1-20 of 301 Search Results for

circulation cleaning

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004143
EISBN: 978-1-62708-184-9
... Abstract This article describes the eight chemical cleaning methods, namely, circulation, fill and soak, cascade, foam, vapor-phase organic, steam-injected, on-line chemical, and mechanical cleaning. It presents information on deposit types, solvents used to remove them, and construction...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003610
EISBN: 978-1-62708-182-5
... metal coolants is described. Some information on safety precautions for handling liquid metals, operating circulating systems, dealing with fire and spillage, and cleaning contaminated components, are also provided. liquid-metal corrosion liquid-metal system liquid-vapor metal coolants safety...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005350
EISBN: 978-1-62708-187-0
... the various factors for improving and maintaining furnace efficiencies. It explains the benefits of circulating molten metal in reverberatory furnaces and circulation methods. aluminum metal casting dry hearth reverberatory furnace reverberatory furnace stack furnace wet hearth reverberatory furnace...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001222
EISBN: 978-1-62708-170-2
... solution Moving conveyor cleaning , in which solution flow is created as parts are dragged through the cleaner Mechanical agitation , in which the cleaner is circulated using pumps, mechanical mixers, or ultrasonic waves Mechanical contact , in which the cleaner is applied with external forces...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005997
EISBN: 978-1-62708-168-9
... from the bars and carefully machined and cleaned to give smoth, bright surfaces. They were then heated for various times at several temperatures in air-circulating furnaces controlled to within ±3 °C (±5 °F) of the desired temperatures. The results of this study are shown in Fig. 1 for 1035 steel...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001324
EISBN: 978-1-62708-170-2
.... Arrangement of parts in the dip basket is very important. The parts should not overlap and there should be space between each part to allow the cleaning solution to circulate. The most common reason for unsatisfactory results is failing to follow these requirements. Ultrasonic Dip Tank Methods...
Book Chapter

By Te-Lin Yau
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003645
EISBN: 978-1-62708-182-5
..., volume, velocity, and waterline effects; specimen surface preparation; method of immersion of specimens; duration of test; and method of cleaning specimens. The article discusses the different conditions of immersion testing, namely, full immersion condition, high temperature condition, partial immersion...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006528
EISBN: 978-1-62708-207-5
... are normally unacceptable. Enameling Process The porcelain enameling process involves grinding a mixture of frit, water, and various suspending agents to form a slurry of creamlike consistency that can be applied, typically by spraying, to the cleaned and prepared aluminum. This section briefly...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003189
EISBN: 978-1-62708-199-3
... the lubrication and cooling requirements are not severe. The oils are noncorrosive and stable and, if kept clean, can be used almost indefinitely. They lubricate all exposed moving parts, and minor leakage into or from gear boxes, bearings, and hydraulic systems does not upset a machine's performance. Fatty...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005992
EISBN: 978-1-62708-166-5
... not be used for parts whose configurations make them hard to clean Fluidized beds 100–750 212–1380 Broad range of heat transfer rates are possible by varying the choice of fluidizing gas, gas velocity, bed temperature and the bed particle size. More energy efficient than convection furnaces...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001256
EISBN: 978-1-62708-170-2
... or grease in solution Check and dump if positive. Poor cleaning Check/analyze descale and activation for proper operating conditions. Insufficient solution agitation Check circulating pump. Rough deposits Particles (anode sludge, dirt) in solution Check filter for proper operating condition...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006407
EISBN: 978-1-62708-192-4
... that deflects the oil to a drilled passage leading to the bearing. A limitation of sump systems is the lack of effective filtration. Such systems are only suitable for inherently clean-running applications. Circulating Fluid Systems Operation at higher speeds will cause the temperature to increase...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005196
EISBN: 978-1-62708-187-0
... the furnace coils and power supplies of the induction furnaces need to be cooled, a closed-loop water system is generally called for. In a medium-frequency power supply, the electronic components of the system contain a dc leg; it is therefore important to have clean, demineralized water circulating...
Book Chapter

Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003412
EISBN: 978-1-62708-195-5
.... It presents a discussion on the major elements of an autoclave system, namely, pressure vessel, gas stream heating and circulation sources, gas stream pressurizing systems, loading systems, and vacuum systems. The article describes a computerized approach to the simultaneous control of materials reaction...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001277
EISBN: 978-1-62708-170-2
..., porosity, dimensional stability, and corrodibility affect the choice of a proper finishing system. Smooth, clean metal surfaces that cannot be phosphate coated lack sufficient “tooth” for good adhesion of some air-dried coatings. (“Tooth” is the coarse or abrasive quality of a substrate that facilitates...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006254
EISBN: 978-1-62708-169-6
.... The use of sulfur dioxide requires frequent cleaning of furnace controls and fixtures and replacement of furnace parts because of the formation of corrosive sulfuric acid in the furnace system. When heat treating both magnesium and aluminum alloy castings in the same furnace is desired, a carbon dioxide...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006504
EISBN: 978-1-62708-207-5
... of applications of such products. It describes the two main categories of cleaning that can be used with most any metal, namely, mechanical cleaning and chemical cleaning. The article provides a discussion on the laboratory evaluation of cleaners, field testing of cleaners, and cleaner types and procedures...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001227
EISBN: 978-1-62708-170-2
... as sequesterants by tying up the dissolved metal ions and carrying them away from the surface being cleaned. With the use of heated solutions and proper circulation of cleaning solution, organic acids efficiently remove metal oxides. Low corrosivity to the cleaned metal surface is another important reason...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005927
EISBN: 978-1-62708-166-5
... perforated plate and porous plate gas distributors. Because of the nonuniformities of temperature and atmosphere in the grid zone, the parts to be treated are commonly not placed in this zone. Main Zone and Particle Circulation The part-loading zone is the main zone above the grid zone and can extend...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005667
EISBN: 978-1-62708-198-6
... from a biocompatibility perspective. These include raw materials, the manufacturing process, cleaning and sterilization processes, and biodegradation and biostability. The article reviews the general testing methods of polymers, such as chemical, mechanical and thermal. It concludes with a section...