Published: 01 January 1994
Fig. 1 Spray cleaning equipment More
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004143
EISBN: 978-1-62708-184-9
... foam cleaning vapor-phase organic cleaning on-line chemical cleaning sulfamic acid process equipment CHEMICAL CLEANING is the use of chemicals to dissolve or loosen deposits from process equipment and piping. It offers several advantages over mechanical cleaning, including more uniform removal...
Image
Published: 01 January 1994
Fig. 1 Equipment for spray cleaning operation More
Image
Published: 01 December 1998
Fig. 1 Equipment for spray cleaning operation More
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001226
EISBN: 978-1-62708-170-2
... Abstract Ultrasonic cleaning involves the use of high-frequency sound waves that is above the upper range of human heating, or about 18 kHz, to remove a variety of contaminants from parts immersed in aqueous media. This article describes the process, design considerations and the equipment...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001227
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the mineral and organic acid cleaning of iron and steel. It begins with a discussion on the application methods, process selection criteria, solution composition, equipment used, and control of process variables in mineral acid cleaning. The article...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001228
EISBN: 978-1-62708-170-2
..., indirect-suction (induction) wet or dry blast nozzle systems. This article focuses on the abrasive media, equipment, applications, and limitations of dry and wet blast cleaning. It discusses the health and safety precautions to be taken during mechanical cleaning. airless centrifugal blast blade...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001222
EISBN: 978-1-62708-170-2
... Abstract Alkaline cleaning is a commonly used method for removing a wide variety of soils from the surface of metals. This article focuses on the composition, operating conditions, and test and control of alkaline cleaners, as well as equipment used and their application methods. It describes...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003694
EISBN: 978-1-62708-182-5
... of coating as well as the equipment used. An overview of some of the most common coating inspection points and inspection equipment is also provided. corrosion-resistant coating system surface preparation roughening chemical washing steam cleaning hand tool cleaning power tool cleaning water...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001224
EISBN: 978-1-62708-170-2
... Abstract Emulsion cleaning is an industrial cleaning process that uses an organic solvent as the main active agent. This article provides information on the applications, concerns and limitations, and process parameters of emulsion cleaning. It describes the processing variables and equipment...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001223
EISBN: 978-1-62708-170-2
... Abstract Solvent cleaning is a surface preparation process that can be accomplished in room temperature baths (cold cleaning ) or by condensing vapors of a solvent on a workpiece (vapor degreasing). This article provides a detailed discussion on solvents, equipment, process limitations...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004103
EISBN: 978-1-62708-184-9
... Abstract Materials of construction for equipment and piping in pharmaceutical processing plants must be resistant to corrosion from the high-purity water, the buffer solutions used in preparation of the products, and the cleaning solutions used to maintain the purity of the product. The primary...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001225
EISBN: 978-1-62708-170-2
.... It provides an overview of the basic design and safety considerations of the salt bath equipment and describes the environmental impact of molten salt bath cleaning. casting cleaning environmental impact flame spray removal glass removal molten salt bath cleaning paint stripping personnel safety...
Book Chapter

Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001274
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the types, composition, and applications of phosphate coatings and describes the characteristics of phosphate-coated ferrous and nonferrous materials, including steel and aluminum. It addresses five successive process fundamentals: cleaning, rinsing, phosphating...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005725
EISBN: 978-1-62708-171-9
..., cleaning, roughening, masking, and preheating. Information on the equipment and process variables of dry abrasive grit blasting are also provided. The article describes the roles of spray stream and the spray pattern for all thermal spray processes. It discusses the defects arising from poor temperature...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006008
EISBN: 978-1-62708-172-6
... Abstract Coatings, such as those applied to ships, must be resistant to abrasion, in the case of cargo hold coatings, and cyclic changes of chemicals and tank cleaning, in the case of tank linings. Failures and defects can manifest themselves at various times in the life of a coating...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003996
EISBN: 978-1-62708-185-6
... Abstract This article begins with discussion on forgeability and the factors affecting the forgeability of aluminum and aluminum alloys. It describes the types of forging methods and equipment and reviews critical elements in the overall aluminum forging process: die materials, die design...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004000
EISBN: 978-1-62708-185-6
... affecting forgeability. It describes the forging techniques, equipment, and common processing elements associated with titanium alloy forging. The processing elements include the preparation of forging stock, preheating of the stock, die heating, lubrication, forging process, trimming and repair, cleaning...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003992
EISBN: 978-1-62708-185-6
.... This article discusses the forging methods, primary mill practices (primary forging and ingot breakdown), trimming, and cleaning operations of stainless steels. It describes the use of forging equipment, dies, and die material in the forging operation. The article provides an overview of the forgeability...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
... Abstract Precipitation hardening is a hardening mechanism found in various steels and alloy systems, such as nickel-, cobalt-, titanium-, copper-, and iron-base alloys. This article provides a brief description of precipitation hardening process, furnace equipment, surface-related problems...