1-12 of 12 Search Results for

chlorendic resins

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By Tim Pepper
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003363
EISBN: 978-1-62708-195-5
... Abstract This article provides an overview of the various types of unsaturated polyester resins and low-profile additives. The resins include general-purpose resins, isophthalic resins, bisphenol A fumarate resins, chlorendic resins, and vinyl ester resin. The article describes the mechanical...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003010
EISBN: 978-1-62708-200-6
... Abstract A thermosetting resin, or thermoset, is a synthetic organic polymer that cures to a solid, infusible mass by forming a three-dimensional network of covalent chemical bonds. Significant applications include construction and thermoset engineering plastics. This article discusses...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006945
EISBN: 978-1-62708-395-9
... Association computed tomography; compact tension coef cient of thermal expansion chlorotri uoroethylene crack tip opening displacement Diallyl chlorendate; distance amplitude correction diallyl phthalate ductile-brittle transition temperature dynamic dielectric analysis diaminodiphenylsulfone design...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006009
EISBN: 978-1-62708-172-6
... Abstract This article provides a discussion on polyester coating applications such as powder coatings, can coatings, and automotive paints. It includes an overview, structure, properties, and benefits of vinyl ester resins. The article discusses the additives for both unsaturated polyester...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003845
EISBN: 978-1-62708-183-2
..., as indicated in Table 1 . Corrosion-resistant resins Table 1 Corrosion-resistant resins Family Types Polyester Isophthalic Terephthalic Bisphenol-A fumarate Chlorendic anhydride Epoxy Bisphenol-A Epoxy novolac Epoxy vinyl ester Bisphenol-A Epoxy novolac Furan...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006077
EISBN: 978-1-62708-172-6
... Abstract This article provides a detailed discussion on the principal classes and curatives of epoxy resins used in the coatings industry. The principal classes are bisphenol A epoxy, bisphenol F epoxy, epoxy phenol novolac, cycloaliphatic epoxies, epoxy acrylate, brominated bisphenol-A-based...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006037
EISBN: 978-1-62708-172-6
... Abstract Polymeric floor coatings refer to flooring materials composed of multicomponent thermoset resins formulated with various fillers and pigments that are installed in situ, usually over concrete substrates. Polymeric flooring systems, specified for all industrial and commercial...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003005
EISBN: 978-1-62708-200-6
... (grade A ingot) 1.36 2.38 Magnesium (ingot) 0.29 0.51 Brass (ingot) 1.25 2.18 Mild steel (sheet) 0.27 0.47 Amino resin thermoset 0.85 1.49 Nylon 6/6 0.25 0.44 Aluminum (ingot) 0.78 1.37 Aluminum (ingot) 0.21 0.37 Phenolic thermoset 0.75 1.31 PMMA 0.19 0.33 Silicon...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.9781627082006
EISBN: 978-1-62708-200-6
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003068
EISBN: 978-1-62708-200-6
.... increase in mass of a porous solid body resulting from formed by the decomposition of the resin. the penetration of a liquid into its permeable pores. See ABA copolymers. Block copolymers with three se- also adsorption. acid refractory. Siliceous ceramic materials of a quences, but only two domains. high...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004184
EISBN: 978-1-62708-184-9
.... The article discusses the corrosion effects of caustic soda on nonmetallic materials: plastics, thermoplastics, thermosetting resin materials, carbon and graphite, and ceramics. It concludes with information on the effects of contamination of and by caustic and of admixtures of caustic with other chemicals...