1-20 of 721 Search Results for

chemical embrittlement

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006087
EISBN: 978-1-62708-175-7
... such as precipitation from salt solution and gas, chemical embrittlement, hydride decomposition, and thermite reactions are also discussed. The article also discusses the methods used to produce powders electrolytically and the types of metal powders produced. The physical and chemical characteristics of these powders...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006867
EISBN: 978-1-62708-395-9
... performance. Plasticizer migration from PVC is a well-known phenomenon ( Ref 7 ) that results not only in embrittlement and/or loss of flexibility of the PVC part but also loss of the plasticizer chemical(s) into the environment. Plasticizer migration from flexible PVC onto or into a different polymer...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001268
EISBN: 978-1-62708-170-2
... not require the use of toxic chemicals Simplifies waste treatment Does not require baking in most cases Provides greater uniformity of coatings (when used for galvanizing) Hydrogen Embrittlement The need to prevent hydrogen embrittlement was one of the major reasons for the creation and use...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... in the selection of stainless steel, namely corrosion resistance, fabrication characteristics, product forms, thermally induced embrittlement, mechanical properties in specific temperature ranges, and product cost. austenitic stainless steel chemical composition corrosion resistance duplex stainless steel...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003667
EISBN: 978-1-62708-182-5
... in the published literature over the definition of hydrogen embrittlement. Metal processing, chemical, and petrochemical industries have experienced various types of hydrogen problems for many years. The aerospace industry has experienced new and unexpected hydrogen embrittlement problems, principally in dealing...