EISBN: 978-1-62708-172-6
... Abstract Independent verification of coating system performance can be based on laboratory testing and/or field exposure. Qualification testing is a critical component to coating system selection. This article focuses on performance evaluations that are used to prequalify coating systems...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006006
EISBN: 978-1-62708-172-6
... Abstract This article provides a detailed discussion on the functions, applications, types, and selection criteria of exterior and interior rail coatings. It includes a discussion on the corrosivity, inspection/maintenance, and qualification of applicators/inspectors/facilities. cleaning...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006010
EISBN: 978-1-62708-172-6
... industry and American National Standards Institute/American Society of Mechanical Engineers (ANSI/ASME) N45.2.6, “Qualification of Inspection, Examination and Testing Personnel for Construction Phase of Nuclear Power Plants,” and ANSI N101.4, “Quality Assurance for Protective Coatings Applied to Nuclear...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003690
EISBN: 978-1-62708-182-5
.... AWS C2.16-92, “Guide for Thermal Spray Operator Qualification.” This guide recommends thermal spray operator qualification procedures. It covers applicable documents relating to thermal spray equipment, consumables, and safety. It also contains operator qualification and coating system analysis forms...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006438
EISBN: 978-1-62708-190-0
... and Qualification The efficacy of NDE tests depends on the capabilities of practitioners. Many NDE contracts demand proof of personnel capabilities through certification programs. Qualification is the compliance with requirements of certification. These requirements typically include education and training...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... abrasives. However, these agricultural abrasives are not considered aggressive enough to remove industrial protective coatings and are not hard enough to generate a surface profile in steel. The SSPC abrasive specification No. 1 (SSPC-AB 1), “Mineral and Slag Abrasives,” defines the qualification...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005747
EISBN: 978-1-62708-171-9
...: The Society for Protective Coatings (formerly the Steel Structures Painting Council), and NACE International (formerly the National Association of Corrosion Engineers): AWS C2.16/C2.16M:2002, “Guide for Thermal Spray Operator Qualification” (86 pages). This guide provides recommendations for thermal...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001462
EISBN: 978-1-62708-173-3
... Abstract Thermal spray coatings (TSCs) are surface coatings engineered to provide wear-, erosion-, abrasion-, and corrosion-resistant coatings for original equipment manufacture and for the repair and upgrading of in-service equipment. This article presents an overview of five thermal spray...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005576
EISBN: 978-1-62708-174-0
.... The critical features of FSW tool design, initial process parameters, systematic welding trials, and robustness testing are reviewed. The article provides information on the common features of welding procedure qualification. It also includes a table that lists the procedures used in the production of sound...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006035
EISBN: 978-1-62708-172-6
... and in PWRs. For the past thirty years, two standards ( Ref 2 , 3 ) have defined DBA qualification criteria for SR containment coatings. Both test protocols recommend temperature and pressure transients during specimen exposure. The DBA test procedure uses test coupons that have been previously...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005712
EISBN: 978-1-62708-171-9
... Abstract This article focuses on coatings and overlays adopted for use as wear- and corrosion-resistant materials in oil sand processing. It describes the most common application processes for oil sand coatings and overlays, including welding, high-velocity oxyfuel thermal spray, laser cladding...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003434
EISBN: 978-1-62708-195-5
... Operation of internal combustion engines Prohibited Use of motors and equipment that spray or throw lubricants Prohibited Generation of nonvolatile residue Controlled Compressed gas use Controlled Cardboard Limited Exposed wooden surfaces Allowed if no visible damage and coated...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005716
EISBN: 978-1-62708-171-9
... Abstract Thermal spray coatings are often modified or treated by a variety of post-coating operations to transform the as-coated material into a final product based on coating composition and application. This article provides a detailed description of the post-coating operations that fall...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003391
EISBN: 978-1-62708-195-5
... Qualification In the design of aerospace composite structures, “building block” qualification programs are frequently conducted to verify the capability of the structure under design loads. This method utilizes a combination of tests and supporting analyses to minimize developmental risk, cost, and weight...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004120
EISBN: 978-1-62708-184-9
... particularly successful in specifications for metallic materials; however, in other areas, such as paints and coatings, most military specifications have been retained by the various services. (For additional information on U.S. policy regarding federal agency use of voluntary consensus standards, refer...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004215
EISBN: 978-1-62708-184-9
... with a clear written procedure or instruction that identifies the capabilities and limitations of the inspection technique in terms of detection and sizing of defects, the minimum training and qualification requirements for the person performing the inspection, the methods of reporting...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005632
EISBN: 978-1-62708-174-0
... known as cladding, is an industrial process used to improve the corrosion resistance and wear resistance of common structural materials. This deposited material forms a coating on the substrate material that alters its surface properties and supplies a combination of desired properties not found in any...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001360
EISBN: 978-1-62708-173-3
..., qualification, and inspection of stud-welding. fasteners joining metal studs quality control stud arc welding STUD ARC WELDING (SW), also known as arc stud welding, is a commonly used method for joining a metal stud, or fastener, to a metal workpiece. The process has been used as an alternative...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001325
EISBN: 978-1-62708-170-2
... Abstract This article discusses coating products available for use in the aerospace industry that are compliant with regulations requiring reductions in emissions from organic solvents. The coating products addressed include primers, topcoats, and chemical milling maskants. It describes...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006016
EISBN: 978-1-62708-172-6
... and installation of the protective coating/lining system. Prior to beginning surface-preparation operations, many specifications will require a presurface-preparation inspection to verify the correction of fabrication defects and removal of surface contamination such as grease, oil, cutting compounds, lubricants...