, compound casting, deposition welding, and thermal spraying. abrasive wear-resistant coating borides carbides metal-matrix composites cemented carbides hardness wear-resistant material cobalt alloys iron alloys nickel-base alloys wear tribomechanical properties...
Abstract
This article provides a brief introduction to abrasive wear-resistant coating materials that contain a large amount of hard phases, such as borides, carbides, or carboborides. It describes some of the commonly used methods of producing thick wear-resistant coatings. The article also provides information on metal-matrix composites and cemented carbides. The three base-alloying concepts, including cobalt-, iron-, and nickel-base alloys used for wear-protection applications, are also described. The article compares the tribomechanical properties of the materials in a qualitative manner, thus allowing a rough materials selection for practitioners. It presents a brief discussion on hot isostatic pressing (HIP) cladding, sinter cladding, and manufacturing of thick wear-resistant coatings by extrusion or ring rolling. The article also discusses the processing sequence of thick wear-resistant coatings, namely, compound casting, deposition welding, and thermal spraying.
Book Chapter
Metal and Alloy Powders for Welding, Hardfacing, Brazing, and Soldering
Available to PurchaseBook: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006079
EISBN: 978-1-62708-175-7
... would cause longitudinal cracks immediately after extrusion. Transversal cracks might appear after baking. Conversely, an extrusion pressure that is too low produces a coating that is too soft. In such a case, the electrode can easily be deformed during handling and transportation. For those high...
Abstract
Metals and alloy powders are used in welding, hardfacing, brazing, and soldering applications, which include hardface coatings, the manufacturing of welding stick electrodes and flux-cored wires, and additives in brazing pastes or creams. This article reviews these applications and the specific powder properties and characteristics they require.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
... life when resistance to corrosion, wear, and erosion is required. The common methods include electroplating, electroless plating, hardfacing, weld cladding, surface hardening, porcelain enameling, and organic coatings. cast iron conversion coatings corrosion resistance ductile iron...
Abstract
This article provides a brief review of the classification and characteristics of cast irons. It describes the processes used to clean iron castings, including mechanical cleaning and finishing and nonmechanical cleaning. The article discusses surface treatments used to extend casting life when resistance to corrosion, wear, and erosion is required. The common methods include electroplating, electroless plating, hardfacing, weld cladding, surface hardening, porcelain enameling, and organic coatings.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006071
EISBN: 978-1-62708-172-6
... Abstract An alkyd is an ester-based polymer derived from the polycondensation reaction of polyhydric alcohol and polybasic acid. This article provides useful information on the chemistry, production, coating formulations, modification, commercial products, and application methods of alkyd...
Abstract
An alkyd is an ester-based polymer derived from the polycondensation reaction of polyhydric alcohol and polybasic acid. This article provides useful information on the chemistry, production, coating formulations, modification, commercial products, and application methods of alkyd resins. It also provides a section on drying oil, which is used in the manufacture of resins. The article describes the three categories of metals that have been used in drier compounds: primary driers (active or oxidation driers), secondary driers (through-driers), and auxiliary driers. It also provides information on the oil length of an alkyd resin and on solvents, which play a critical role in the formulation and use of the coating. The article concludes with a description of the concerns that a user, specifier, or applicator should be aware of when using alkyd coatings.
1