1-5 of 5 Search Results for

chlorobutyl

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003847
EISBN: 978-1-62708-183-2
... natural rubber, semihard natural rubber, hard natural rubber, neoprene or polychloroprene, chlorobutyl, three-ply linings, nitrile, and ethylene propylene with a diene monomer. Emphasis is placed on advantages, disadvantages, and common uses of each material discussed. abrasion resistance corrosion...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006027
EISBN: 978-1-62708-172-6
...) Butyl rubber (IIR, a blend of isoprene and isobutylene copolymers) Chlorobutyl rubber (CUR, manufactured by the chlorination of IIR) Ethylene-propylene rubber (EPDM, a copolymer of ethylene and propylene with the addition of a diene monomer) Nitrile rubber (NBR, a copolymerization of...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006006
EISBN: 978-1-62708-172-6
... acid, which forms a hard chloride layer that inhibits or at least slows further acid attack. Synthetic chlorobutyl rubber is used for other exposures that do not require the chloride conversion process, most notably phosphoric and superphosphoric acid. It is formulated either with a certain...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003030
EISBN: 978-1-62708-200-6
... plastics ( Ref 23 ). A wheel faced with a chlorobutyl rubber tire revolves against a stationary test specimen while a flow of sand is forced between the wheel and the specimen. The severity of the test is adjusted by varying test duration and the force with which the specimen is applied to the wheel. This...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003026
EISBN: 978-1-62708-200-6
... acrylonitrile constituent Butyl IIR Isobutylene-isoprene Electrical properties generally good but not outstanding in any area Chlorobutyl IIR Chloroisobutylene-isoprene Same general properties as butyl Cis-4 BR Polybutadiene Used principally as a blend in other rubbers Thiokol (PS...